IMPROVEMENT OF ADHESION BETWEEN ION PLATED TiN COATING AND BASE METAL BY ADDING Y |
JIN Zhujing;YU Li;DAI Shaoxia;YU Zhiming Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang |
|
Cite this article:
JIN Zhujing;YU Li;DAI Shaoxia;YU Zhiming Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang. IMPROVEMENT OF ADHESION BETWEEN ION PLATED TiN COATING AND BASE METAL BY ADDING Y. Acta Metall Sin, 1989, 25(1): 135-140.
|
Abstract The adhesion between the ion plated TiN coating and the base metalis improved by adding Y. By means of SEM, EPMA and X-ray diffraction analy-sis, the behaviour of Y in coating has been studied. The machenism of the effectof Y has been discussed as well.
|
Received: 18 January 1989
|
1 冲猛雄,金柱京,川出義之,沢田吉裕.金属表面技术协会第65届学术讲演会论文集,(日本).1982:96 2 Jacobson B E. Nimmagadda R. Bunshah R F. Thin Solid Films, 1979; 63: 333 3 Jin Zhujing (金柱京), Yu Li (于力), Dai Shaoxia (戴少侠), Yu Zhiming (于志明). Shenyang Int Conf on Physical Vapour Deposition, Shenyang, China, 1987: 28 4 金柱京,于力,于志明,戴少侠.中国真空学会编,第一届全国PVD会议论文集,长沙,1986:(No.)34 5 姜辛.中国科学院金属研究所硕士学位论文,1986 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|