| BEHAVIOR OF CERIUM IN GRAIN BOUNDARY SEGREGATION AND ITS INFLUENCE ON EQUILIBRIUM SEGREGATION OF PHOSPHORUS AT GRAIN BOUNDARIES IN α-IRON |
| ZHANG Dongbin Beijing University of Iron and Steel Technology WU Chengjian Department of Materials Science;Beijing University of Iron and Steel Technology |
|
Cite this article:
ZHANG Dongbin Beijing University of Iron and Steel Technology WU Chengjian Department of Materials Science;Beijing University of Iron and Steel Technology. BEHAVIOR OF CERIUM IN GRAIN BOUNDARY SEGREGATION AND ITS INFLUENCE ON EQUILIBRIUM SEGREGATION OF PHOSPHORUS AT GRAIN BOUNDARIES IN α-IRON. Acta Metall Sin, 1988, 24(2): 100-105.
|
|
|
Abstract The equilibrium intergranular segregation of Ce and P in α-Fehas been analyzed by employing the combination of TEM+EDAX and AES. Theeffect of Ce on the equilibrium segregation of P and the embrittlement of the alloyshas also been studied in detail. The results show that there is cosegregation of Ceand P at the grain boundaries in Fe-0.3%P-0.16%Ce alloy. The addition of Ce doesnot decrease the equilibrium segregation of P, but significantly lowers the ductile-brittle transition temperature. The interaction between Ce and P at grain bounda-ries was discussed from the point of the interfacial two-dimensional phase.
|
|
Received: 18 February 1988
|
1 袁泽喜,李景慧,冯松筠,吴承建.北京钢铁学院学报,1982;增刊2:42 2 余宗森,褚幼义,贺信莱,杜国维,高佩钰,朱逢吾.钢中稀士,冶金工业出版社,1982:132 3 邱巨峰.稀土,1983;4:58 4 谷野满.日本金属学会会报,1983;22:653 5 Doig P, Flewitt P E J. J Microsc, 1978; 112: 257 6 Doig P, Flewitt P E J, Wild R K. Philos Mag A, 1978; 37: 759 7 任允蓉,金建灵,李晓风.电子显微镜学报,1983;3:15 8 张东彬.硕士学位论文,北京钢铁学院,1984 9 Hondros E D, Seah M P. Int Metall Rev, 1977; 22: 262 10 McLean D, Grain Brundaries in Metals, Oxford University Press, 1957: 101 11 Davis L E, McDonald N C, Palmberg P W. Riach E, Weber R E. Handbook of Anger Electron Spectroscopy, 2nd ed. physical Electronics Industries, Edina, MN, 1976 12 Guttmann M, Mclean D. In: Johnson W C, Blakely J M eds. Interfacial Segregation, Ohio: Metals Park ASM. 1979: 261 13 安彦兼次,铃木茂,木村宏.铁钢,1983;69:625 14 汤晓丽.硕士学位论文,北京钢铁学院,1985 |