DEFORMAION AND WORK HARDENING OF HADFIELD MANGANESE STEEL
SHI Deke;LIU Junhai X'ian Jiaotong University
Cite this article: 

SHI Deke;LIU Junhai X'ian Jiaotong University. DEFORMAION AND WORK HARDENING OF HADFIELD MANGANESE STEEL. Acta Metall Sin, 1989, 25(4): 142-145.

Download:  PDF(1005KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Work hardening of Hadfield manganese steel is mainly from twocauses: 1) a large amount of twinning makes perfect dislocal is or shockley dislo-cations to be blocked up at the coherent twin boundaries. 2) deformation leads tostrong unsymmetrical distortion due to a large number of Mn-C pairs or Mn-vaca-ncy carbon-carbon clusters. It has been demonstrated by TEM observation and in-ternal friction tests. As deformation proceeds, slip constantly accommodates twin-hing shear giving rise to stress relaxation. Thus, Hadfield steel possesses both rapidwork hardening and good ductility.
Key words:  twin      work hardening      dislocation     
Received:  18 April 1989     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1989/V25/I4/142

1 White C H, Honeycombe R W K. J Iron Steel Inst, 1962; 200: 457
2 Roberts W N. TMS-AIME, 1964; 230: 372
3 Raghavan K S, Sastri A S, Mareinkowski M J. TMS-AIME, 1969; 245: 1569
4 Dastur Y N, Leslie W C. Metall Trans, 1981; 12A: 749
5 Adler P H, Olson G B, Owen W S. Metall Trans, 1986; 17A: 1725
6 石德珂,刘军海.待发表
7 王其闵,谢成刚.中国科学A辑,1986;11:1189
8 Cahn J W. Acta Metall, 1977; 25: 1021
9 Sleeswyk A W, Verbraak C A. Acta Metall, 1961; 9: 917
10 Remy L. Metall Trans, 1981; 12A: 38
[1] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[2] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[3] ZHANG Zhefeng, LI Keqiang, CAI Tuo, LI Peng, ZHANG Zhenjun, LIU Rui, YANG Jinbo, ZHANG Peng. Effects of Stacking Fault Energy on the Deformation Mechanisms and Mechanical Properties of Face-Centered Cubic Metals[J]. 金属学报, 2023, 59(4): 467-477.
[4] SHAO Xiaohong, PENG Zhenzhen, JIN Qianqian, MA Xiuliang. Unravelling the {101¯2} Twin Intersection Between LPSO Structure/SFs in Magnesium Alloy[J]. 金属学报, 2023, 59(4): 556-566.
[5] WAN Tao, CHENG Zhao, LU Lei. Effect of Component Proportion on Mechanical Behaviors of Laminated Nanotwinned Cu[J]. 金属学报, 2023, 59(4): 567-576.
[6] HAN Weizhong, LU Yan, ZHANG Yuheng. Mechanism of Ductile-to-Brittle Transition in Body-Centered-Cubic Metals:A Brief Review[J]. 金属学报, 2023, 59(3): 335-348.
[7] HAN Dong, ZHANG Yanjie, LI Xiaowu. Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies[J]. 金属学报, 2022, 58(9): 1208-1220.
[8] GAO Dong, ZHOU Yu, YU Ze, SANG Baoguang. Selection of Twin Variants in Dynamic Plastic Deformation of Pure Ti at Liquid Nitrogen Temperature[J]. 金属学报, 2022, 58(9): 1141-1149.
[9] ZHOU Hongwei, GAO Jianbing, SHEN Jiaming, ZHAO Wei, BAI Fengmei, HE Yizhu. Twin Boundary Evolution Under Low-Cycle Fatigue of C-HRA-5 Austenitic Heat-Resistant Steel at High Temperature[J]. 金属学报, 2022, 58(8): 1013-1023.
[10] ZHENG Shijian, YAN Zhe, KONG Xiangfei, ZHANG Ruifeng. Interface Modifications on Strength and Plasticity of Nanolayered Metallic Composites[J]. 金属学报, 2022, 58(6): 709-725.
[11] REN Ping, CHEN Xingpin, WANG Cunyu, YU Feng, CAO Wenquan. Effects of Pre-Strain and Two-Step Aging on Microstructure and Mechanical Properties of Fe-30Mn-11Al-1.2C Austenitic Low-Density Steel[J]. 金属学报, 2022, 58(6): 771-780.
[12] TIAN Ni, SHI Xu, LIU Wei, LIU Chuncheng, ZHAO Gang, ZUO Liang. Effect of Pre-Tension on the Fatigue Fracture of Under-Aged 7N01 Aluminum Alloy Plate[J]. 金属学报, 2022, 58(6): 760-770.
[13] GAO Chuan, DENG Yunlai, WANG Fengquan, GUO Xiaobin. Effect of Creep Aging on Mechanical Properties of Under-Aged 7075 Aluminum Alloy[J]. 金属学报, 2022, 58(6): 746-759.
[14] CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng. Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact[J]. 金属学报, 2022, 58(5): 660-672.
[15] GUO Xiangru, SHEN Junjie. Modelling of the Plastic Behavior of Cu Crystal with Twinning-Induced Softening and Strengthening Effects[J]. 金属学报, 2022, 58(3): 375-384.
No Suggested Reading articles found!