Please wait a minute...
Acta Metall Sin  1988, Vol. 24 Issue (4): 299-304    DOI:
Current Issue | Archive | Adv Search |
ACTIVITIES OF CaO AND La_2O_3 IN LIQUID CaO-SiO_2-La_2O_3 SLAGS AND SLAG STRUCTURE
WU Jianzhong;WANG Changzhen Northeast University of Technology; ShenyangProfessor;Dept.Non-ferrous Metallurgy;Northeast University of Technology; Shenyang
Cite this article: 

WU Jianzhong;WANG Changzhen Northeast University of Technology; ShenyangProfessor;Dept.Non-ferrous Metallurgy;Northeast University of Technology; Shenyang. ACTIVITIES OF CaO AND La_2O_3 IN LIQUID CaO-SiO_2-La_2O_3 SLAGS AND SLAG STRUCTURE. Acta Metall Sin, 1988, 24(4): 299-304.

Download:  PDF(451KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The activity of CaO and La_2O_3 in the liquid ternary slag CaO-SiO-La_2O_3 has been determined by equilibrating Sn with the slag phase in a graphitecrucible under 1 atm of CO at 1600℃. The experimental results showed that theactivity of CaO and La_2O_3 changes slowly while the ratio of mole fraction, x_(CaO)/x_(SiO_2), is less than unit, but varies sharply while the ratio increases from 1 to 1.2.In addition, by equilibrating Sn with the binary slag B_2O_3-La_2O_3 saturated with solidLa_2O_3 at three different temperatures, the relation between lg γ°_(La) and 1/T isdetermined as follows: lg γ°_(La)=-29400/T+11.37(1500-1600℃) A random network model of molten silicate structure was applied to CaO-SiO-La_2O_3. It was found that the experimentally determined activity-composition curvesof CaO are qualitatively reproduced by the curves calculated with the model, butthe curves of La_2O_3 are considerably different from the calculated ones. It impliesthat the model used is over-simplified and that the difference in interaction energybetween the metal cations of different valence and silicate anions should be consid-ered.
Key words:  ternary system of CaQ-SiO-La_2O_3      slag      slag structure      activity     
Received:  18 April 1988     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1988/V24/I4/299

