Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (8): 344-347    DOI:
Current Issue | Archive | Adv Search |
IN SITU OBSERVATION OF GROWTH OF BAINITE IN Fe-Ni ALLOY
YANG Liu; ZHU Degui; ZHANG Jun; CHEN Jian (Southwestern Jiaotong University; Chengdu)
Cite this article: 

YANG Liu; ZHU Degui; ZHANG Jun; CHEN Jian (Southwestern Jiaotong University; Chengdu). IN SITU OBSERVATION OF GROWTH OF BAINITE IN Fe-Ni ALLOY. Acta Metall Sin, 1994, 30(8): 344-347.

Download:  PDF(280KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  TEM is used to study the interface structure and the thickening kinetics of bainitic ferrite during isothermal transformation of an Fe-30wt-%Ni alloy with the hot stage. It is demonstrated that ferrite possesses ledge morphology with [111]b dislocations at the ferrite/austenite ledge interface. The experimentally measured ferrite thickening rate is shown to be of the same order with those calculated according to Zener-Hillert equation developed for the growth kinetics of ferrite controlled by the volume diffussion of carbon in austenite. All of the results are considered to be support for the ledge growth mechanism for the bainitic ferrite.
Key words:  bainitic ferrite      growth kinetics      ledge growth mechanism     
Received:  18 August 1994     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I8/344

1HehemannRF,KinsmanDR、AaronsonHI.MetallTrans,1972;3:10772KinsmanKR,EichenE,AaronsonHI.MetallTrans1975;6A:3033RigsbeeJM,AaronsonHI.ActaMetall,1979,27:3654CahnJW,HilligWB,SearsGW.ActaMetall,1964;12:14215ZenerC.TransAIME;1964;167:5506HillertM,JernkontoretsAnn,1957;141:757
[1] Huidong WU,Chi ZHANG,Wenbo LIU,Zhigang YANG. SIMULATION OF GROWTH KINETICS OF PRO-EUTECTOID FERRITE USING MIXED CONTROL MODEL WITH CONSIDERATION OF DISLOCATION INTERACTION[J]. 金属学报, 2015, 51(9): 1136-1144.
[2] Wenjing MA,Changbo KE,Minbo ZHOU,Shuibao LIANG,Xinping ZHANG. PHASE-FIELD CRYSTAL SIMULATION ON EVOLU- TION AND GROWTH KINETICS OF KIRKENDALL VOIDS IN INTERFACE AND INTERMETALLIC COMPOUND LAYER IN Sn/Cu SOLDERING SYSTEM[J]. 金属学报, 2015, 51(7): 873-882.
[3] KE Changbo, ZHOU Minbo, ZHANG Xinping. PHASE FIELD SIMULATION ON MICROSTRUCTURE EVOLUTION AND GROWTH KINETICS OF Cu6Sn5 INTERMETALLIC COMPOUND DURING EARLY INTERFACIAL REACTION IN Sn/Cu SOLDERING SYSTEM[J]. 金属学报, 2014, 50(3): 294-304.
[4] ZHOU Minbo, MA Xiao, ZHANG Xinping. THE INTERFACIAL REACTION AND INTERMETALLIC COMPOUND GROWTH BEHAVIOR OF BGA STRUC-TURE Sn-3.0Ag-0.5Cu/Cu SOLDER JOINT AT LOW REFLOW TEMPERATURES[J]. 金属学报, 2013, 49(3): 341-350.
[5] WANG Xixia, GUO Hui, WANG Ding, BAI Yin, YANG Shanwu, HE Xinlai. INFLUENCE OF COHERENT AUSTENITE TWIN BOUNDARIES ON THE VARIANT SELECTION OF BAINITIC FERRITE IN Fe-C-Mn-Si STEELS[J]. 金属学报, 2012, 48(4): 385-392.
[6] KE Changbo MA Xiao ZHANG Xinping. PHASE FIELD SIMULATION OF EFFECTS OF PORES ON B2-R PHASE TRANSFORMATION IN NiTi SHAPE MEMORY ALLOY[J]. 金属学报, 2011, 47(2): 129-139.
[7] LIU Zhiyuan YANG Zhigang LI Zhaodong LIU Zhenqing ZHANG Chi. SIMULATION OF LEDGEWISE GROWTH KINETICS OF PROEUTECTIOD FERRITE UNDER INTERFACIAL REACTION–DIFFUSION MIXED CONTROL MODEL[J]. 金属学报, 2010, 46(4): 390-395.
[8] KE Changbo MA Xiao ZHANG Xinping. PHASE FIELD SIMULATION OF GROWTH KINETICS OF COHERENT Ni4Ti3 PRECIPITATE IN NiTi SHAPE MEMORY ALLOY[J]. 金属学报, 2010, 46(1): 84-90.
[9] . MODELING DYNAMIC RECRYSTALLIZATION OF PURE COPPER USING CELLULAR AUTOMATON METHOD[J]. 金属学报, 2008, 44(3): 292-296 .
[10] . Refinement of Grain and Enhancement of Impact Energy Absorption for Low-Alloy Ultra-High Strength Bainite Steels Containing Silicon[J]. 金属学报, 2007, 43(3): 315-320 .
[11] LI Fengzhao; AO Qing; GU Yingni; JIANG Jiang; SUN Dongsheng (Shandong University of Technology; Jinan 250061)DAI Jiyan; PENG Hongying (Laboratory of Atomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015). TEM OBSERVATION OF THE FINE STRUCTURE OF BAINITE[J]. 金属学报, 1997, 33(3): 241-247.
[12] Correspondent: YANG Yanqing; Department of Physics; Nanjing University; Nanjing 210008 YANG Yanqing;LIU Donghui;KANG Mokuang;SUN Yuan Northwestern Polytechnical University Beijing Centre of Physical and Chemical Analysis. HIGH-TEMPERATURE TEM IN SITU STUDY OF GROWTH KINETICS OF BAINITE IN β BRASS[J]. 金属学报, 1992, 28(3): 1-5.
[13] JIN Qiang;FANG Hongsheng;CAO Jianjun;ZHENG Yankang;CHEN Xiuyun Tsinghua University; Beijing. LEDGE STRUCTURE AT BROAD FACES OF FERRITE PLATES IN LOWER BAINITE[J]. 金属学报, 1990, 26(6): 5-9.
No Suggested Reading articles found!