STUDY OF INTERFACES AND SURFACES OF YBa_2Cu_3O_(7-x)-Ag
FAN Yongnian; TANG Baozhen; QIAO Guiwen (Institute of Metal Research; Academia Sinica; Shenyang)
Cite this article:
FAN Yongnian; TANG Baozhen; QIAO Guiwen (Institute of Metal Research; Academia Sinica; Shenyang). STUDY OF INTERFACES AND SURFACES OF YBa_2Cu_3O_(7-x)-Ag. Acta Metall Sin, 1992, 28(7): 70-73.
Abstract Interfaces and surfaces of YBa_2Cu_3O_(7-x) (YBCO)-Ag have been studied by SEM-EDX and AES. No effect of Ag on 123 structure in X-ray diffraction pattern was observed for 0.4 mol Ag doped YBCO. AES analysis indicated that Ag segregated on surface of YBCO and resulted in decrease of YBCO-metal lead resistance. In addition, solution and segregation of Ag as elemental state were often appreared on interfaces and surfaces of high temperature annealed YBCO, whether elemental Ag or compound Ag_2O and AgNO_3 adopted as doping material.
1 Mizushima K, Sagoi M, Miura T, Yoshida J. Jpn J Appl Phys, 1988; 27: L1489 2 Salama K, Selvamanickam V, Gao L, Sun K. Appl Phys Lett, 1989; 54: 2352 3 汤宝珍,崔永姬,樊永年,乔桂文.全国高温超导学术会议论文集(一),宝鸡:稀有金属加上研究所出版,1988:19-12 4 Nishio T, Itoh Y. Ogasawara F, Suganuma M, Yamada Y, Mizutani U. J Mater Sci, 1989; 24; 3228 5 Singh J P, Leu H J, Poeppel R B. Van Voorhees E, Goudey G T, Winsley K. Shi D. J Appl Phys, 1989; 66: 3154 6 Mansour A N, Dallek S, Anderson G R. Physics, 1989; B158: 519