Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (8): 25-30    DOI:
Current Issue | Archive | Adv Search |
IN SITU OBSERVATION OF BAINITIC NUCLEATION BY SHEAR IN SOLUTE DEPLETED ZONE IN Cu-Zn-Al ALLOY
MENG Xiangkang;KANG Mokuang Northwestern Polytechnical Uiversitydoctoral candidate;Faculty 401;Norhtwestern Polytchnical University; Xi'an 710072
Cite this article: 

MENG Xiangkang;KANG Mokuang Northwestern Polytechnical Uiversitydoctoral candidate;Faculty 401;Norhtwestern Polytchnical University; Xi'an 710072. IN SITU OBSERVATION OF BAINITIC NUCLEATION BY SHEAR IN SOLUTE DEPLETED ZONE IN Cu-Zn-Al ALLOY. Acta Metall Sin, 1993, 29(8): 25-30.

Download:  PDF(784KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The analytical electron microscopic in situ study on a Cu-Zn-Al alloy indi-cates that solute depleted zone occurs within baintic incubation period, and after the periodbainite nucleates in this zone by way of matensitic shear.
Key words:  bainitic reaction      bainitic incubation period      solute depleted zone     
Received:  18 August 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I8/25

1 Kurdjumov G. Trans AIME. 1933; 105:253
2 Entin R I. In: Zackay V E, Aaronson H I eds., Decomposition of Austenite by Diffusional Processes, New York: John Willey, 1962: 295
3 Lim C, Wutting M. Acta Metall. 1974; 22: 1215
4 谢朝阳,康沫狂,材料科学进展,1990;4:161
5 杨全民,康沫狂,金属学报,1990;26:A235
6 Takezawa K, Sato S. Proc Inter Conf on Martensitic Transformation, Nara, The Japan Institute of Metals, 1986: 625
7 Takezawa K, Sato S. Metall. Trans., 1990; 21A: 1541
8 徐祖耀,上海金属,1991;13:7
9 徐祖耀,上海金属,1992;14:8
10 Meng X K, Kang M K, Yang Y Q, Liu D H. Metall. Trans., 1993; 24A: in press
11 杨全民,西北工业大学博士学位论文,西安,1989:32
12 Kang M K, Yang Y Q, Wei Q M, Meng X K. Metall. Trans., 1993; 24A: in press
13 张骥华,陈树川,徐祖耀,金属学报,1986;22:A372
14 张骥华,陈树川,徐祖耀,材料科学进展,1989;3:105
15 Zhao Z Q, Chen F X, Yang D Z. J Phys: Condens Matter, 1989; 1: 1395
16 赵增祺,陈绯瑕,杨大智,包耳,第二届全国贝氏体相变讨论会论文集,峨眉,1990;101
17 沈惠敏,芮煜明,张志方,袁方,王业宁,第三届全国马氏体相变会议论文集,秦皇岛;1990:137
18 张丽萍,李福全,张恩涛,邓肇豪,机械工程材料,1990;14:7
19 魏秋明,西北工业大学博士学位论文,西安,1991:30
20 Chattopadhyay K, Aaronson H I.Acta Metall., 1984; 34: 695
21 Guenin G, Cobin P F. Metall. Trans. 1982; 13A: 1127
22 Cliff G, Hasan F, Lorimer G W, Kikuchi M. Metall. Trans., 1990; 21A: 831
23 Wu M H, Wayman C M. Proc Inter Conf on Martensitic Transformation, Nara, The Japan Institute of Metals, 1986: 619q
No related articles found!