| [1] Curtze S, Kuokkala V T, Hokka M, Peura P. Mater Sci Eng, 2009; A507: 124 [2] Huh H, Lim J H, Park S H. Int J Auto Tech-Kor, 2009; 10(2): 195 [3] Khan A S, Baig M, Choi S H, Yang H S, Sun X. Int J Plast, 2012; 30-31: 1 [4] Ma M T, Yi H L, Lu H Z, Wan X M. Eng Sci, 2009; 11(9): 20 (马鸣图, 易红亮, 路洪洲, 万鑫铭. 中国工程科学, 2009; 11(9): 20) [5] Maggi S, Murgia M. Weld Int, 2008; 22: 610 [6] Reisgen U, Schleser M, Mokrov O, Ahmed E. J Mater Process Technol, 2010; 210: 2188 [7] Yu H D, Guo Y J, Lai X M. Mater Des, 2009; 30: 2501 [8] Wang H Y, Chen J Y. Lightweight Structure of Autobody and Lightweight Material. Beijing: Peking University Press, 2009: 20 (王宏雁, 陈军毅. 汽车车身轻量化结构与轻质材料. 北京: 北京大学出版社, 2009: 20) [9] Singh N K, Cadoni E, Singha M K, Gupta N K. Mater Des, 2011; 32: 5091 [10] Wei X C, Fu R Y, Li L. Mater Sci Eng, 2007; A465: 260 [11] Oliver S, Jones T B, Fourlaris G. Mater Charact, 2007; 58: 390 [12] Boyce B L, Dilmore M F. Int J Impact Eng, 2009; 36: 263 [13] Huh H, Kim S B, Song J H, Lim J H. Int J Mech Sci, 2008; 50: 918 [14] Smerd R, Winkler S, Salisbury C, Worswick M, Lloyd D, Finn M. Int J Impact Eng, 2005; 32: 541 [15] Ishikawa K, Watanabe H, Mukai T. Mater Lett, 2005; 59: 1511 [16] Odeshi A G, Al-ameeri S, Bassim M N. J Mater Process Technol, 2005; 162-163: 385 [17] Gong X, Fan J L, Huang B Y, Tian J M. Mater Sci Eng, 2010; A527: 7565 [18] Ludwik P. Physics, 1909; 10Z: 411 [19] Hollomon J H. Trans ASM, 1944; 32: 123 [20] Plumbridge W J. J Mater Sci, 1996; 31: 2501 [21] Castany P, Pettinari-Sturmel F, Crestou J, Douin J, Coujou A. Acta Mater, 2007; 55: 6284 [22] Walgraef D. Mater Sci Eng, 2010; A322: 167 [23] Johnston W G, Gilman J J. J Appl Phys, 1959; 30: 129 [24] Meyers M A, translated by Zhang Q M, Liu Y, Huang F L, Lu Z J. Dynamic Behavior of Materials. Beijing: National Defense Industry Press, 2006: 225 (Meyers M A著, 张庆明, 刘彦, 黄风雷, 吕中杰译. 材料的动力学行为. 北京: 国防工业出版社, 2006: 225) [25] Rajeev K, Sia N N. Metall Mater Trans, 2000; 31A: 815 [26] Liu Y, Wang L, He S S, Feng F, Lu X D, Zhang B J. Acta Metall Sin, 2012; 48: 49 (刘杨, 王磊, 何思斯, 冯飞, 吕旭东, 张北江. 金属学报, 2012; 48: 49) [27] Liu J T, Wang Z G, Shang J K. Acta Metall Sin, 2008; 44: 1409 (刘江涛, 王中光, 尚建库. 金属学报, 2008; 44: 1409) [28] Liu Z L, You X C, Zhuang Z. Int J Solids Struct, 2008; 45: 3674 [29] Livingston J D, Chalmers B. Acta Mater, 1957; 5: 322 [30] Rajeev K, Sia N N. Mech Mater, 1998; 27(1): 1 [31] Tang C G, Zhu J H, Zhou H J. Chin J Mater Res, 1996; 10: 19 (唐长国, 朱金华, 周惠久. 材料研究学报, 1996; 10: 19) [32] Rusinek A, Klepaczko J R. Mater Des, 2009; 30(1): 35 |