| APPROACH TO STRENGTHENING AND DUCTILIZING OF Fe_3Al-BASED INTERMETALLIC ALLOYS |
| SUN Zuqing;HUANG Yuanding;YANG Wangyue;MAO Weimin;CHEN Guoliang University of Science and Technology Beijing; Beijingprofessor;Department of Materials Science and Engineering;University of Science and Technology Beijing; Beijing 100083 |
|
Cite this article:
SUN Zuqing;HUANG Yuanding;YANG Wangyue;MAO Weimin;CHEN Guoliang University of Science and Technology Beijing; Beijingprofessor;Department of Materials Science and Engineering;University of Science and Technology Beijing; Beijing 100083. APPROACH TO STRENGTHENING AND DUCTILIZING OF Fe_3Al-BASED INTERMETALLIC ALLOYS. Acta Metall Sin, 1993, 29(8): 20-24.
|
|
|
Abstract The properties of Fe_3Al-based intermetallic alloys at room temperature havebeen significantly improved through multi-alloying composition control and optimization ofthermomechanical process. The elongation was increased from2--3% for as-cast state to 15--20%, the yield strength up to 500 MPa. It is found that the elongated flattened grains,B_2 structure and dispersive second phase are beneficial to the comperehensive improvementof mechanical properties at room temperature.
|
|
Received: 18 August 1993
|
1 McKamey C G, DeVan J H, Tortorelli P F, Sikka V K. J Mater Res. 1991; 6: 1779 2 McKamey C G, HortonJ A, Liu C T. J Mater Res. 1989; 4: 1156 3 孙祖庆,黄原定,杨王玥,陈国良,北京科技大学学报,1991;13:539 4 孙祖庆,黄原定,陈国良,北京科技大学学报,1992;14:328 5 郭建亭,孙超,谭明晖,李辉,赖万慧,金属学报,1990;26:A20 6 孙扬善,郭军,张力宁,张谨平,金属学报,1991;27:A225x |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|