    					| BINOCULAR STEREO VISION MEASUREMENT RESEARCH FOR SUPERPLASTIC FREE BULGING |  
						| MA Pinkui(  ), SONG Yuquan |  
						| Superplastic and Plastic Research Institute, Jilin University, Changchun 130025 |  
						|  |  
					
			      MA Pinkui, SONG Yuquan. BINOCULAR STEREO VISION MEASUREMENT RESEARCH FOR SUPERPLASTIC FREE BULGING. Acta Metall Sin, 2014, 50(4): 471-478.	
				 
					
						| 
								
									|  
          
          
            
              
				
												  
													
													    |  |  
														| Abstract It is a significant foundation of superplastic free bulging analytic theory to accurately measure the surface profile and the deformation of each point on surface. Based on an important feature of the profile of the free bulging part which can be depicted as axisymmetric rotating surface, in this study, the measurement of the surface was translated into that of the feature points on the part surface, and the three-dimensional coordinates of these points were measured by the binocular stereo vision system for the first time. Then, through curve fitting, contour surface and geometric parameters were determined, and the strain were characterized through analyzing coordinates change of the feature points and distance change between two adjacent points. The setup and the measuring method of the vision system were introduced, as well as several key steps, such as system model, calibration method, elimination of influence of high temperature, and image processing. The methods were proposed for measuring geometric parameters and deformation of bulging part , and the related experiments were performed. |  
															| Received:  02 December 2013 |  
															|  |  
															| Fund: Supported by National Natural Science Foundation of China (Nos.51005099 and 51005098) and Natural Science Foundation of Jilin Province (No.201115015) |  
															| About author:  null 
 马品奎, 男, 1975年生, 副教授, 博士 |  
            
									            
									               
																							
					| [1] | Giuliano G, Franchitti S. Int J Mach Tool Manuf, 2007; 47: 471 |  
					| [2] | Jovance F. Int J Mech Sci, 1968; 10: 403 |  
					| [3] | Holt D L. Int J Mech Sci, 1970; 12: 491 |  
					| [4] | Cheng J H. J Mater Process Technol, 1996; 58: 233 |  
					| [5] | Cornfield G C, Johnson R H. Int J Mech Sci, 1970; 12: 479 |  
					| [6] | Jeyasingh J J V, Rao B N. J Mater Process Technol, 2005; 160: 370 |  
					| [7] | Luo Z J, Guo N C, Gong Q Y. J Northwestern Polytech Univ, 1985; 3: 419 |  
					|  | (罗子键, 郭乃成, 龚泉源. 西北工业大学学报, 1985; 3: 419) |  
					| [8] | Tang S, Robbins T L. J Eng Mater Technol, 1974; 96: 77 |  
					| [9] | Enikeev F U, Kruglov A A. Int J Mech Sci, 1995; 37: 473 |  
					| [10] | Cheng J H. Int J Mech Sci, 1994; 36: 981 |  
					| [11] | Song Y Q, Zhao J. Mater Sci Eng, 1986; 84: 111 |  
					| [12] | Song Y Q. Mater Sci Eng, 1987; 86: 179 |  
					| [13] | Song Y Q. Chin J Mech Eng, 1989; 25: 80 |  
					|  | (宋玉泉. 机械工程学报, 1989; 25: 80) |  
					| [14] | Song Y Q, Lian S J. Sci China, 1990; 33A: 1246 |  
					| [15] | Yang H S, Mukhjee A K. Int J Mech Sci, 1992; 34: 283 |  
					| [16] | Brandon J F, Lecoanet H, Oytana C. Int J Mech Sci, 1979; 21: 379 |  
					| [17] | Song Y Q, Zuo W Y. Sci China, 1992; 35A: 122 |  
					| [18] | Song Y Q, Zuo W Y. Sci China, 1992: 35A: 247 |  
					| [19] | Song Y Q, Zuo W Y. Sci China, 1992; 35A: 1388 |  
					| [20] | Hsu C C, Wang W H. Mater Sci Eng, 1996; A205: 247 |  
					| [21] | Huang A, Lowe A, Cardew-Hall M J. J Mater Process Technol, 2001; 112: 136 |  
					| [22] | Song Y Q, Zhao J, Wan S D. Met Sci Technol, 1985; 4(3): 89 |  
					|  | (宋玉泉, 赵 军, 万胜狄.金属科学与工艺, 1985; 4(3): 89) |  
					| [23] | Lin Y Y, Lou X S, Zhang A B. J Exp Mech, 1992; 7: 351 |  
					|  | (林有义, 骆晓森, 张爱斌. 实验力学, 1992; 7: 351) |  
					| [24] | Zhou J H, Fu G L, Chen M H, Zhang Z Y, Zhao D P. J Data Acquis Process, 1996; 11(1): 69 |  
					|  | (周建华, 傅桂龙, 陈明和, 张中元, 赵大朋. 数据采集与处理, 1996; 11(1): 69) |  
					| [25] | Chan K C, Chow K K. Int J Mech Sci, 2002; 44: 1467 |  
					| [26] | Jeyasingh J J V, Kothandaraman G, Sinha P P, Rao B N, Reddy A C. Chennakesava R A. Mater Sci Eng, 2008; A478: 397 |  
					| [27] | Song Y Q, Ma P K, Guan Z P. Acta Metall Sin, 2010; 46: 1 |  
					|  | (宋玉泉, 马品奎, 管志平. 金属学报, 2010; 46: 1) |  
					| [28] | Tsai R Y. IEEE Trans Robot Autom, 1987; 3: 323 |  
					| [29] | Zhang Z Y. IEEE Trans Pattern Anal Mach Intell, 2000; 22: 1330 |  
             
								                
															
																| 
																																																																									
																				| No Suggested Reading articles found! |  |  
             
												
											    	
											        	|  | Viewed |  
											        	|  |  |  
												        |  | Full text 
 | 
 
 |  
												        |  |  |  
												        |  | Abstract 
 | 
 |  
												        |  |  |  
												        |  | Cited |  |  
												        |  |  |  |  
													    |  | Shared |  |  
													    |  |  |  |  
													    |  | Discussed |  |  |  |  |