Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (4): 47-51    DOI:
Current Issue | Archive | Adv Search |
NUMERICAL SIMULATION ON FLOW AND MIXING PROCESSES IN BOTTOM BLOWN LADLES
LI Baokuan;HE Jicheng;LU Zhongwu Northeast University of Technology; Shenyang doctor;Department of Thermal Eneragy Northeast University of Technology; Shenyang 110006
Cite this article: 

LI Baokuan;HE Jicheng;LU Zhongwu Northeast University of Technology; Shenyang doctor;Department of Thermal Eneragy Northeast University of Technology; Shenyang 110006. NUMERICAL SIMULATION ON FLOW AND MIXING PROCESSES IN BOTTOM BLOWN LADLES. Acta Metall Sin, 1993, 29(4): 47-51.

Download:  PDF(367KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  An improvement on the flow and mixing conditions in bottom blown ladlesmay be made by either shifting the nozzle from centre to off-centre or changing from one totwo nozzles. Thus, the shorter time for homogeneous mixing in ladle seems to be available.
Key words:  bottom blown gas ladle      numerical simulation      flow      mixing     
Received:  18 April 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I4/47

1 Asai S, Okamoto T, He J C, Muchi I. Trans Iron Steel Inst Jpn, 1983; 23: 43
2 李宝宽.东北工学院博士学位论文,1992
3 Launder B E, Spalding D B. Comput Math Appl Mech Eng, 1974; 3: 269
4 Castilljeos A H, Brimacombe J K. Metall Trans, 1987; 18B: 659
5 李宝宽,赫冀成,陆钟武.金属学报.1992;28:B475
6 Dromer H C, Oeters F. Int Conf Injection Metallurgy. Lelea, Sweden. 1983; 9: 1
7 赫冀成,浅井滋生,鞭严.铁钢 1984;11:59
[1] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[2] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
[3] ZHANG Limin, LI Ning, ZHU Longfei, YIN Pengfei, WANG Jianyuan, WU Hongjing. Macrosegregation Mechanism of Primary Silicon Phase in Cast Hypereutectic Al-Si Alloys Under Alternating Electropulsing[J]. 金属学报, 2023, 59(12): 1624-1632.
[4] ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping. Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes[J]. 金属学报, 2023, 59(12): 1633-1643.
[5] XIA Dahai, DENG Chengman, CHEN Ziguang, LI Tianshu, HU Wenbin. Modeling Localized Corrosion Propagation of Metallic Materials by Peridynamics: Progresses and Challenges[J]. 金属学报, 2022, 58(9): 1093-1107.
[6] LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong. Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold[J]. 金属学报, 2022, 58(10): 1236-1252.
[7] HU Long, WANG Yifeng, LI Suo, ZHANG Chaohua, DENG Dean. Study on Computational Prediction About Microstructure and Hardness of Q345 Steel Welded Joint Based on SH-CCT Diagram[J]. 金属学报, 2021, 57(8): 1073-1086.
[8] LI Zihan, XIN Jianwen, XIAO Xiao, WANG Huan, HUA Xueming, WU Dongsheng. The Arc Physical Characteristics and Molten Pool Dynamic Behaviors in Conduction Plasma Arc Welding[J]. 金属学报, 2021, 57(5): 693-702.
[9] HE Changshu, QIE Mofan, ZHANG Zhiqiang, ZHAO Xiang. Effect of Axial Ultrasonic Vibration on Metal Flow Behavior During Friction Stir Welding[J]. 金属学报, 2021, 57(12): 1614-1626.
[10] TANG Haiyan, LIU Jinwen, WANG Kaimin, XIAO Hong, LI Aiwu, ZHANG Jiaquan. Progress and Perspective of Functioned Continuous Casting Tundish Through Heating and Temperature Control[J]. 金属学报, 2021, 57(10): 1229-1245.
[11] LI Tianrui, LIU Guohuai, YU Shaoxia, WANG Wenjuan, ZHANG Fengyi, PENG Quanyi, WANG Zhaodong. Microstructure Evolution and Deformation Mechanisms by Direct Hot-Pack Rolling for As-Cast Ti-46Al-8Nb Alloys[J]. 金属学报, 2020, 56(8): 1091-1102.
[12] WANG Fuqiang, LIU Wei, WANG Zhaowen. Effect of Local Cathode Current Increasing on Bath-Metal Two-Phase Flow Field in Aluminum Reduction Cells[J]. 金属学报, 2020, 56(7): 1047-1056.
[13] ZHENG Jincan, LIU Runcong, WANG Xiaodong. Online Electromagnetic Measurement of Molten Zinc Surface Velocity in Hot Galvanized Process[J]. 金属学报, 2020, 56(7): 929-936.
[14] LIU Jizhao, HUANG Hefei, ZHU Zhenbo, LIU Awen, LI Yan. Numerical Simulation of Nanohardness in Hastelloy N Alloy After Xenon Ion Irradiation[J]. 金属学报, 2020, 56(5): 753-759.
[15] WANG Bo,SHEN Shiyi,RUAN Yanwei,CHENG Shuyong,PENG Wangjun,ZHANG Jieyu. Simulation of Gas-Liquid Two-Phase Flow in Metallurgical Process[J]. 金属学报, 2020, 56(4): 619-632.
No Suggested Reading articles found!