RULE OF SEGREGATION OF ALLOYING ELEMENTS IN CAST Ni-BASE SUPERALLOYS
QIU Yiming;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang
Cite this article:
QIU Yiming;ZHU Yaoxiao Institute of Metal Research; Academia Sinica; Shenyang. RULE OF SEGREGATION OF ALLOYING ELEMENTS IN CAST Ni-BASE SUPERALLOYS. Acta Metall Sin, 1989, 25(1): 78-80.
Abstract An investigation was made on the Possibility of using Ni-x binary diagram to ju-dge the positive, negative segregation or almost no segregation and degree of segregation of alloyingelement x in cast Ni-base superalloys. The prejudicat coincides with the experimental data.
1 Williams Dr, Moffatt G. The Handbook of Binary Phase Diagrams, New York: the General Electric Company, 1978 2 郑运荣,金属材料研究,1985;11(6) :26 3 金柱,马实基.金属学报,1974;10:1