| HIGH-TEMPERATURE ISOPIESTIC STUDIES ON Hg-Pb BINARY AMALGAM |
| ZHANG Xinhua;HE Yuzhi;BAO Yuhong;WANG ? arises Shanghai Institute of Nuclear Research; Academia Sinica ? tion |
|
Cite this article:
ZHANG Xinhua;HE Yuzhi;BAO Yuhong;WANG ? arises Shanghai Institute of Nuclear Research; Academia Sinica ? tion. HIGH-TEMPERATURE ISOPIESTIC STUDIES ON Hg-Pb BINARY AMALGAM. Acta Metall Sin, 1989, 25(4): 146-147.
|
|
|
Abstract # The activities of mercury in the mercury-lead binanv omalgam ???? neasured usinga high-temperature isopiestie technique at 600K. The activities ???ead in the ???ary amalgamwere also calculated using the Gibbs-Duhem integration.
|
|
Received: 18 April 1989
|
1 Hultgren R, Desal P D, Hawkins D T, leiser M, Kelley K K. Selected Values of the Thermodynamic Properties of Binary Alloys, Metals Park, Ohio: ASM, 1973 2 Wang Z-C (王之昌), Zhang X-H (张新华), He Y-Z (何玉枝), Bao Y-H (包于洪). J Chem Soc Faraday Trans I, 1988; 84, 4369 3 Pomianek T. Z Metallk, 1986; 77: 388 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|