Abstract One-way and two-way shape memory effects of the Ni-34.6at.-% Al thin ribbon were observed. The ribbon of one-way shape memory effect, occuired over 300℃ , has very good shape recovery(100%). A ductile γ′-Ni_3Al phase precipitated out up to 16 v.-%after high temperature annealing. Both ductility and toughness were further improved.Meanwhile, the annealed ribbon has also good one-way and two-way high temperature shape memory effects. It is believed that the Ni-riched NiAI alloy may possibly develop into a new high temperature shape memory alloy.Correspondent: CHENG Tianyi, associate professor, Beijing institute of Technology, Beijing 100081
|
Received: 18 September 1994
|
1KainumaR,NakanoH,OikanaK,IshidaK,NishizawaT.ProcoftheMaterialsResearchSocietySymposium,Pittsburgh,1992;246:4032KainumaR,IshidaK,NishizawaT.MetallTrans,1992;23A:11473LiuCT,SparksCJ,HortonJA,GeorgeEF,CamichaelCA,KaoM,KunsmannR.ProcoftheMaterialsResearchSocictySymposium,Pittsburgh,1992;246:1694DaroliaRInDaroliaRLewandowskiJJ,LiuCT,MartinPL,MiracleDB,NathalMV.StructuralIntermetallics,Warrendale,TMS,1993:4955ChengTianyi.JMaterSci,1993;28:59096程天一.材料研究学报,待发表7ChengTianyi.JNanostructuralMater,1993:2:198程天一,章守华.快速凝固技术与新型合金,北京:宇航出版社,1990;319ChengTianyi.ScrMetallMater,1994;30:33110KimYD,WaymanCM.ScrMetallMater,1990;24:24511HortonJD,GeorgeEP,SparksCJ,KaoM,CarinOB,ThomaP.ProcoftheMaterialsResearchSocietySymposium,Pittsburgh,1992;246:6112SmialekJL,HehemannRF.MetallTrans,1973;4:157113EnamiK,NennoS.MetallTrans,1971;2:148714AuYK,WaymanCM.ScrMetall,1972;6:1209 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|