DISTRIBUTION OF HYDROGEN ATOMS IN HYDRIDES OF METALLIC GLASS TiCu AND Zr_(3.12)Ni
CHEN Jizhou;WANG Junqiao;YE Xuxin Tianjin Institute of Technology; Tianjin Institute of Chemical Engineering Materi als Research Center Tianjin Institute of Technology; Tianjin
Cite this article: 

CHEN Jizhou;WANG Junqiao;YE Xuxin Tianjin Institute of Technology; Tianjin Institute of Chemical Engineering Materi als Research Center Tianjin Institute of Technology; Tianjin. DISTRIBUTION OF HYDROGEN ATOMS IN HYDRIDES OF METALLIC GLASS TiCu AND Zr_(3.12)Ni. Acta Metall Sin, 1988, 24(3): 267-272.

Download:  PDF(496KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The changes in the reduced radial distribution function of metallicglasses TiCu and Zr_(3.12)Ni before and after hydriding have been measured using thewide-angle X-ray scattering. It is shown that if hydrogen atoms mainly occupy thetetrahedral interstices defined by four Ti or Zr atoms, the displacement of the firstpeak can be interpreted quantitatively. Broad peaks with approximate periodicity atlarger r range is also discussed.
Key words:  metallic glass      TiCu      Zr_(3.12)Ni      hydride      radial distribution function     
Received:  18 March 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I3/267

1 Maeland A J. In: Barnbakidis G ed., Metal Hydrides, New York: Plenum, 1981: 177
2 Suzuki K. J Less-Common Met, 1983; 89: 183
3 Samwer K, Johnson W L. Phys Rev B, 1983; 28(6) : 2907
4 陈济舟,叶绪莘,王俊桥.计算机与应用化学,1988;5(1) :31
5 陈济舟,韩甫田,伍宣池.分析测试通报,1987;6(5) :56
6 陈济舟,王俊桥,蒋世承.中国科学,B辑,1985;28(1) :16-
[1] SUN Xiaojun, HE Jie, CHEN Bin, ZHAO Jiuzhou, JIANG Hongxiang, ZHANG Lili, HAO Hongri. Effect of Fe Content on the Microstructure, Electrical Resistivity, and Nanoindentation Behavior of Zr60Cu40-xFex Phase-Separated Metallic Glasses[J]. 金属学报, 2021, 57(5): 675-683.
[2] BI Jiazi, LIU Xiaobin, LI Ran, ZHANG Tao. Tribological Properties of Polyalphaolefin (PAO6) Lubricant Modified with Particles Additives of Metallic Glass[J]. 金属学报, 2021, 57(4): 559-566.
[3] GUAN Pengfei, SUN Shengjun. Atomic-Level Study in the Structure and Its Instability of Metallic Glasses[J]. 金属学报, 2021, 57(4): 501-514.
[4] ZENG Qiaoshi, YIN Ziliang, LOU Hongbo. Polyamorphic Transitions in Metallic Glasses[J]. 金属学报, 2021, 57(4): 491-500.
[5] ZHANG Nizhen, MA Xindi, GENG Chuan, MU Yongkun, SUN Kang, JIA Yandong, HUANG Bo, WANG Gang. Effect of Adding Ag on the Nanoindentation Behavior of Cu-Zr-Al-Based Metallic Glass[J]. 金属学报, 2021, 57(4): 567-574.
[6] PAN Jie, DUAN Fenghui. Rejuvenation Behaviors in Metallic Glasses[J]. 金属学报, 2021, 57(4): 439-452.
[7] CAO Qingping, LV Linbo, WANG Xiaodong, JIANG Jianzhong. Magnetron Sputtering Metal Glass Film Preparation and the “Specimen Size Effect” of the Mechanical Property[J]. 金属学报, 2021, 57(4): 473-490.
[8] QU Ruitao, WANG Xiaodi, WU Shaojie, ZHANG Zhefeng. Research Progress in Shear Banding Deformation and Fracture Mechanisms of Metallic Glasses[J]. 金属学报, 2021, 57(4): 453-472.
[9] YANG Qun, PENG Sixu, BU Qingzhou, YU Haibin. Revealing Glass Transition and Supercooled Liquid in Ni80P20 Metallic Glass[J]. 金属学报, 2021, 57(4): 553-558.
[10] LI Ning, HUANG Xin. Recent Advances on 3D Printed Bulk Metallic Glasses[J]. 金属学报, 2021, 57(4): 529-541.
[11] JIANG Minqiang, GAO Yang. Structural Rejuvenation of Metallic Glasses and Its Effect on Mechanical Behaviors[J]. 金属学报, 2021, 57(4): 425-438.
[12] HUANG Huogen, ZHANG Pengguo, ZHANG Pei, WANG Qinguo. Comparison of Glass Forming Ability Between U-Co and U-Fe Base Systems[J]. 金属学报, 2020, 56(6): 849-854.
[13] YANG Gaolin, LIN Xin, LU Xiangang. Crystallization Morphology and Evolution Mechanism of Laser Multiple Remelting of Zr55Cu30Al10Ni5 Metallic Glass[J]. 金属学报, 2019, 55(12): 1544-1550.
[14] Yanchun ZHAO, Hao SUN, Chunling LI, Jianlong JIANG, Ruipeng MAO, Shengzhong KOU, Chunyan LI. High Temperature Deformation Behavior of High Strength and Toughness Ti-Ni Base Bulk Metallic Glass Composites[J]. 金属学报, 2018, 54(12): 1818-1824.
[15] Weihua WANG, Peng LUO. The Dynamic Behavior Hidden in the Long Time Scale of Metallic Glasses and Its Effect on the Properties[J]. 金属学报, 2018, 54(11): 1479-1489.
No Suggested Reading articles found!