| A PARAMETER FOR EVALUATING ABILITY OF GRAIN REFINEMENT OF SOLUTE ELEMENTS |
| HAN Qingyou;HU Hanqi Beijing University of Iron and Steel Technology |
|
Cite this article:
HAN Qingyou;HU Hanqi Beijing University of Iron and Steel Technology. A PARAMETER FOR EVALUATING ABILITY OF GRAIN REFINEMENT OF SOLUTE ELEMENTS. Acta Metall Sin, 1988, 24(5): 392-396.
|
|
|
Abstract The gradient of the equilibrium melting temperature on liquid side ofadvancing solid-liquid interface has been derived. From it, a parameter, H, used forevaluating the ability of grain refinement of solute elements has been proposed.Experiments on Al-base alloys show that the grain size of alloys decrease withincreasing H value. This indicates that parameter H can be used as an index forselecting the grain refiners.
|
|
Received: 18 May 1988
|
1 胡汉起.金属凝固,冶金工业出版社,1985:89 2 Winegard W C, Chalmers B. Trans Am Soc Met, 1954; 46: 1214 3 Genolers R. J Inst Met, 1926; 35: 259 4 Papapetron A Z. Krist, 1935; A92: 89 5 大野笃美,唐彦斌,张正德译.金属凝固学,机械工业出版社,1983:88 6 韩青有,胡汉起.北京钢铁学院学报,1985;(1) :1 7 张兴中.溶质分配系数的研究,北京钢铁学院硕士研究生论文,1985 8 Smithells C J. Metals Reference Book, 5th ed., London: Butterworths, 1976 9 Rinaldi M D, Sharp R M, Flemings M C. Metall Trans. 1972; 3: 3133 10 胡汉起,钟雪友,力航.金属学报,1984;20:A247 11 胡汉起,钟雪友,韩青有,金属学报,1987;23:A176{ |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|