| Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study |
WANG Shuo1, WANG Junsheng1,2( ) |
1.School of Materials, Beijing Institute of Technology, Beijing 100081, China 2.Advanced Research Institute for Multidisciplinary Science, Beijing Institute of Technology, Beijing 100081, China |
|
Cite this article:
WANG Shuo, WANG Junsheng. Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study. Acta Metall Sin, 2022, 58(10): 1325-1333.
|
|
|
Abstract To obtain the stable interfacial structures of a δ'/θ'/δ' nanocomposite precipitate in Al-Li alloys, the formation enthalpy, interfacial energy, cleavage work, and ideal cleavage strength are calculated for all constructed interface structures at different growth stages. Thus, the results indicate that the δ'/θ'/δ' adopts an anti-phase a /2[110] interfacial structure when the θ' phase contains an odd number of Cu layers; conversely, it adopts an in-phase #2 interfacial structure. As θ' increases, these two structures transform by slipping a /2 along the [110] direction. Simultaneously, the heterogeneous nucleation of δ' achieves the stable δ'/θ' interfacial structure spontaneously. Under Rose's fracture model, this stable interfacial structure also possesses the highest bonding strength and the largest ideal cleavage strength. Finally, the crystal orbital Hamilton population and bond length analyses reveal the relation between the electronic bonding and structural stability. It is shown that the inter Al—Al interactions significantly influence the structural stability, which mainly originated from the 3p—3p orbital-pair contributions.
|
|
Received: 26 February 2021
|
|
|
| Fund: National Natural Science Foundation of China(52073030) |
About author: WANG Junsheng, professor, Tel: (010)68915043, E-mail: junsheng.wang@bit.edu.cn
|
| 1 |
Zhang P, Chen M H. Progress in characterization methods for thermoplastic deforming constitutive models of Al-Li alloys: A review [J]. J. Mater. Sci., 2020, 55: 9828
doi: 10.1007/s10853-020-04682-8
|
| 2 |
Decreus B, Deschamps A, De Geuser F, et al. The influence of Cu/Li ratio on precipitation in Al-Cu-Li-x alloys [J]. Acta Mater., 2013, 61: 2207
doi: 10.1016/j.actamat.2012.12.041
|
| 3 |
Miao J S, Sutton S, Luo A A. Microstructure and hot deformation behavior of a new aluminum-lithium-copper based AA2070 alloy [J]. Mater. Sci. Eng., 2020, A777: 139048
|
| 4 |
Kilmer R J, Stoner G E. Effect of Zn additions on precipitation during aging of alloy 8090 [J]. Scr. Metall. Mater., 1991, 25: 243
doi: 10.1016/0956-716X(91)90388-H
|
| 5 |
Meng L, Zheng X L. Overview of the effects of impurities and rare earth elements in Al-Li alloys [J]. Mater. Sci. Eng., 1997, A237: 109
|
| 6 |
Vasudévan A K, Fricke W G, Malcolm R C, et al. On through thickness crystallographic texture gradient in Al-Li-Cu-Zr alloy [J]. Metall. Trans., 1988, 19A: 731
|
| 7 |
Zhao T Z, Jin L, Xu Y, et al. Anisotropic yielding stress of 2198 Al-Li alloy sheet and mechanisms [J]. Mater. Sci. Eng., 2019, A771: 138572
|
| 8 |
Kaibyshev R, Shipilova K, Musin F, et al. Continuous dynamic recrystallization in an Al-Li-Mg-Sc alloy during equal-channel angular extrusion [J]. Mater. Sci. Eng., 2005, A396: 341
|
| 9 |
Liu B, Chen Z, Wang Y X, et al. The effect of an electric field on the mechanical properties and microstructure of Al-Li alloy containing Ce [J]. Mater. Sci. Eng., 2001, A313: 69
|
| 10 |
Sidhar H, Mishra R S. Aging kinetics of friction stir welded Al-Cu-Li-Mg-Ag and Al-Cu-Li-Mg alloys [J]. Mater. Des., 2016, 110: 60
