| Effect of Microstructure Instability on Hot Plasticity During Thermomechanical Processing in PM Nickel-Based Superalloy |
Ming ZHANG1,2, Guoquan LIU1,2( ), Benfu HU1 |
1 School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083, China 2 Collaborative Innovation Center of Steel Technology, University of Science and Technology Beijing, Beijing 100083, China |
|
Cite this article:
Ming ZHANG, Guoquan LIU, Benfu HU. Effect of Microstructure Instability on Hot Plasticity During Thermomechanical Processing in PM Nickel-Based Superalloy. Acta Metall Sin, 2017, 53(11): 1469-1477.
|
|
|
Abstract High alloying Ni-based powder metallurgy (PM) superalloys show excellent fatigue performance and damage tolerance properties, and good creep resistance at 750 ℃, and are used for advanced gas turbine disks and other hot components. The hot-working window of high alloying PM superalloy is narrow because of its poor workability. The formation of the γ+γ′ microduplex structure during the thermomechanical processing always results in a decrease in flow stress and a promotion of hot plasticity. However, the stability of the γ+γ′ microduplex structure has not been evaluated. The high temperature flow behavior of a Ni-based superalloy FGH98 prepared by hot isostatic pressing has been examined by means of uniaxial compression testing isothermally at 1060, 1105, 1138 and 1165 ℃ and at constant true strain rates between 0.01 and 10 s-1. The microstructural evolution and instabilities during plastic flow have been studied. Under all testing conditions, the as-hipped material exhibits flow hardening, flow softening and steady-state flow sequentially with the true strain increased. The dynamic recrystallization occurs and the γ+γ′ microduplex structures are generated when steady state flow or highest strains achieved at temperatures below the γ′ solvus. The formation of the γ+γ′ microduplex structures results in a remarkable decrease in grain size and a promotion of hot plasticity. The relationships between steady-state grain sizes and steady-state stresses during deformation and the formation mechanism of the γ+γ′ microduplex structure were analyzed. The possibility of the microstructure controlling during hot working was discussed.
|
|
Received: 08 May 2017
|
| ZTFLH: |
TG132.32
|
|
| |
TG113.12
|
|
| |
TG113.26
|
|
|
| Fund: Supported by National High Technology Research and Development Program of China (No.2015AA034201) and National Natural Science Foundation of China No.51371030 |
| [1] | Gessinger G H, Bomford M J.Powder metallurgy of superalloys[J]. Int. Metall. Rev., 1974, 19: 51 | | [2] | Wilkinson N A.Technological considerations in the forging of superalloy rotor parts[J]. Met. Technol., 1977, 4: 346 | | [3] | Immarigeon J P A, Van Drunen G, Wallace W. The hot working behaviour of Mar M200 superalloy compacts [A]. Superalloys 1976: Proceedings of the Third International Symposium[C]. Seven Springs, PA: TMS, 1976: 463 | | [4] | Coyne J E.Microstructural control in titanium-and nickel-base forgings; An overview[J]. Met. Technol., 1977, 4: 337 | | [5] | Semiatin S L, McClary K E, Rollett A D, et al. Plastic flow and microstructure evolution during thermomechanical processing of a PM nickel-base superalloy[J]. Metall. Mater. Trans., 2013, 44A: 2778 | | [6] | Wu K, Liu G Q, Hu B F, et al.Effect of processing parameters on hot compressive deformation behavior of a new Ni-Cr-Co based P/M superalloy[J]. Mater. Sci. Eng., 2011, A528: 4620 | | [7] | Ning Y Q, Yao Z K, Li H, et al.High temperature deformation behavior of hot isostatically pressed P/M FGH4096 superalloy[J]. Mater. Sci. Eng., 2010, A527: 961 | | [8] | Alniak M O, Bedir F.Modelling of deformation and microstructural changes in P/M René 95 under isothermal forging