CARBIDES IN STEEL 4335 V
ZHONG Jiaxiang;ZHENG Xiuhua;XU Zongrui;BAI Dezhong Beijing University of Science and Engineering Nei Monggol Machine Works No.2
Cite this article: 

ZHONG Jiaxiang;ZHENG Xiuhua;XU Zongrui;BAI Dezhong Beijing University of Science and Engineering Nei Monggol Machine Works No.2. CARBIDES IN STEEL 4335 V. Acta Metall Sin, 1989, 25(1): 31-36.

Download:  PDF(2329KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Three kinds of alloy carbides have been observed in tempered steel4335V: M_3C, M_7C_3 and M_4C_3. The precipitation temperatures are 200--700℃,>400℃and>500℃ respectively. The compositions, morphologies and distribution of thecarbides as well as the relationship between them and the quenching substrutureshave been investigated. The influence of the carbides on the low temperature im-pact thoughness of the steel has also been discussed.
Key words:  Steel 4335V      carbide      tempering     
Received:  18 January 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I1/31

1 内蒙古金属材料研究所相分析组.金属材料与热加工工艺,1979;(1) :80
2 章守华.合金钢,北京:冶金工业出版社,1981
3 郭可信.金属学报,1957;2:303
4 Raynor D, Whiteman J A, Honeycombe R W K. J Iron Steel Inst, 1966; 204: 1114
5 Materkowski J P, Krauss G. Metall Trans, 1979; 10A: 1643
6 内蒙古金属材料研究所2019组.金属材料与热加工工艺,1980;(11) :11
7 Horn R M, Ritchie R O. Metall Trans, 1978; 9A: 1039
8 Sarikaya M, Steinberg B G, Thomas G. Metall Trans, 1982; 13A: 2227
9 Thomas G, Metall Trans, 1978; 9A: 439
10 钟家湘,张丽华,毛清奇.et.al.见:内蒙古金属材料研究所主编,炮钢系统分析会议论文汇编,1984:181
11 林宝军,孙文山,严志齐.金属材料与热加工工艺,1980;(11) :1
[1] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[2] LI Shanshan, CHEN Yun, GONG Tongzhao, CHEN Xingqiu, FU Paixian, LI Dianzhong. Effect of Cooling Rate on the Precipitation Mechanism of Primary Carbide During Solidification in High Carbon-Chromium Bearing Steel[J]. 金属学报, 2022, 58(8): 1024-1034.
[3] SHEN Guohui, HU Bin, YANG Zhanbing, LUO Haiwen. Influence of Tempering Temperature on Mechanical Properties and Microstructures of High-Al-Contained Medium Mn Steel Having δ-Ferrite[J]. 金属学报, 2022, 58(2): 165-174.
[4] ZHOU Cheng, ZHAO Tan, YE Qibin, TIAN Yong, WANG Zhaodong, GAO Xiuhua. Effects of Tempering Temperature on Microstructure and Low-Temperature Toughness of 1000 MPa Grade NiCrMoV Low Carbon Alloyed Steel[J]. 金属学报, 2022, 58(12): 1557-1569.
[5] HE Shuwen, WANG Minghua, BAI Qin, XIA Shuang, ZHOU Bangxin. Effect of TaC Content on Microstructure and Mechanical Properties of WC-TiC-TaC-Co Cemented Carbide[J]. 金属学报, 2020, 56(7): 1015-1024.
[6] WANG Zhanhua, HUI Weijun, XIE Zhiqi, ZHANG Yongjian, ZHAO Xiaoli. Effects of Tempering Temperature on Microstructure and Mechanical Properties of a Mn-Cr Type Bainitic Forging Steel[J]. 金属学报, 2020, 56(11): 1441-1451.
[7] YANG Ke,LIANG Ye,YAN Wei,SHAN Yiyin. Preferential Distribution of Boron and its Effect on Microstructure and Mechanical Properties of (9~12)%Cr Martensitic Heat Resistant Steels[J]. 金属学报, 2020, 56(1): 53-65.
[8] LI Jiarong,XIE Hongji,HAN Mei,LIU Shizhong. High Cycle Fatigue Behavior of Second Generation Single Crystal Superalloy[J]. 金属学报, 2019, 55(9): 1195-1203.
[9] Futao DONG,Fei XUE,Yaqiang TIAN,Liansheng CHEN,Linxiu DU,Xianghua LIU. Effect of Annealing Temperature on Microstructure, Properties and Hydrogen Embrittlement of TWIP Steel[J]. 金属学报, 2019, 55(6): 792-800.
[10] HUANG Yu, CHENG Guoguang, LI Shijian, DAI Weixing. Precipitation Mechanism and Thermal Stability of Primary Carbide in Ce Microalloyed H13 Steel[J]. 金属学报, 2019, 55(12): 1487-1494.
[11] ZHANG Min,JIA Fang,CHENG Kangkang,LI Jie,XU Shuai,TONG Xiongwei. Influence of Quenching and Tempering on Microstructure and Properties of Welded Joints of G520 Martensitic Steel[J]. 金属学报, 2019, 55(11): 1379-1387.
[12] Tao ZHANG, Wei YAN, Zhuoming XIE, Shu MIAO, Junfeng YANG, Xianping WANG, Qianfeng FANG, Changsong LIU. Recent Progress of Oxide/Carbide Dispersion Strengthened W-Based Materials[J]. 金属学报, 2018, 54(6): 831-843.
[13] Shenghu CHEN, Lijian RONG. Microstructure Evolution During Solution Treatment and Its Effects on the Properties of Ni-Fe-Cr Alloy[J]. 金属学报, 2018, 54(3): 385-392.
[14] Xirong LIU, Kai ZHANG, Shuang XIA, Wenqing LIU, Hui LI. Effects of Triple Junction and Grain Boundary Characters on the Morphology of Carbide Precipitation in Alloy 690[J]. 金属学报, 2018, 54(3): 404-410.
[15] Xiaolin LI, Yang CUI, Baoliang XIAO, Dawei ZHANG, Zhao JIN, Zheng CHENG. Effects of On-Line Rapid Induction Tempering on Pricipitation Strengthening Mechanism of V(C, N) in V-N Microalloyed Steel[J]. 金属学报, 2018, 54(10): 1368-1376.
No Suggested Reading articles found!