| XPS STUDY ON TOUGHENING EFFECT OF Cr IN Fe_3Al |
| GAO Hiaomei; QIAN Xiangrong (Shanghai Iron and Steel Research Institute)(Manuscript received 3 May; 1993; in revised form 20 January; 1994) |
|
Cite this article:
GAO Hiaomei; QIAN Xiangrong (Shanghai Iron and Steel Research Institute)(Manuscript received 3 May; 1993; in revised form 20 January; 1994). XPS STUDY ON TOUGHENING EFFECT OF Cr IN Fe_3Al. Acta Metall Sin, 1994, 30(7): 307-311.
|
|
|
Abstract The room temperature ductility of Fe_3Al was improved by a suitable amount of Cr addition to the alloy, so as to form an oxide protective film.XPS study shows that the oxide film has a moderate amount of Al_2O_3, which is dense and protective enough to restrain and retard the reaction of environmental water vapour on Al. Thus the own intrinsic toughness of the alloy will fully be developed.Correspondent: QIAN Hiangrong, professor, Shanghai Iron and Steel Research institute, Shanghai 200940
|
|
Received: 18 July 1994
|
| 1BordeauRG.AFWAL-TR-87-4009.19872Horton,JA,LiuCT,KochCC.Bethesda,MarylandUSA,April9-11,1984:3093MckameyCG,HortonJA,MetallTrans,1989;20A:7514严文.高校科技,1990;5:55LiuCT,LeeEH,MckameyCG.ScrMetall,1989;23:8756LiuCT.MckameyCG.In:WhangSHed.HighTemperatureAluminidesandIntermetallics,TheMinerals,MetalsandMaterialsSociety,1990:1337LiuCT,MckameyCG,LeeEH.ScrMetallMater,1990;24:3858MckameyCG,LiuCT.ScrMetallMater,1990;24:21199GcstRJ,TroianoAR.Corrosion,1974;30:27410MorrisonSR著,赵璧英等译.表面化学物理.北京大学出版社,1984:267,37111LiuCT,LeeEH,HensonTJ.InitialDevelopmentofHigh-TemperatureTitaniumSilicideAlloys,OakRidgeNationalLaboratory,OakRidge,TN,ORNL-6435,1988> |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|