Abstract The bonding characteristic in Pd doping Ni_3Al was studied by DV-Xα clustermethod, and the mechanism for ductilization of Ni_3Al with Pd-doping was discussed basedon the theoretical model proposed by the authors. The ductilization is related with the in-crease of delocalized bonding electrons caused by Pd-doping. Since Pd-Al bond is strongerthan Pd-Ni bond, the delocalized bonding electrons will increase with the drop of Al content,this implies that hypo-stoichiomcrty in Al is necessary to the ductilization in Ni_3Al.
|
|
Received: 18 November 1993
|
1 Takasugi T, Izumi O. Acta Metall, 1985; 33: 1247 2 Takasugi T, Izumi O, Masahasi N. Acta Metall 1985; 33: 1259 3 Taub A I, Briant C L, Huang S C, Chang K M, Jackson M R. Scr Metall, 1986; 20: 129 4 Taub A I, Briant C L. Acta Metall. 1987; 35: 1597 5 Chiba A, Hanada S. Watanabe S. Acta Metall 1991; 39: 1799 6 Chiba A, Hanada S, Watanabe S. Mater Sci Eng, 1992; A 152: 108 7 Hu Z Q, Meng C G, Guo J T. J Mater Sci, to be published 8 Meng C G, Guo J T, Hu Z Q. In: International Workshop on Ordered Intermetalllics, Hangzhou: 1992 9 Chiba A, Shindo D, Hanada S. Acta Metall, 1991; 39: 13 10 Sato M. Solid State Commun. 1974; 15: 1863 11 Ellis D E, Painter G S. Phys Rev, 1970: 2B: 2887 12 孟长功、徐东生、郭建亭、胡壮麒.金属学报,1993;29:A:56 13 Morinaga M, Yukawa N, Adachi H. J Phys Soc Jpn, 1984; 53: 653 14 Ochiai S, Oya Y, Suzuki T. Acta Metall, 1984; 32: 289 15 Enomoto M, Harada H. Metall Trans. 19891 A 20: 649 16 Jena A K, Chaturvedi M C. J Mater Sci, 1984; 19: 3121 17 Cahn R W, Siemers P A, Hall F L. Acta Metall, 1987; 35: 2753 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|