conditions[J]. Mater. Sci. Eng., 2006, A429: 295 | | [9] | Liu Y H, Ning Y Q, Yao Z K, et al.Plastic deformation and dynamic recrystallization of a powder metallurgical nickel-based superalloy[J]. J. Alloys Compd., 2016, 675: 73 | | [10] | He G A, Liu F, Si J Y, et al.Characterization of hot compression behavior of a new HIPed nickel-based P/M superalloy using processing maps[J]. Mater. Des., 2015, 87: 256 | | [11] | Zhang C, Zhang L W, Li M F, et al.Effects of microstructure and γ′ distribution on the hot deformation behavior for a powder metallurgy superalloy FGH96[J]. J. Mater. Res., 2014, 29: 2799 | | [12] | Zhang H B, Zhang K F, Lu Z, et al.Hot deformation behavior and processing map of a γ′-hardened nickel-based superalloy[J]. Mater. Sci. Eng., 2014, A604: 1 | | [13] | Wu K, Liu G Q, Hu B F, et al.Characterization of hot deformation behavior of a new Ni-Cr-Co based P/M superalloy[J]. Mater. Charact., 2010, 61: 330 | | [14] | Zhang M J, Li F G, Wang S Y, et al.Characterization of hot deformation behavior of a P/M nickel-base superalloy using processing map and activation energy[J]. Mater. Sci. Eng., 2010, A527: 6771 | | [15] | Kandeil A Y, Immarigeon J P A, Wallace W, et al. Flow behaviour of Mar M200 powder compacts during isothermal forging[J]. Met. Sci., 1980, 14: 493 | | [16] | Alniak M O, Bedir F.Change in grain size and flow strength in P/M René 95 under isothermal forging conditions[J]. Mater. Sci. Eng., 2006, B130: 254 | | [17] | Kikuchi S, Ando S, Shu F, et al.Superplastic deformation and microstructure evolution in PM IN-100 superalloy[J]. J. Mater. Sci., 1990, 25: 4712 | | [18] | Yu Q Y, Yao Z H, Dong J X.Deformation and recrystallization behavior of a coarse-grain, nickel-base superalloy Udimet720Li ingot material[J]. Mater. Charact., 2015, 107: 398 | | [19] | Chen J Y, Dong J X, Zhang M C, et al.Deformation mechanisms in a fine-grained Udimet 720LI nickel-base superalloy with high volume fractions of γ′ phases[J]. Mater. Sci. Eng., 2016, A673: 122 | | [20] | Zhang B J, Zhao G P, Zhang W Y, et al.Deformation mechanisms and microstructural evolution of γ+γ′ duplex aggregates generated during thermomechanical processing of nickel-base superalloys [A]. Proceedings of the 13th International Symposium on Superalloys[C]. Seven Springs, PA: TMS, 2016: 487 | | [21] | Exner H E.Analysis of grain-and particle-size distributions in metallic materials[J]. Int. Metall. Rev., 1972, 17: 25 | | [22] | Hu B F, Jin K S, Li H Y, et al.The interaction of recrystallizing interfaces with precipitates in a P/M nickel-base superalloy[J]. J. Univ. Sci. Eng. Beijing, 1993, 15: 14(胡本芙, 金开生, 李慧英等. FGH95合金再结晶界面与晶内析出γ′相的作用[J]. 北京科技大学学报, 1993, 15: 14) | | [23] | Menzies R G, Davies G J, Edington J W.Microstructural changes during recrystallization of powder-consolidated nickel-base superalloy IN-100[J]. Met. Sci., 1981, 15: 217 | | [24] | Prasad Y V R K, Gegel H L, Doraivelu S M, et al. Modeling of dynamic material behavior in hot deformation: Forging of Ti-6242[J]. Metall. Trans., 1984, 15A: 1883 | | [25] | Prasad Y V R K, Seshacharyulu T. Modelling of hot deformation for microstructural control[J]. Int. Mater. Rev., 1998, 43: 243 | | [26] | Immarigeon J A, Floyd P H.Microstructural instabilities during superplastic forging of a nickel-base superalloy compact[J]. Metall. Trans., 1981, 12A: 1177 | | [27] | Lin Y C, Wu X Y, Chen X M, et al.EBSD study of a hot deformed nickel-based superalloy[J]. J. Alloys Compd., 2015, 640: 101 | | [28] | Chen X M, Lin Y C, Wen D X, et al.Dynamic recrystallization behavior of a typical nickel-based superalloy during hot deformation[J]. Mater. Des., 2014, 57: 568 | | [29] | Menzies R G, Edington J W, Davies G J.Superplastic behaviour of powder-consolidated nickel-base superalloy IN-100[J]. Met. Sci., 1981, 15: 210 |
|