Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (1): 96-101    DOI:
Current Issue | Archive | Adv Search |
PROPERTIES OF ION PLATED TiN COATING MODIFIED BY ADDING Al and La
JIN Zhujing;YU Li;DAI Shaoxia;YU Zhiming Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang research assistant;Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang 110015
Cite this article: 

JIN Zhujing;YU Li;DAI Shaoxia;YU Zhiming Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang research assistant;Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang 110015. PROPERTIES OF ION PLATED TiN COATING MODIFIED BY ADDING Al and La. Acta Metall Sin, 1990, 26(1): 96-101.

Download:  PDF(1380KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A modified ion-plated IP-TiN coating has been developed by adding6 wt-% elementary Al and various small amounts of La. Examination of this coat-ing shows that the adhesion between the coating and substrate may be remarkablyimproved by the La added up to 2 wt-%, and the microhardness and wear resistanceof the coating surface may regularly change with the increase of La content. EPMAand X-ray diffraction analysis showed that the Al and La added are concentratedat the interface of the coating/substrate where a thicker transition zone formedwith an alternation of phase composition and grain orientation of the coating.Thus, an improvement over the properties of coating was proposed.
Key words:  ion plated TiN coating      Al      La      adhesivity     
Received:  18 January 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I1/96

1 金柱京,于力,戴少侠,于志明.金属学报,1989;25:B55
2 金柱京,于力,戴少侠,于志明,呼格吉夫.腐蚀科学与防护技术,待发表
3 Jin Zhujing (金柱京), Yu Li (于力), Dai Shaoxia (戴少侠), Yu Zhiming (于志明). Proc Int Conf of PVD Coatings, Shenyang, 1987
4 Hummer E. Thin Solid Films, 1983; 101; 243
[1] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[3] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[4] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[5] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[6] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[7] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[8] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[9] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[10] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[11] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[12] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[13] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[14] DU Jinhui, BI Zhongnan, QU Jinglong. Recent Development of Triple Melt GH4169 Alloy[J]. 金属学报, 2023, 59(9): 1159-1172.
[15] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
No Suggested Reading articles found!