| PROCESSING, MICROSTRUCTURE AND MECHANICAL PROPERTIES OF LARGE DIRECTIONALLY SOLIDIFIED CASTINGS FOR INDUSTRIAL GAS TURBINE APPLICATIONS |
| ZHANG Jian, SHEN Jian, LU Yuzhang, LOU Langhong |
| Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016 |
|
Cite this article:
ZHANG Jian SHEN Jian LU Yuzhang LOU Langhong. PROCESSING, MICROSTRUCTURE AND MECHANICAL PROPERTIES OF LARGE DIRECTIONALLY SOLIDIFIED CASTINGS FOR INDUSTRIAL GAS TURBINE APPLICATIONS. Acta Metall Sin, 2010, 46(11): 1322-1326.
|
|
|
Abstract Contamination of low melting point metal and distortion and fracture of ceramic shell during directional solidification assisted by liquid metal cooling (LMC) were discussed. Large DS castings with 430 mm in length were produced by optimizing the processing parameters. The microstructure, heat treatment response and typical creep rupture properties of the large casting were analyzed. Results of the preliminary casting trials of large blades were also reported.
|
|
Received: 27 September 2010
|
| Fund: Supported by National Natural Science Foundation of China (No.{\footnotesize\it 50931004}), National Basic Research Program of China (No. 2010CB631201) and National High Technology Research and Development Program of China (No.2008AA05A302) |
| [1] Seth B B. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, Mclean M, Olson S, Schirra J J, eds., Superalloys 2000, Warrendale, PA: TMS, 2000: 3
[2] Konter M, Thumann M. J Mater Proc Technol, 2001; 117: 386
[3] Zhang J, Lou L H. J Mater Sci Technol, 2007; 23: 289
[4] Lohmueller A, EsserW, Grossmann J, Hoerdler M, Preuhs J, Singer R F. In: Pollock T M, Kissinger R D, Bowman R R, Green K A, Mclean M, lson S, Schirra J J, eds., Superalloys 2000, Warrendale, PA: TMS, 2000: 181
[5] Tang W S, Shen J, Zhang J, Chen L J. J Shenyang Univ Technol, 2009; 31: 397
(唐文书, 申 健, 张 健, 陈立佳. 沈阳工业大学学报, 2009; 31: 397) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|