DETERMINATION OF ACTIVITY OF Al IN SOLID Cu-Al ALLOYS |
ZHANG Qianxian University of science and Technology Beijing |
|
Cite this article:
ZHANG Qianxian University of science and Technology Beijing. DETERMINATION OF ACTIVITY OF Al IN SOLID Cu-Al ALLOYS. Acta Metall Sin, 1989, 25(2): 149-151.
1 Wilder T C. TMS AIME, 1965; 223: 1202--1207 2 Hansen M, Anderko K. Constitution of Binary Alloys, 2nded, New York: McGraw-Hill, 1958 3 Wagner J B, Wagner C. J Chem Phys, 1957; 26: 1602--1606 4 Alcock B, Belfoard T N. Trans Faraday Soc, 19?4; 60: 833--835 5 Ramanarayanan T A. In: Hagenmuller P, Van Gool W eds., Solid Eletrolyte, New York: Academic Press, 1978: 81--9 |