NEUTRON DIFFRACTION STUDY ON R_2Fe_(17)N_χ(R=Y, Dy, Nd) |
YANG Jilian;ZHANG Baisheng;DING Yongfan;YANG Yingchang;ZHANG Xiaodong;PAN Shuming China Institute of Atomic Energy; Beijing Department of Physics; Peking University; Beijing General Research Institute for Non-Ferrous Metals; Beijing associate professor; P.O. Box 275; Branch No.30; Beijing 102413 |
|
Cite this article:
YANG Jilian;ZHANG Baisheng;DING Yongfan;YANG Yingchang;ZHANG Xiaodong;PAN Shuming China Institute of Atomic Energy; Beijing Department of Physics; Peking University; Beijing General Research Institute for Non-Ferrous Metals; Beijing associate professor; P.O. Box 275; Branch No.30; Beijing 102413. NEUTRON DIFFRACTION STUDY ON R_2Fe_(17)N_χ(R=Y, Dy, Nd). Acta Metall Sin, 1993, 29(3): 84-87.
|
Abstract Samples of R_2Fe_(17)N_x(R=Y, Dy, Nd) were measured by neutron diffraction,and their magnetic structures and N site were determined. The effect of the site occupation ofN on magnetic properties was discussed primarily.
|
Received: 18 March 1993
|
1 Coey J MD, Sun Hong. J Magn Magn Mater, 1990; 57: L251 2 Rietveld H M. J Appl Crystallogr, 1969; 2: 65 3 Otani Y, Hurley D P F, Sun Hong, Coey J M D. J Appl Phys, 1991; 69: 5584 4 Zhong X-P, Radwahski R J, De Boer F R, Jacobe T H, Buschow K H J. J Magn Magn Mater, 1990; 86: 333 5 Allred A L, Rochow E G. J Inorg Nucl Chem, 1958; 5: 264 6 Gschneidner K A. In: Michelsen O B ed., Analysis and Application of Rare Earth Materials, Universitets Forlaget, 1973: |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|