| THE EFFECT OF LONG-TERM AGING ON THE GAMMA PRIME CHARACTERISTICS AND TENSILE PROPERTIES IN Ni-BASE SUPERALLOY K44 |
|
Cite this article:
. THE EFFECT OF LONG-TERM AGING ON THE GAMMA PRIME CHARACTERISTICS AND TENSILE PROPERTIES IN Ni-BASE SUPERALLOY K44. Acta Metall Sin, 2006, 42(5): 481-486 .
|
|
|
Abstract The effect of long-term aging on the γ’ characteristics and the mechanical properties have been investigated in a corrosion resistant nickel-base superalloy K44 aged isothermally in the temperature range of 800-900℃ up to 10000 h. SEM observation reveals that the coarsening kinetics of γ’ follows Lifshitz-Slyozof-Wagner (LSW) theory at different temperatures, with the activation energy of 255 kJ/mol for growth. Morphological instability occurs in relatively small γ’ precipitates during aging process. At room temperature (RT) and 900℃, yield strength decreases with aging temperature and aging time increasing, while fluctuation of elongation is observed. The dependence of the yield stress on particle size is explained by Labusch-Schwarz hardening theory rather than classical strengthening theory on coherency and mismatch strengthening. Shearing of strong-coupled dislocations is dominant strengthening mechanism.
|
|
Received: 23 September 2005
|
|
|
[1] Nembach E. Particle Strengthening for Metals and Alloys. New York: John Wiley & Sons, 1997: 230 [2] Reppich B, Schepp P. Wehner G. Acta Metall, 1982; 30: 95 [3] Brown L M, Ham R K. In: Kelly A, Nicholson R B, eds., Strengthening Methods in Crystals, Amsterdam: Elsevier, 1971: 9 [4] Ardell A J. Met Trans, 1985; 16A: 2131 [5] Hou J S, Zhang Y L, Guo J T, Ji G, Zhou L Z, Ye H Q. Acta Metall Sin, 2004; 40: 579 (侯介山,张玉龙,郭建亭,冀光,周兰章,叶恒强.金属学 报,2004;40:579) [6] Lifshitz I M, Slyozov V V. J Phys Chem Solids, 1961; 19: 35 [7] Wagner C Z. Elektrochem, 1961; 65: 581 [8] Stevens R A, Flewitt P E J. Mater Sci Eng, 1979; 37: 237 [9] Baldan A. J Mater Sci, 2002; 37: 2379 [10] Yoo Y S. Scr Mater, 2005; 53: 81 [11] Narayan V. http://www.msm.cam.ac.uk/map /data/ neural/lattmisfit-b.html. University of Cambridge. [12] Pollock T M, Argon A S. Acta Metall Mater, 1991;40:1 [13] Fior N F. High Temp Mater, 1975; 2: 373 [14] Guo S R, Lu D Z, Guo J T. Acta Metall Sin,1998;34: 482 (郭守仁,卢德忠,郭建亭.金属学报,1998;34:482) [15] Morinaga M, Yukawa N, Ezaki H. Philos Mag, 1995; 51A: 223 [16] Durrand-Charre M. The Microstructure of Superalloys. Amsterdam: Gordon and Breach Science Publishers, 1997:12 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|