MORPHOLOGY OF (Mn, Fe)S SINGLE CRYSTAL GROWTH IN CAST STEEL |
JIANG Xishan;GONG Yansheng;ZHANG Guichang Research Institute of Qiqihar Steel Plant; Qiqihar Heilongjiang |
|
Cite this article:
JIANG Xishan;GONG Yansheng;ZHANG Guichang Research Institute of Qiqihar Steel Plant; Qiqihar Heilongjiang. MORPHOLOGY OF (Mn, Fe)S SINGLE CRYSTAL GROWTH IN CAST STEEL. Acta Metall Sin, 1988, 24(4): 295-298.
|
Abstract The step pattern of single crystal growth and the morphology at equilbriiumstate of (Mn, Fe)S on the wall of micro-voids in ZG25 cast steel have been observed using scan-ning electron microscope. The face-centred cubic (Mn, Fe)S single crystal at equilibrium stateis shown to be tetrakaidecahedron consisted of eight {111} planes and six {100} planes, and isa typical example of the O_h-m3m cubic crystal system.
|