1 张庆登,周祖惠.稀士,1982;(3) :34
2 王渭源,邹元爔.金属学报,1963;6:40
3 王常珍,邹元爔.金属学报,1980;16:190
4 王常珍,叶树青,于丁羽,郭文全.金属学报,1984;20:A357
5 Levin E M, Robbins CBR, McMurdie H F. In: Reser M K ed., Phase Diagrams for Ceramists, Supplement, The American Ceramic Society, 1969: Fig. 237. Fig. 2299. Fig. 2372
6 郭祝崑,CaSiO_3-La_2O_3伪二元相图,(未发表)
7 王常珍,杨代银.金属学报,1979;15:433
8 张子青,周继程,田彦文等.全国第5届冶金过程物理化学年会论文集,上册,西安,中国金属学会冶金物理化学学术委员会,1984:254
9 Gschneidner K A Jr., Kippenhan N, NcMasters O D. Thermochemistry of the Rare Earths, Amesl Iowa: Rare Earth Infoimation Center, Institute for Atomic Research, 1973: 25
10 Fincham C J B, Richarason F D. Proc Roy Soc, London, 1954: A223: 40
11 Yokokawa t, Niwa K. Trans Jpn Inst Met, 1969; 10: 3
12 Yokokawa T, Niwa K. Trans Jpn Inst Met, 1969; 10: 81
13 Lin P L Pelton A D. Metall Tians, 1979; 10B: 667
[1] ZHOU Xiaobin, ZHAO Zhanshan, WANG Wanxing, XU Jianguo, YUE Qiang. Physical and Mathematical Simulation on the Bubble Entrainment Behavior at Slag-Metal Interface[J]. 金属学报, 2023, 59(11): 1523-1532.
[2] JU Tianhua, SHU Nian, HE Wei, DING Xueyong. A Predicted Model for Activity Interaction Coefficient Between Solutes in Alloy Solutions[J]. 金属学报, 2023, 59(11): 1533-1540.
[3] Rongyao MA, Lin ZHAO, Changgang WANG, Xin MU, Xin WEI, Junhua DONG, Wei KE. Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion[J]. 金属学报, 2019, 55(2): 281-290.
[4] Qiang WANG, Lianyu WANG, Hongxia LI, Jiawei JIANG, Xiaowei ZHU, Zhancheng GUO, Jicheng HE. Suppression Mechanism and Method of Vortex During Steel Teeming Process in Ladle[J]. 金属学报, 2018, 54(7): 959-968.
[5] Zibing HOU,Jianghai CAO,Yi CHANG,Wei WANG,Han CHEN. Morphology Characteristics of Carbon Segregation in Die Steel Billet by ESR Based on Fractal Dimension[J]. 金属学报, 2017, 53(7): 769-777.
[6] Qing LI,Zixing WANG,Shuyuan XIE. Research on the Development of Mathematical Model of the Whole Process of Electroslag Remelting and the Process Simulation[J]. 金属学报, 2017, 53(4): 494-504.
[7] Xiaofeng LU, Ming XIAO, Yangmei CHEN, Bangcheng YANG. Bioactivity of Titanium Metal Hybridized with Inactivated Bacterial Biofilm[J]. 金属学报, 2017, 53(10): 1402-1412.
[8] Muqin LI, Haitao YAO, Fanghong WEI, Mingda LIU, Zan WANG, Shuhao PENG. The Microstructure and in Vivo and in Vitro Property of Multi-Component Composite Films on the Biomedical Pure Magnesium Surface[J]. 金属学报, 2017, 53(10): 1337-1346.
[9] Chuan HONG,Yunming GAO,Chuanghuang YANG,Zhibo TONG. ELECTROCHEMICAL BEHAVIOR OF Ni2+ IN SiO2-CaO-MgO-Al2O3 MOLTEN SLAG AT 1673 K[J]. 金属学报, 2015, 51(8): 1001-1009.
[10] Xiaoyan CHEN,Zhe JIN,Xuefeng BAI,Yizhou ZHOU,Tao JIN,Xiaofeng SUN. EFFECT OF C ON THE INTERFACIAL REACTION AND WETTABILITY BETWEEN A Ni-BASED SUPERALLOY AND CERAMIC MOULD[J]. 金属学报, 2015, 51(7): 853-858.
[11] Dongsong RONG,Yong JIANG,Jianming GONG. EXPERIMENTAL RESEARCH AND THERMODYNAMIC SIMULATION OF LOW TEMPERATURE COLOSSAL CARBURIZATION OF AUSTENITIC STAINLESS STEEL[J]. 金属学报, 2015, 51(12): 1516-1522.
[12] NI Zifei SUN Yangshan XUE Feng BAI Jing. STUDY ON FABRICATION, MICROSTRUCTURE AND PROPERTIES OF IN SITU TiC PARTICLE ON DISPERSION–STRENGTHENED 304 STAINLESS STEEL[J]. 金属学报, 2010, 46(8): 935-940.
[13] WANG Fang LI Baokuan. ANALYSIS OF ELECTROMAGNETIC FIELD AND JOULE HEATING OF ELECTROSLAG REMELTING PROCESSES[J]. 金属学报, 2010, 46(7): 794-799.
[14] YU Hai-Qi. The interfacial behavior of molten steel and liquid slag in a slab continuous casting mold with electromagnetic brake and argon gas injection[J]. 金属学报, 2008, 44(9): 1141-1148 .
[15] WU Ling. The improvement of regular solution model based on GA-NN and its application in binary slag system[J]. 金属学报, 2008, 44(7): 799-802 .
No Suggested Reading articles found!