NUMERICAL SIMULATION ON FLOW AND MIXING PROCESSES IN BOTTOM BLOWN LADLES
LI Baokuan;HE Jicheng;LU Zhongwu Northeast University of Technology; Shenyang doctor;Department of Thermal Eneragy Northeast University of Technology; Shenyang 110006
Cite this article:
LI Baokuan;HE Jicheng;LU Zhongwu Northeast University of Technology; Shenyang doctor;Department of Thermal Eneragy Northeast University of Technology; Shenyang 110006. NUMERICAL SIMULATION ON FLOW AND MIXING PROCESSES IN BOTTOM BLOWN LADLES. Acta Metall Sin, 1993, 29(4): 47-51.
Abstract An improvement on the flow and mixing conditions in bottom blown ladlesmay be made by either shifting the nozzle from centre to off-centre or changing from one totwo nozzles. Thus, the shorter time for homogeneous mixing in ladle seems to be available.
1 Asai S, Okamoto T, He J C, Muchi I. Trans Iron Steel Inst Jpn, 1983; 23: 43 2 李宝宽.东北工学院博士学位论文,1992 3 Launder B E, Spalding D B. Comput Math Appl Mech Eng, 1974; 3: 269 4 Castilljeos A H, Brimacombe J K. Metall Trans, 1987; 18B: 659 5 李宝宽,赫冀成,陆钟武.金属学报.1992;28:B475 6 Dromer H C, Oeters F. Int Conf Injection Metallurgy. Lelea, Sweden. 1983; 9: 1 7 赫冀成,浅井滋生,鞭严.铁钢 1984;11:59