doi: 10.1016/j.matdes.2016.07.126
|
| 11 |
Terrones L A H, Monteiro S N. Composite precipitates in a commercial Al-Li-Cu-Mg-Zr alloy [J]. Mater. Charact., 2007, 58: 156
doi: 10.1016/j.matchar.2006.04.008
|
| 12 |
Deschamps A, Garcia M, Chevy J, et al. Influence of Mg and Li content on the microstructure evolution of Al-Cu-Li alloys during long-term ageing [J]. Acta Mater., 2017, 122: 32
doi: 10.1016/j.actamat.2016.09.036
|
| 13 |
Gumbmann E, De Geuser F, Sigli C, et al. Influence of Mg, Ag and Zn minor solute additions on the precipitation kinetics and strengthening of an Al-Cu-Li alloy [J]. Acta Mater., 2017, 133: 172
doi: 10.1016/j.actamat.2017.05.029
|
| 14 |
Mao Z, Chen W, Seidman D N, et al. First-principles study of the nucleation and stability of ordered precipitates in ternary Al-Sc-Li alloys [J]. Acta Mater., 2011, 59: 3012
doi: 10.1016/j.actamat.2011.01.041
|
| 15 |
Wang S, Zhang C, Wang J S. Structures and properties of nano-precipitates in Al-Li alloys [J]. Aeronaut. Manuf. Technol., 2021, 64: 68
|
|
王 硕, 张 弛, 王俊升. 铝锂合金纳米析出相结构与性能综述 [J]. 航空制造技术, 2021, 64: 68
|
| 16 |
Wang S, Zhang C, Li X, et al. Heterophase interface dominated deformation and mechanical properties in Al-Cu-Li Alloys [J]. Adv. Theory Simul., 2021, 4: 2100059
doi: 10.1002/adts.202100059
|
| 17 |
Duan S Y, Wu C L, Gao Z, et al. Interfacial structure evolution of the growing composite precipitates in Al-Cu-Li alloys [J]. Acta Mater., 2017, 129: 352
doi: 10.1016/j.actamat.2017.03.018
|
| 18 |
Wang S, Zhang C, Li X, et al. First-principle investigation on the interfacial structure evolution of the δ'/θ'/δ' composite precipitates in Al-Cu-Li alloys [J]. J. Mater. Sci. Technol., 2020, 58: 205
doi: 10.1016/j.jmst.2020.03.065
|
| 19 |
Wang S, Zhang C, Li X, et al. Uncovering the influence of Cu on the thickening and strength of the δ'/θ'/δ' nano-composite precipitate in Al-Cu-Li alloys [J]. J. Mater. Sci., 2021, 56: 10092
doi: 10.1007/s10853-021-05894-2
|
| 20 |
Rose J H, Smith J R, Ferrante J. Universal features of bonding in metal [J]. Phys. Rev., 1983, 28B: 1835
|
| 21 |
Maintz S, Deringer V L, Tchougréeff A L, et al. Analytic projection from plane-wave and PAW wavefunctions and application to chemical-bonding analysis in solids [J]. J. Comput. Chem., 2013, 34: 2557
doi: 10.1002/jcc.23424
pmid: 24022911
|
| 22 |
Kresse G, Furthmüller J. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set [J]. Phys. Rev., 1996, 54B: 11169
|
| 23 |
Blöchl P E. Projector augmented-wave method [J]. Phys. Rev., 1994, 50B: 17953
|
| 24 |
Monkhorst H J, Pack J D. Special points for Brillouin-zone integrations [J]. Phys. Rev., 1976, 13B: 5188
|
| 25 |
Vaithyanathan V, Wolverton C, Chen L Q. Multiscale modeling of θ′ precipitation in Al-Cu binary alloys [J]. Acta Mater., 2004, 52: 2973
doi: 10.1016/j.actamat.2004.03.001
|
| 26 |
Wang Y, Liu Z K, Chen L Q, et al. First-principles calculations of β″-Mg5Si6/α-Al interfaces [J]. Acta Mater., 2007, 55: 5934
doi: 10.1016/j.actamat.2007.06.045
|
| 27 |
Butler K T, Gautam G S, Canepa P. Designing interfaces in energy materials applications with first-principles calculations [J]. npj Comput. Mater., 2019, 5: 19
doi: 10.1038/s41524-019-0160-9
|
| 28 |
Zhang S H, Fu Z H, Zhang R F. ADAIS: Automatic derivation of anisotropic ideal strength via high-throughput first-principles computations [J]. Comput. Phys. Commun., 2019, 238: 244
doi: 10.1016/j.cpc.2018.12.012
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|