| THERMODYNAMICS OF Ga-In-As SYSTEM UNDER LATTICE DEFORMATION |
| SHEN Jianyun(General Research Institute for Non-Ferrous Metals;Beijing);CHATILLON C(Laboratoire de Thermodynamique et Physico-chimie Metallurgiques;Fracne)(Manuscript received 16 June;1993) |
|
Cite this article:
SHEN Jianyun(General Research Institute for Non-Ferrous Metals;Beijing);CHATILLON C(Laboratoire de Thermodynamique et Physico-chimie Metallurgiques;Fracne)(Manuscript received 16 June;1993). THERMODYNAMICS OF Ga-In-As SYSTEM UNDER LATTICE DEFORMATION. Acta Metall Sin, 1994, 30(16): 145-149.
|
|
|
Abstract The parameters of the thermodynamic model for the ternary system Ga-In-As are optimized from the available experimental data,and the influence of the elastic energy on the phase diagram,induced by the dismatch of the growing lattice with the substrate,is quantified.Correspondent:SHEN Jianyun,Laboratory No.301,(General Reserach Intitute for Non-Ferrous Metals,Beijins 100088)
|
|
|
| 1LukasHL,HenigET,ZimmermannB.Calphad1,1977:2252TmarM.PhDThesis,INPG,French,19853ShenJY.PhDThesis,INPG,French,19894SundmanB.ProcConfCalphadVIII,Stockholm,1979:1025HockingsEF,KudmanI,SiedelTE,SchmelzCM,SteigineierEF.JApplPhys,1966;37:28796MirtskhulavaAA,SakvarelidzeLG.RussJPhysChem,1977;51:3027VanHockHJ,LenkerES,TransMetallSocAIME,1963;227:2208WooleyJC,SmithBA.ProcPhysSocLondon,1958;B72:2149WangerJW.JElectrochemSoc,1970;117:119310RakovVV,UfimtsevVB.RussJPhysChem,1969;43:26711CremouxBDe.JPhysColloq,1982;43:C5-1 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|