STUDY OF INTERFACES AND SURFACES OF YBa_2Cu_3O_(7-x)-Ag
FAN Yongnian; TANG Baozhen; QIAO Guiwen (Institute of Metal Research; Academia Sinica; Shenyang)
Cite this article: 

FAN Yongnian; TANG Baozhen; QIAO Guiwen (Institute of Metal Research; Academia Sinica; Shenyang). STUDY OF INTERFACES AND SURFACES OF YBa_2Cu_3O_(7-x)-Ag. Acta Metall Sin, 1992, 28(7): 70-73.

Download:  PDF(670KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Interfaces and surfaces of YBa_2Cu_3O_(7-x) (YBCO)-Ag have been studied by SEM-EDX and AES. No effect of Ag on 123 structure in X-ray diffraction pattern was observed for 0.4 mol Ag doped YBCO. AES analysis indicated that Ag segregated on surface of YBCO and resulted in decrease of YBCO-metal lead resistance. In addition, solution and segregation of Ag as elemental state were often appreared on interfaces and surfaces of high temperature annealed YBCO, whether elemental Ag or compound Ag_2O and AgNO_3 adopted as doping material.
Key words:  YBa_2Cu_3O_(7-x)      Ag      interface      surface      segregation     
Received:  18 July 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I7/70

1 Mizushima K, Sagoi M, Miura T, Yoshida J. Jpn J Appl Phys, 1988; 27: L1489
2 Salama K, Selvamanickam V, Gao L, Sun K. Appl Phys Lett, 1989; 54: 2352
3 汤宝珍,崔永姬,樊永年,乔桂文.全国高温超导学术会议论文集(一),宝鸡:稀有金属加上研究所出版,1988:19-12
4 Nishio T, Itoh Y. Ogasawara F, Suganuma M, Yamada Y, Mizutani U. J Mater Sci, 1989; 24; 3228
5 Singh J P, Leu H J, Poeppel R B. Van Voorhees E, Goudey G T, Winsley K. Shi D. J Appl Phys, 1989; 66: 3154
6 Mansour A N, Dallek S, Anderson G R. Physics, 1989; B158: 519
[1] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[2] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[3] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[4] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[5] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[6] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[7] LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun. Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion[J]. 金属学报, 2023, 59(8): 986-1000.
[8] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[9] LU Yuhua, WANG Haizhou, LI Dongling, FU Rui, LI Fulin, SHI Hui. A Quantitative and Statistical Method of γ' Precipitates in Superalloy Based on the High-Throughput Field Emission Scanning Eelectron Microscope[J]. 金属学报, 2023, 59(7): 841-854.
[10] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[11] WANG Furong, ZHANG Yongmei, BAI Guoning, GUO Qingwei, ZHAO Yuhong. First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface[J]. 金属学报, 2023, 59(6): 812-820.
[12] LIANG Kai, YAO Zhihao, XIE Xishan, YAO Kaijun, DONG Jianxin. Correlation Between Microstructure and Properties of New Heat-Resistant Alloy SP2215[J]. 金属学报, 2023, 59(6): 797-811.
[13] WANG Bin, NIU Mengchao, WANG Wei, JIANG Tao, LUAN Junhua, YANG Ke. Microstructure and Strength-Toughness of a Cu-Contained Maraging Stainless Steel[J]. 金属学报, 2023, 59(5): 636-646.
[14] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[15] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
No Suggested Reading articles found!