SOLUBILITIES OF Ce, Nd AND Y IN α-Fe
LI Laifeng;XING Zhongshu Institute of Metal Research; Academia Sinica; 1992 professor;Institute of Metal Research;Academia Sinica; Shenyang 110015
Cite this article: 

LI Laifeng;XING Zhongshu Institute of Metal Research; Academia Sinica; 1992 professor;Institute of Metal Research;Academia Sinica; Shenyang 110015. SOLUBILITIES OF Ce, Nd AND Y IN α-Fe. Acta Metall Sin, 1993, 29(3): 40-45.

Download:  PDF(509KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The solubilities of Ce, Nd and Y in α-Fe at 873 to 1153K have been determined by means of electron microprobe quantitative analyses. The temperature dependencesof the solubilities were obtained from the experimental data. The results have been comparedwith those determined by three other technigues, very good agreement was obtained betweenthe results of all these techniques.
Key words:  α-Fe      Ce      Nd      Y      solubility     
Received:  18 March 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I3/40

1 Ricard J. Mem Sci Rev Metall, 1962; 59: 527
2 Jepson J O, Duweg P. Trans ASM, 1961, 53: 543
3 #12
4 Domagala R F. Rasch J J. Levinson S W. Trans ASM, 1961, 53: 137
5 邵宗宝,中国科学院金属研究所硕士学位论文,1984
6 He You, Chang Xiangrong, Tian Zhongzhuo, Xiao Jimei, Wang Minghua, Lu Hongbang. Wang Yunyu, Liu Nianq, Scr Metall, 1985: 19: 79
7 王蕴玉,刘年庆,田中卓,常香荣.金属学报,1987,23:B149
8 章复中,谷力军,翟柳兴,刘沃垣,颜玉新.金属学报,1987;23:A503
9 Kubaschewski O. Iron-Binary Phase Diagrams, Berlin: Springer-Verlag, 1982: 9
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[3] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[4] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[5] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[6] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[7] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[8] DU Jinhui, BI Zhongnan, QU Jinglong. Recent Development of Triple Melt GH4169 Alloy[J]. 金属学报, 2023, 59(9): 1159-1172.
[9] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[10] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[11] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[12] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[13] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[14] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[15] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
No Suggested Reading articles found!