| DEFORMAION AND WORK HARDENING OF HADFIELD MANGANESE STEEL |
| SHI Deke;LIU Junhai X'ian Jiaotong University |
|
Cite this article:
SHI Deke;LIU Junhai X'ian Jiaotong University. DEFORMAION AND WORK HARDENING OF HADFIELD MANGANESE STEEL. Acta Metall Sin, 1989, 25(4): 142-145.
|
|
|
Abstract Work hardening of Hadfield manganese steel is mainly from twocauses: 1) a large amount of twinning makes perfect dislocal is or shockley dislo-cations to be blocked up at the coherent twin boundaries. 2) deformation leads tostrong unsymmetrical distortion due to a large number of Mn-C pairs or Mn-vaca-ncy carbon-carbon clusters. It has been demonstrated by TEM observation and in-ternal friction tests. As deformation proceeds, slip constantly accommodates twin-hing shear giving rise to stress relaxation. Thus, Hadfield steel possesses both rapidwork hardening and good ductility.
|
|
Received: 18 April 1989
|
1 White C H, Honeycombe R W K. J Iron Steel Inst, 1962; 200: 457 2 Roberts W N. TMS-AIME, 1964; 230: 372 3 Raghavan K S, Sastri A S, Mareinkowski M J. TMS-AIME, 1969; 245: 1569 4 Dastur Y N, Leslie W C. Metall Trans, 1981; 12A: 749 5 Adler P H, Olson G B, Owen W S. Metall Trans, 1986; 17A: 1725 6 石德珂,刘军海.待发表 7 王其闵,谢成刚.中国科学A辑,1986;11:1189 8 Cahn J W. Acta Metall, 1977; 25: 1021 9 Sleeswyk A W, Verbraak C A. Acta Metall, 1961; 9: 917 10 Remy L. Metall Trans, 1981; 12A: 38 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|