| ACTIVITIES OF CaO AND La_2O_3 IN LIQUID CaO-SiO_2-La_2O_3 SLAGS AND SLAG STRUCTURE |
| WU Jianzhong;WANG Changzhen Northeast University of Technology; ShenyangProfessor;Dept.Non-ferrous Metallurgy;Northeast University of Technology; Shenyang |
|
Cite this article:
WU Jianzhong;WANG Changzhen Northeast University of Technology; ShenyangProfessor;Dept.Non-ferrous Metallurgy;Northeast University of Technology; Shenyang. ACTIVITIES OF CaO AND La_2O_3 IN LIQUID CaO-SiO_2-La_2O_3 SLAGS AND SLAG STRUCTURE. Acta Metall Sin, 1988, 24(4): 299-304.
|
|
|
Abstract The activity of CaO and La_2O_3 in the liquid ternary slag CaO-SiO-La_2O_3 has been determined by equilibrating Sn with the slag phase in a graphitecrucible under 1 atm of CO at 1600℃. The experimental results showed that theactivity of CaO and La_2O_3 changes slowly while the ratio of mole fraction, x_(CaO)/x_(SiO_2), is less than unit, but varies sharply while the ratio increases from 1 to 1.2.In addition, by equilibrating Sn with the binary slag B_2O_3-La_2O_3 saturated with solidLa_2O_3 at three different temperatures, the relation between lg γ°_(La) and 1/T isdetermined as follows: lg γ°_(La)=-29400/T+11.37(1500-1600℃) A random network model of molten silicate structure was applied to CaO-SiO-La_2O_3. It was found that the experimentally determined activity-composition curvesof CaO are qualitatively reproduced by the curves calculated with the model, butthe curves of La_2O_3 are considerably different from the calculated ones. It impliesthat the model used is over-simplified and that the difference in interaction energybetween the metal cations of different valence and silicate anions should be consid-ered.
|
|
Received: 18 April 1988
|
1 张庆登,周祖惠.稀士,1982;(3) :34 2 王渭源,邹元爔.金属学报,1963;6:40 3 王常珍,邹元爔.金属学报,1980;16:190 4 王常珍,叶树青,于丁羽,郭文全.金属学报,1984;20:A357 5 Levin E M, Robbins CBR, McMurdie H F. In: Reser M K ed., Phase Diagrams for Ceramists, Supplement, The American Ceramic Society, 1969: Fig. 237. Fig. 2299. Fig. 2372 6 郭祝崑,CaSiO_3-La_2O_3伪二元相图,(未发表) 7 王常珍,杨代银.金属学报,1979;15:433 8 张子青,周继程,田彦文等.全国第5届冶金过程物理化学年会论文集,上册,西安,中国金属学会冶金物理化学学术委员会,1984:254 9 Gschneidner K A Jr., Kippenhan N, NcMasters O D. Thermochemistry of the Rare Earths, Amesl Iowa: Rare Earth Infoimation Center, Institute for Atomic Research, 1973: 25 10 Fincham C J B, Richarason F D. Proc Roy Soc, London, 1954: A223: 40 11 Yokokawa t, Niwa K. Trans Jpn Inst Met, 1969; 10: 3 12 Yokokawa T, Niwa K. Trans Jpn Inst Met, 1969; 10: 81 13 Lin P L Pelton A D. Metall Tians, 1979; 10B: 667 |