| INFLUENCES OF APPLIED POTENTIALS AND LOADING WAVEFORM ON FATIGUE CRACK GROWTH FOR STEEL A537 |
| WANG Zhengfu;KE Wei Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academia Sinica; ShenyangLINJin;Institute of Corrosion and Protection of Metals;Academia Sinica;Shenyang 110015 |
|
Cite this article:
WANG Zhengfu;KE Wei Corrosion Science Laboratory; Institute of Corrosion and Protection of Metals; Academia Sinica; ShenyangLINJin;Institute of Corrosion and Protection of Metals;Academia Sinica;Shenyang 110015. INFLUENCES OF APPLIED POTENTIALS AND LOADING WAVEFORM ON FATIGUE CRACK GROWTH FOR STEEL A537. Acta Metall Sin, 1993, 29(6): 82-87.
|
|
|
Abstract Influences of applied potentials and loading waveform on the fatigue crackgrowth for steel A537 in 3.5%NaCl solution, and corresponding straining electrode behaviourhave been studied. Under the applied potentials over or below-800 mV (SCE), the anodicdissolution or the hydrogen embrittlement is predominant, respectively. For applied anodicpotential, the acceleration effect of continuous loading pattern on the CF crack growth main-ly appeared at the range of low △K values, while for cathodic potential, it appeared at therange of high △K values. The continuous straining causes a decrease of natural potential andan increase of anodic dissolution current.
|
|
Received: 18 June 1993
|
1 Barson J M. J Eng Fract Mech. 1971; 3: 15 2 Achilles R D, Bulloch J H. Int J Pres Ves piping 1987; 30: 375 3 Saxena A, Liaw P K, Landes J D. Mat Sci Engng. 1987; 95: 137 4 Patel C, Pyle P, Rollins V. Matal Science. June, 1977; 185 5 Haor T P, Ford F P. J Electrochem Soc, 1973; 120: 1013 6 Wang Z F, Zhu Z M, Ke W. Metall Trans, 1992; 23A: 3337 7 Wang M, Hardie D. Proc Conf Hydrogen and Marerials, Beijing, Published by Institut Superieur des metaux et de la Construction Mecanique, 1988; 900 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|