| SOLUBILITY OF Ca IN Mn AND INTERACTION COEFFICIENTS OF Al AND Fe ON Ca IN Mn AT 1350℃ |
| NI Ruiming;CHENG Wu;WEI Shoukun Beijing University of Science and Technology Manuscript received 9 March; 1988 |
|
Cite this article:
NI Ruiming;CHENG Wu;WEI Shoukun Beijing University of Science and Technology Manuscript received 9 March; 1988. SOLUBILITY OF Ca IN Mn AND INTERACTION COEFFICIENTS OF Al AND Fe ON Ca IN Mn AT 1350℃. Acta Metall Sin, 1989, 25(1): 81-85.
|
|
|
Abstract Solubility of Ca in manganese and manganese alloys was measured un-der sealed conditions at 1350℃. The interaction coefficients of Al and Fe on Cain Mn were evaluated with the experimental data. The standard free energy ofliquid Ca in liquid manganese based on thel wt-%. solution standard was estimatedas well.
|
|
Received: 18 January 1989
|
1 魏寿昆,倪瑞明,方克明,成武,张昱,钢铁,1985;20(8) :67 2 倪瑞明,成武,魏寿昆,第六届冶金过程物理化学学术会议论文集(上册),重庆,1986:157 3 Schenck H,Frohberg M G,Steinmetz E.Arch Eisenhuettenwes,1960;31:671;另见魏寿昆·活度在冶金物理化学中的应用,北京:中国工业出版社,1964:9 |