| STUDY ON KINETICS OF PRECIPITATION IN Al—0.6Mg—0.9Si—0.2Cu ALLOY FOR AUTOMOTIVE APPLICATION |
| ZHANG Qiaoxia, GUO Mingxing, HU Xiaoqian, CAO Lingyong, ZHUANG Linzhong, ZHANG Jishan |
| State Key Laboratory for Advanced Metals and Materials, University of Science and Technology Beijing, Beijing 100083 |
|
Cite this article:
ZHANG Qiaoxia, GUO Mingxing, HU Xiaoqian, CAO Lingyong, ZHUANG Linzhong, ZHANG Jishan. STUDY ON KINETICS OF PRECIPITATION IN Al—0.6Mg—0.9Si—0.2Cu ALLOY FOR AUTOMOTIVE APPLICATION. Acta Metall Sin, 2013, 49(12): 1604-1610.
|
|
|
Abstract The kinetics of precipitation in Al—0.6Mg—0.9Si—0.2Cu (mass fraction, %) alloy under different conditions was investigated by differential scanning calorimetric analyses (DSC) and microhardness measurements. The results show that, an exothermic peak at about 100—-150℃ can be observed in the DSC curve for the nature aged (T4) alloy, but no peak for the pre—aged (T4P) alloy, and the peak corresponding with β″ phase moves toward the low temperature zone for T4P alloy. The fraction of transformation Y, the rate of transformation dY/dT, and the kinetic parameters such as activation energy Q and frequency factor k0 for GP zones dissolution and β″phase transformation were calculated by Avrami—Johnson—Mehl equation. The values of activation energy for GP zones dissolution after natural aging and pre—aging were 66 and 119 kJ/mol, respectively, and the values forβ″phase formation after natural aging and pre—aging were 114 and 60 kJ/mol, respectively. The kinetics expressions were obtained as follows, for T4 alloy:YGP=1-exp[-1.3×107t exp(-7977/T)],Yβ″=1-exp[-4.7×1022t2 exp(-27484/T)];for T4P alloy: YGP=1-exp[-2.4×1013 t exp(-14345/T)],Yβ″=1-exp[-2.9×1011t2 exp(-14392/T)].In addition, with the increasing of aging time, the wholetrend of hardness changing for pre—aged alloy is increasing at first, and then keeps constant basically,but for the nature aged alloy, the hardness decreases after aging at 185℃ for 20 min, which was explained by the kinetics obtained above.
|
|
Received: 17 June 2013
|
| [1] Miller W S, Zhuang L, Bottema J, Wittebrood A J, De Smet P, Haszler A,Vieregge A. Mater Sci Eng, 2000; A280: 37
[2] Birol Y, Karlik M. Scr Mater, 2006; 55: 625
[3] Birol Y. Mater Sci Eng, 2005; A391:175
[4] Liu H, Chen Y, Zhao G, Liu C M, Zuo L. Trans Nonferrous Met Soc China, 2006; 16: 917
[5] Zhen L, Kang S B. Scr Mater, 1997; 36: 1089
[6] Ou B L, Shen C H. Scand J Metall, 2005; 34: 318
[7] Esmaeili S, Lloyd D J. Acta Mater, 2005; 53: 5257
[8] Wei F, Li J S, Chen C Q. Rare Met Mater Eng, 2008; 37: 1348
(魏芳, 李金山, 陈昌麒. 稀有金属材料与工程, 2008; 37: 1348)
[9] Gupta A K, Jena A K, Chaturvedi M C. Scr Metall, 1988; 22: 369
[10] Ghosh K S, Gao N. Trans Nonferrous Met Soc China, 2011; 21: 1199
[11] Oguocha I N A, Yannacopoulos S. Mater Sci Eng, 1997; A231: 25
[12] Edwards G A, Stiller K, Dunlop G L, Couper M J. Acta Mater, 1998; 46: 3893
[13] De Geuser F, Lefebvre W, Blavette D. Philos Mag Lett, 2006; 86: 227
[14] Zhen L, Kang S B, Kim H W. Mater Sci Technol, 1997; 13: 905
[15] Murayama M, Hono K. Acta Mater, 1999; 47: 1537
[16] Miao W F, Laughlin D E. Metall Mater Trans, 2000; 31A: 361
[17] Esmaeili S, Lloyd D J. Mater Charact, 2005; 55: 307
[18] An Y G, Zhang L, Vegter H, Hurkmans A. Metall Mater Trans, 2002; 33A: 3121
[19] Luo A, Lloyd D J, Gupta A, Youdelis W V. Acta Metall Mater, 1993; 41: 769
[20] Ortega A. Thermochim Acta, 1996; 284: 379
[21] Matsuda K, Naoi T, Fujii K, Uetani Y, Sato T, Kamio A, Ikeno S. Mater Sci Eng, 1999;A262: 232
[22] Chakrabarti D J, Laughlin D E. Prog Mater Sci, 2004; 49: 389
[23] Gaber A, Ali A M, Matsuda K, Kawabata T, Yamazaki T, Ikeno S. J Alloys Compd, 2007;432: 149
[24] Cuniberti A, Tolley A, Riglos M V, Giovachini R. Mater Sci Eng, 2010; A527: 5307
[25] Buha J, Lumley R N, Crosky A G, Hono K. Acta Mater, 2007; 55: 3015
[26] Galwey A K, Brown M E. Handbook of Thermal Analysis and Calorimetry. Amsterdam: Elesvier, 1998: 147 |