Please wait a minute...
Acta Metall Sin  1990, Vol. 26 Issue (5): 79-85    DOI:
Current Issue | Archive | Adv Search |
THERMODYNAMICAL CRITERION OF SPINODAL DECOMPOSITION IN TERNARY SYSTEM
JIANG Bohong;CHANG Meihua;WEI Qing;XU Zuyao (T.Y. Hsu) Shanghai Jiaotong University
Cite this article: 

JIANG Bohong;CHANG Meihua;WEI Qing;XU Zuyao (T.Y. Hsu) Shanghai Jiaotong University. THERMODYNAMICAL CRITERION OF SPINODAL DECOMPOSITION IN TERNARY SYSTEM. Acta Metall Sin, 1990, 26(5): 79-85.

Download:  PDF(577KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By expanding the Gibbs free energy of ternary system into a Taylorseries with respect to the composition, a thermodynamical criterion of spinodal de-composition is conducted as G_(xx)(δ_x)~2 + 2G_(xy)δ_xδ_y + G_(yy)(δy)~2<0, from which, various con-ditions of spinodal decomposition are discussed. When G_(xx)<0, G_(xx)~2-G_(xx)G_(yy)<0, it iscalled as unstable decomposition unrestricted by the direction of composition fluctu-ation; when G_(xx)<0, G_(xy)~2-G_(xx)G_(yy)>0, or G_(xx)>0, G_(xy)~2-G_(xx)G_(yy)>0, as well as G_(xx)=0,are all considered as unstable decomposition restricted by the direction of composi-tion fluctuation δ_x and δ_y. The phenomenon of turning round in composition duringspinodal decomposition is attempted to be explained from above poiat of view. Thecomputer calculated ranges of unstable decomposition according to the criterion ofspinodal decomposition on Cu-Ni-Fe ternary system is consistent with the experi-mental results obtained from literatures.
Key words:  spinodal decomposition      thermodynamics      criterion      CuNiFe system     
Received:  18 May 1990     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1990/V26/I5/79

