| FATIGUE BEHAVIOUR OF M/B DUPLEX STRUCTURE IN A HIGH CARBON Cr-Mo-W STEEL |
| TIAN Baohong;ZHENG Shi'an;WU Lei Luoyang Institute of Technology associate professor;Department of Materials Engineering;Luoyang Institute of Technology; Luoyang 471039 |
|
Cite this article:
TIAN Baohong;ZHENG Shi'an;WU Lei Luoyang Institute of Technology associate professor;Department of Materials Engineering;Luoyang Institute of Technology; Luoyang 471039. FATIGUE BEHAVIOUR OF M/B DUPLEX STRUCTURE IN A HIGH CARBON Cr-Mo-W STEEL. Acta Metall Sin, 1993, 29(3): 46-50.
|
|
|
Abstract Determination was carried out of fatigue crack propagation rate of steel65Cr5Mo3W2VSiTi (LM2) with various bainite contents and M/B duplex structure tem-pered at various temperatures. The threshold value of fatigue for each processing was esti-mated by experimental data. The mechanism for fatigue crack propagation of M / B duplexstructure in steel LM2 seems to be non-continuous. Both calculated and measured fatiguecrack micro-propagation rates are found to be matched.
|
|
Received: 18 March 1993
|
1 Tomita Y, Okabayashi K, Metall Trans, 1983: 14A: 485 2 Ohmori Y, Ohtani H, Kuntake T. Met Sci, 1974; 8: 357 3 Su Deda, Li Yutong, Wang Jian, Microstructure and Behavior of Materials. Vol. Ⅱ, Warley: Engineering Materials Advisory Services Ltd., 1985: 919 4 Smith R A,顾海澄译.疲劳裂纹扩展--30年来的进展.西安:西安交通大学出版社,1989:35 5 邓蓉英,李禾,于程清.金属学报,1984;20:A76 6 Yan M, Gu M, Liu C. In: Baecklund J, Blom A F, Beevers C J eds., Fatigue Thresholds, Fundamentals and Engineering Applications, Vol. Ⅱ, Warley: Engineering Materials Advisory Services Ltd., 1982; 615% |