Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (4): 5-11    DOI:
Current Issue | Archive | Adv Search |
CHARACTER OF CARBON DEPLETED REGIONS IN UNDERCOOLED AUSTENITE AND THERMODYNAMICS OF BAINITIC TRANSFORMATION
YANG Quanmin;KANG Mokuang Northwestern Polytechnical University; Xi'an Department of Material Science;Zhejiang Uniyersity;Hangzhou 310027
Cite this article: 

YANG Quanmin;KANG Mokuang Northwestern Polytechnical University; Xi'an Department of Material Science;Zhejiang Uniyersity;Hangzhou 310027. CHARACTER OF CARBON DEPLETED REGIONS IN UNDERCOOLED AUSTENITE AND THERMODYNAMICS OF BAINITIC TRANSFORMATION. Acta Metall Sin, 1990, 26(4): 5-11.

Download:  PDF(548KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The chemical driving forces for the phase transformation from auste-nite in three different carbon depleted regions into ferrite with identical composi-tion have been derived respectively. The starting temperature of bainitic transform-ation, B_s, has been also calculated according to the shearing mechanism of baini-tic transformation in the carbon depleted regions of austenite. The maximum driv-ing forces for the phase transformation in both 3%Cr containing and CrMo steelsmay be obtained at temperature B_s. It was shown that the proposal of the shearingmechanism of the bainitic transformation is thermodynamically possible.
Key words:  bainite      carbon depleted region      transformation      thermodynamics     
Received:  18 April 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I4/5

1 Entin R I. In: Zackay V E, Aaronson H I eds., Decomposition of Austenite by Diffusional Processes, New York: John Willey, 1962: 295
2 Aaronson H I, Domian H A, Pound G M. TMS AIME, 1966; 236: 753
3 Hsu T Y, Mou Yiwen. Acta Metall, 1984; 32: 1469
4 Lim C, Wuttig M. Acta Metall, 1974; 22: 1215
5 冯华,康沫狂,李春信.材料科学进展,1988;2(3) :32
6 杨全民,康沫狂.材料科学进展,待发表
7 杨全民.西北工业大学博士论文,1989
8 谢朝阳,康沫狂.材料科学进展,1988;2(6) :32
9 Shiflet G J, Bradley J R, Aaronson H I. Metall Trans, 1978; 8A: 999
10 徐祖耀.金属材料热力学,北京:冶金工业出版社,1983:272
11 Lyman T, Troiano A R. Trans ASM, 1946; 37: 402
12 Mcynet G. Rev Metall, 1954; 51: 365
13 Aaronson H I, Domian H A, Pound G M. Trans AIME, 1966: 236: 768
[1] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[3] ZHAO Yafeng, LIU Sujie, CHEN Yun, MA Hui, MA Guangcai, GUO Yi. Critical Inclusion Size and Void Growth in Dual-Phase Ferrite-Bainite Steel During Ductile Fracture[J]. 金属学报, 2023, 59(5): 611-622.
[4] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
[5] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[6] ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping. Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes[J]. 金属学报, 2023, 59(12): 1633-1643.
[7] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite[J]. 金属学报, 2023, 59(11): 1419-1427.
[8] LI Xiaobing, QIAN Kun, SHU Lei, ZHANG Mengshu, ZHANG Jinhu, CHEN Bo, LIU Kui. Effect of W Content on the Phase Transformation Behavior in Ti-42Al-5Mn- xW Alloy[J]. 金属学报, 2023, 59(10): 1401-1410.
[9] LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang. Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation[J]. 金属学报, 2023, 59(10): 1376-1388.
[10] GAO Jianbao, LI Zhicheng, LIU Jia, ZHANG Jinliang, SONG Bo, ZHANG Lijun. Current Situation and Prospect of Computationally Assisted Design in High-Performance Additive Manufactured Aluminum Alloys: A Review[J]. 金属学报, 2023, 59(1): 87-105.
[11] SUN Yi, ZHENG Qinyuan, HU Baojia, WANG Ping, ZHENG Chengwu, LI Dianzhong. Mechanism of Dynamic Strain-Induced Ferrite Transformation in a 3Mn-0.2C Medium Mn Steel[J]. 金属学报, 2022, 58(5): 649-659.
[12] LI Wei, JIA Xingqi, JIN Xuejun. Research Progress of Microstructure Control and Strengthening Mechanism of QPT Process Advanced Steel with High Strength and Toughness[J]. 金属学报, 2022, 58(4): 444-456.
[13] CHEN Wei, CHEN Hongcan, WANG Chenchong, XU Wei, LUO Qun, LI Qian, CHOU Kuochih. Effect of Dilatational Strain Energy of Fe-C-Ni System on Martensitic Transformation[J]. 金属学报, 2022, 58(2): 175-183.
[14] ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng. Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation[J]. 金属学报, 2022, 58(2): 155-164.
[15] ZHU Dongming, HE Jiangli, SHI Genhao, WANG Qingfeng. Effect of Welding Heat Input on Microstructure and Impact Toughness of the Simulated CGHAZ in Q500qE Steel[J]. 金属学报, 2022, 58(12): 1581-1588.
No Suggested Reading articles found!