1 Cahn J W. Acta Metall, 1961; 9: 795
2 Hilliard J E. In: Aaronson H I ed, Phase Transformations, Metals Park, Ohlo: ASM, 1970: 497
3 de Fontaine D. J Phys Chem Solids, 1972; 33: 297
4 Lupis C H P, Gaye H. In: Kubaschewski O ed, Metallurgical Chemistry, Proceedings of a Symposium held at Brunel University and the National Physical Laboratory on the 14, 15 and 16 July 1971. London: Her Majesty's Stationery Office, 1972: 469
5 Lupis C H P. In: Chemecal Thermodynamics of Materials, New York: Elsevier Science, 1983: 304
6 Morral J E. Acta Metall, 1972; 20: 1069
7 Hoyt J J, Sluiter M. Clark B. Kraitchman M. de Fontaine D. Acta Metall, 1987; 35: 2315
8 Lyon O, Simon J P. Acta Metall, 1986; 34: 1197
9 Hultgren R, Desai P D, Hawkins D T, Gleiser M, Kelley K K. eds., Sellected Values of the Thermody namic Properties of Binary Alloys, ASM, 1973: 769
10 张美华,江伯鸿,徐祖耀.材料科学进展,待发表
11 Dahlgren S D. Metall Trans, 1977; 8A: 347
12 Butler E P, Thomas G. Acta Metall, 1970; 18: 3477
[1] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[2] GAO Jianbao, LI Zhicheng, LIU Jia, ZHANG Jinliang, SONG Bo, ZHANG Lijun. Current Situation and Prospect of Computationally Assisted Design in High-Performance Additive Manufactured Aluminum Alloys: A Review[J]. 金属学报, 2023, 59(1): 87-105.
[3] XIANG Zhaolong, ZHANG Lin, XIN Yan, AN Bailing, NIU Rongmei, LU Jun, MARDANI Masoud, HAN Ke, WANG Engang. Effect of Cr Content on Microstructure of Spinodal Decomposition and Properties in FeCrCoSi Permanent Magnet Alloy[J]. 金属学报, 2022, 58(1): 103-113.
[4] LIU Feng, WANG Tianle. Precipitation Modeling via the Synergy of Thermodynamics and Kinetics[J]. 金属学报, 2021, 57(1): 55-70.
[5] WANG Zumin,ZHANG An,CHEN Yuanyuan,HUANG Yuan,WANG Jiangyong. Research Progress on Fundamentals and Applications of Metal-Induced Crystallization[J]. 金属学报, 2020, 56(1): 66-82.
[6] Xiaodong LIN,Qunjia PENG,En-Hou HAN,Wei KE. Effect of Annealing on Microstructure of Thermally Aged 308L Stainless Steel Weld Metal[J]. 金属学报, 2019, 55(5): 555-565.
[7] Baojun ZHAO,Yuhong ZHAO,Yuanyang SUN,Wenkui YANG,Hua HOU. Effect of Mn Composition on the Nanometer Cu-Rich Phase of Fe-Cu-Mn Alloy by Phase Field Method[J]. 金属学报, 2019, 55(5): 593-600.
[8] Chengming ZHENG, Qingchao TIAN. Effect of Alloy Elements on Oxidation Behavior of Piercing Plug Steel[J]. 金属学报, 2019, 55(4): 427-435.
[9] Jianxue LIU, Wenjun XI, Neng LI, Shujie LI. Effect of Interfacial Energy on Distribution of Nanoparticle in the Melt During the Preparation of Fe-Based ODS Alloys by Thermite Reaction[J]. 金属学报, 2017, 53(8): 1011-1017.
[10] Liheng LIU,Chunshan CHE,Gang KONG,Jintang LU,Shuanghong ZHANG. DESTABILIZATION MECHANISM OF Fe-Al INHIBITION LAYER IN Zn-0.2%Al HOT-DIP GALVANIZING COATING AND RELATED THERMODYNAMIC EVALUATION[J]. 金属学报, 2016, 52(5): 614-624.
[11] Feng LIU, Kang WANG. DISCUSSIONS ON THE CORRELATION BETWEEN THERMODYNAMICS AND KINETICS DURING THE PHASE TRANSFORMATIONS IN THE TMCP OF LOW-ALLOY STEELS[J]. 金属学报, 2016, 52(10): 1326-1332.
[12] XIE Jun, YU Jinjiang, SUN Xiaofeng, JIN Tao, SUN Yuan. CARBIDE EVOLUTION BEHAVIOR OF K416B AS-CAST Ni-BASED SUPERALLOY WITH HIGH W CONTENT DURING HIGH TEMPERATURE CREEP[J]. 金属学报, 2015, 51(4): 458-464.
[13] WANG Xing, XI Wenjun, CUI Yue, LI Shujie. MICROSTRUCTURE EVOLUTION MECHANISM AND MECHANICAL PROPERTIES OF FeNiCrAl ALLOY REINFORCED BY COHERENT NiAl SYNTHE- SIZED BY THERMITE PROCESS[J]. 金属学报, 2015, 51(4): 483-491.
[14] WU Changjun, ZHU Chenlu, SU Xuping, LIU Ya, PENG Haoping, WANG Jianhua. THERMODYNAMICAL AND KINETIC INVESTIGA-TION OF FORMATION OF PERIODIC LAYERED STRUCTURE IN TiCu/Zn INTERFACE REACTION[J]. 金属学报, 2014, 50(8): 930-936.
[15] MA Ping, WU Erdong, LI Wuhui, SUN Kai, CHEN Dongfeng. MICROSTRUCTURES AND HYDROGEN STORAGE PROPERTIES OF Ti0.7Zr0.3(Cr1-xVx)2 ALLOYS[J]. 金属学报, 2014, 50(4): 454-462.
No Suggested Reading articles found!