| CARBON ORDERING IN Fe-C MARTENSITE Ⅱ. Crystal Structure of Long-Period Ordered Phase |
| REN Xiaobing; Xiaotian(Xi'an Jiaotong University); SHIMIZU Ken'ichi(Kanazawa Institute of Technology;Japan) TADAKI Tsugio(Osaka University; Japan) |
|
Cite this article:
REN Xiaobing; Xiaotian(Xi'an Jiaotong University); SHIMIZU Ken'ichi(Kanazawa Institute of Technology;Japan) TADAKI Tsugio(Osaka University; Japan). CARBON ORDERING IN Fe-C MARTENSITE Ⅱ. Crystal Structure of Long-Period Ordered Phase. Acta Metall Sin, 1994, 30(8): 337-343.
|
|
|
Abstract Split superlattice reflections are detected in Fe-1 .83C martensite aged at room temperature, indicating the existence of long-period ordered phase. The long-period phase is superperiod of 10 c_M(c_M being the length of c axis of martensite), it is named as γ′-FexC(Ⅱ). For the first time it is found that the superperiod of this long-period phase increases with the increase of temperature, but does not change with aging time. It is also found that the superperiod calculated from the split distance of superlattice spots is not an integral multiple of C_M This is an indication of the coexistence of three long-period ordered phases with superperiod of 10 c_M 12 and 14 c_M, respectively, the interference of diffraction beams from them results in the non-integrality of the split distance of superlattice spots.The calculated intensities of the superlattice reflections are in good agreement with experimental observations. It is suggested that the existence of long-period ordered phase is a result of minimization of lattice distortion energy. The relationship betweenγ′-FexC(Ⅰ) and γ′-Fex C(Ⅱ) is also discussed.
|
|
Received: 18 August 1994
|
| 1NagakuraS,ToyoshimaM.TransJpnInstMet,1974;15:1292NagakuraS,HirotsuY,KusunokiM,NakaimuraYMetallTrans,1983;14A:10253TanakaY,ShimizuKTransJpnInstMet,1981;22:7794TaylorKA,ChangL,OlsonGB,SmithGDW,CohenM,VanderSandeJB.MetallTrans,1989;20A:27175UwakwehONC,GeninJMR,SilvainJGMetallTrans22A:7976OlsonCB,TaylorKA,CohenM.MetallTrans1990;21A:28067任晓兵,王笑天,清水谦一,唯木次男.金属学报,1994:30:A2968任晓兵,王笑天,清水谦一,唯木次男,金属学报,1994,30.A2899JohannsonCH,LindeJOAnnPhys,1936;25:110FujiwaraKJPhysSocJpn.1957,12:711OgawaSIn:WarlimountHedProcIntSymponOrder-DisorderTransformationsinAlloys,1974:24012YakelHLJApplPhys1962,13:243913GanguleeA,MossSC.JApplCrystallogr,1968;1:61 |