SULPHATES-INDUCED HOT CORROSION OF Ni_3Al INO_2/SO_2/SO_3 ATMOSPHERE
SHEN Huaqing;ZENG Chaoliu;WU Weitao;GUO Jianting Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang. Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

SHEN Huaqing;ZENG Chaoliu;WU Weitao;GUO Jianting Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academia Sinica; Shenyang. Institute of Metal Research; Academia Sinica; Shenyang. SULPHATES-INDUCED HOT CORROSION OF Ni_3Al INO_2/SO_2/SO_3 ATMOSPHERE. Acta Metall Sin, 1993, 29(10): 68-72.

Download:  PDF(1021KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The short-time hot corrosion kinetics of Ni_3Al in the presence of a salt film(about 2mg/cm~2 (Na,K)_2SO_4) in O_2-0.5%(SO_2+SO_3) atmosphere at temperature range of600--850℃ has been studied by thermal gravimetry, chemical analysis, X-ray diffraction,metallography and SEM. Low temperature hot corrosion occured in Ni_3Al due to the forma-tion of liquidNi-Na-K sulphate eutectic phase. The corrosion rates reached maximum at750℃ in the condition mentioned above. Moreover, the effects of O_2/SO_2/SO_3 gas, saltfilm and CoCrAlY coating on the hot corrosion behavior of Ni_3Al have also beeninvestigated. The salt film may accelerate the oxidation of Ni_3Al in air, and CoCrAlY coatingmay improve the corrosion resistance of Ni_3Al in same environment.
Key words:  hot corrosion      Ni_3Al      intermetallic compound      sulphate     
Received:  18 October 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I10/68

1 Brill U. Werk Korr, 1990, 41: 682
2 Forsen O, Kaskiala M, Tikkanen M H, Tavi M. Werk Korr, 1990, 41: 692
3 王福会.中国科学院金属腐蚀与防护研究所博士论文,1992
4 Lillerud K P, Kofstad P. Oxid Met, 1984, 21(5/6) : 233
5 Misra Ajay K. Oxid Met, 1986, 25(5/6) , 129
6 Erdoes E. In: Hart A B, Cutler A J B eds., Deposition and Corrosion in Gas Turbine, London: Applied Science Publishers LTD, 1973, 115
7 SHIH Shengtai, ZHANG Yunshu, LI Xuanming. J Mater Sci Eng,1989, A120:277
[1] DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo. In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology[J]. 金属学报, 2022, 58(4): 567-580.
[2] ZHOU Lijun, WEI Song, GUO Jingdong, SUN Fangyuan, WANG Xinwei, TANG Dawei. Investigations on the Thermal Conductivity of Micro-Scale Cu-Sn Intermetallic Compounds Using Femtosecond Laser Time-Domain Thermoreflectance System[J]. 金属学报, 2022, 58(12): 1645-1654.
[3] WANG Di, WANG Dong, XIE Guang, WANG Li, DONG Jiasheng, CHEN Lijia. Influence of Pt-Al Coating on Hot Corrosion Resistance Behaviors of a Ni-Based Single-Crystal Superalloy[J]. 金属学报, 2021, 57(6): 780-790.
[4] Hua JI,Yunlai DENG,Hongyong XU,Weiqiang GUO,Jianfeng DENG,Shitong FAN. The Influence of Welding Line Energy on the Microstructure and Property of CMT Overlap Joint of 5182-Oand HC260YD+Z[J]. 金属学报, 2019, 55(3): 376-388.
[5] Yimin LIAO, Min FENG, Minghui CHEN, Zhe GENG, Yang LIU, Fuhui WANG, Shenglong ZHU. Comparative Study of Hot Corrosion Behavior of theEnamel Based Composite Coatings and the ArcIon Plating NiCrAlY on TiAl Alloy[J]. 金属学报, 2019, 55(2): 229-237.
[6] Liqun CHEN, Zhengchen QIU, Tao YU. Effect of Ru on the Electronic Structure of the [100](010) Edge Dislocation in NiAl[J]. 金属学报, 2019, 55(2): 223-228.
[7] CAO Lihua, CHEN Yinbo, SHI Qiyuan, YUAN Jie, LIU Zhiquan. Effects of Alloy Elements on the Interfacial Microstructure and Shear Strength of Sn-Ag-Cu Solder[J]. 金属学报, 2019, 55(12): 1606-1614.
[8] HE Xianmei, TONG Liuniu, GAO Cheng, WANG Yichao. Effect of Nd Content on the Structure and Magnetic Properties of Si(111)/Cr/Nd-Co/Cr Thin Films Prepared by Magnetron Sputtering[J]. 金属学报, 2019, 55(10): 1349-1358.
[9] GAO Bo, WANG Lei, SONG Xiu, LIU Yang, YANG Shuyu, CHIBA Akihiko. Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy[J]. 金属学报, 2019, 55(10): 1273-1281.
[10] Min ZHANG, Erlong MU, Xiaowei WANG, Ting HAN, Hailong LUO. Microstructure and Mechanical Property of the Welding Joint of TA1/Cu/ X65 Trimetallic Sheets[J]. 金属学报, 2018, 54(7): 1068-1076.
[11] Huijun KANG, Jinling LI, Tongmin WANG, Jingjie GUO. Growth Behavior of Primary Intermetallic Phases and Mechanical Properties for Directionally Solidified Al-Mn-Be Alloy[J]. 金属学报, 2018, 54(5): 809-823.
[12] Chengyang JIANG, Yingfei YANG, Zhengyi ZHANG, Zebin BAO, Shenglong ZHU, Fuhui WANG. Preparation and Enhanced Hot Corrosion Resistance of aZr-Doped PtAl2+(Ni, Pt)Al Dual-Phase Coating[J]. 金属学报, 2018, 54(4): 581-590.
[13] Ning ZHAO,Jianfeng DENG,Yi ZHONG,Luqiao YIN. Evolution of Interfacial Intermetallic Compounds in Ni/Sn-xCu/Ni Micro Solder Joints Under Thermomigration During Soldering[J]. 金属学报, 2017, 53(7): 861-868.
[14] Dawei WANG,Shichao XIU. Effect of Bonding Temperature on the Interfacial Micro-structure and Performance of Mild Steel/Austenite Stainless Steel Diffusion-Bonded Joint[J]. 金属学报, 2017, 53(5): 567-574.
[15] Zhijie ZHANG,Mingliang HUANG. Liquid-Solid Electromigration Behavior of Cu/Sn-52In/Cu Micro-Interconnect[J]. 金属学报, 2017, 53(5): 592-600.
No Suggested Reading articles found!