| DIRECTIONAL COARSENING OF γ'PRECIPITATES IN A SINGLE CRYSTAL NICKEL BASE SUPERALLOY |
| PENG Zhifang (Wuhan University of Hydraulic and Electric Engineering; Wuhan 430072); GLATZEL Uwe; FELLER-KNIEPMEIER Monika(Technische Universitat Berlin; Germany) |
|
Cite this article:
PENG Zhifang (Wuhan University of Hydraulic and Electric Engineering; Wuhan 430072); GLATZEL Uwe; FELLER-KNIEPMEIER Monika(Technische Universitat Berlin; Germany). DIRECTIONAL COARSENING OF γ'PRECIPITATES IN A SINGLE CRYSTAL NICKEL BASE SUPERALLOY. Acta Metall Sin, 1995, 31(12): 531-536.
|
|
|
Abstract The coarsening of γ'precipitates along the direction perpendicular to the externally applied stress axis was investigated for [001]-oriented single crystal superalloy CMSX-4 under 1253 K, 350 MPa tensile creep test. It is found that the portion of edge areas of cuboidal γ'precipitates grew preferentially and the γ-γ'interfaces progressed concavely,which was followed by the enclosure of the adjacent vertical matrix channels (parallel to [001]), and the linked γ'precipitates gradually exhauseted the retained vertical channels and finally developed into rafted plates. The directional coarsening led to a decrease in the size of γ'precipitates in the [001] direction and to an increase in the width of the horizontal matrix channels (perpendicular to[001]). The specific growth manner of the γ'precipitates and the characteristics of the morphological evolution of the two coherent phases in the tested samples are discussed.
|
|
|
| 1TienJK,CoplySM.MetallTrans,1971;2:2152NathalMV,EbertLJ.ScriptaMetall,1983:17,11513MackayRA,EbertLJ.ScriptaMetall,1983:17,12174Feller-KniepmeierM,LinkT.MetallTrans,1989;20A:12335GaydaJ,MackayRA.ScriptaMetall,1989;23:18356SchmidtR,Feller-KniepmeierM.ScriptaMetalletMater,1993;29:10797SocrateS,ParksDM.ActaMetallMater,1993;41(7):21858PollockTM,ArgonAS.ActaMetallMater,1994;42(6):18599郭喜平,傅恒志,孙家华.金属学报,1994;30(7):A32110GlatzelU.MicrostructureandInternalStrainsofUndeformedandCreepDeformedSamplesofaNickel-BaseSuperalloyBerlin:VerlagDr.Koster,1994:17" |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|