CRACK INITIATION OF SUPERPURE STAINLESS STEEL DURING LOW CYCLE CORROSION FATIGUE IN 3.5% NaCl SOLUTION
WANG Jianqiu; LI Jing; WANG Zhengfu; ZHU Ziyong; KE Wei (Corrosion science laboratory; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences; Shenyang 110015); ZANG Qishan; WANG Zhongguang (Key laboratory of fatigue and fracture; Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015)
Cite this article: 

WANG Jianqiu; LI Jing; WANG Zhengfu; ZHU Ziyong; KE Wei (Corrosion science laboratory; Institute of Corrosion and Protection of Metals; Chinese Academy of Sciences; Shenyang 110015); ZANG Qishan; WANG Zhongguang (Key laboratory of fatigue and fracture; Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015). CRACK INITIATION OF SUPERPURE STAINLESS STEEL DURING LOW CYCLE CORROSION FATIGUE IN 3.5% NaCl SOLUTION. Acta Metall Sin, 1995, 31(15): 103-108.

Download:  PDF(514KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The behaviour of crack initiation of superpure stainless steel in 3.5% NaCl solution during low cycle corrosion fatiguing was studied by using three-electrode technique.The deformation may induce pitting at the passive potential which is less than the static pitting potential, but pitting was not found to initiate cracks. At low strain rate, the cracks were observed to initiate along the persistent slip bands(PSBs), and the electrochemical etching occurred at the PSBs. At high strain rate the cracks initiated at grain boundaries were obsereved. The results showed that the electrochemical dissolution accelerated the crack initiation process. and pitting at the localized deformed sites did not form the cracks at the passive system. And the strain rate affected the crack initiation mode.
Key words:  crack initiation      pitting      passivation      low cycle corrosion fatigue      strain rate      superpure stainless steel      Fe-26Cr-1 Mo     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I15/103

1McAdamDJ.ProcASTM,1928:41:6962WhitwhamD.JJSI,1950;165:763GreenfieldIG.CorrosionFatigue:ChemistryMechanicsandMicrostructure,1971:1334RebinderP,Physico-chemicalMechanicsofMetals,AcademiaofScienceUSSRisrdelProgramforScientificTranslation,Jerusalen1964:125YanBD,LairdC.ActaMetall,1985;33:15336WANGJianqiu,WANGZhongguang,MAMinya,ZANGQisan,ZHUZiyong,SteelRes,1992;63:4537WangJQ,LiJ,WangZF,ZhuZY,KeW,ZangQS,WangZG,ScriptaMetall,1993;29:14158MughrabiH.PhylosMag,1976;33:963
[1] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[2] WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei. Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K[J]. 金属学报, 2023, 59(2): 277-288.
[3] XIA Dahai, JI Yuanyuan, MAO Yingchang, DENG Chengman, ZHU Yu, HU Wenbin. Localized Corrosion Mechanism of 2024 Aluminum Alloy in a Simulated Dynamic Seawater/Air Interface[J]. 金属学报, 2023, 59(2): 297-308.
[4] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[5] HU Wenbin, ZHANG Xiaowen, SONG Longfei, LIAO Bokai, WAN Shan, KANG Lei, GUO Xingpeng. Corrosion Behavior of AlCoCrFeNi2.1 Eutectic High-Entropy Alloy in Sulfuric Acid Solution[J]. 金属学报, 2023, 59(12): 1644-1654.
[6] WANG Nan, CHEN Yongnan, ZHAO Qinyang, WU Gang, ZHANG Zhen, LUO Jinheng. Effect of Strain Rate on the Strain Partitioning Behavior of Ferrite/Bainite in X80 Pipeline Steel[J]. 金属学报, 2023, 59(10): 1299-1310.
[7] SUN Yangting, LI Yiwei, WU Wenbo, JIANG Yiming, LI Jin. Effect of Inclusions on Pitting Corrosion of C70S6 Non-Quenched and Tempered Steel Doped with Ca and Mg[J]. 金属学报, 2022, 58(7): 895-904.
[8] CHEN Yang, MAO Pingli, LIU Zheng, WANG Zhi, CAO Gengsheng. Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact[J]. 金属学报, 2022, 58(5): 660-672.
[9] ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue. Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels[J]. 金属学报, 2022, 58(2): 193-205.
[10] HUANG Yichuan, WANG Qing, ZHANG Shuang, DONG Chuang, WU Aimin, LIN Guoqiang. Optimization of Stainless Steel Composition for Fuel Cell Bipolar Plates[J]. 金属学报, 2021, 57(5): 651-664.
[11] LV Chenxi, SUN Yangting, CHEN Bin, JIANG Yiming, LI Jin. Influence of Potentionstatic Pulse Technique on Pitting Behavior and Pitting Resistance of 317L Stainless Steel[J]. 金属学报, 2021, 57(12): 1607-1613.
[12] WANG Li,DONG Chaofang,ZHANG Dawei,SUN Xiaoguang,Chowwanonthapunya Thee,MAN Cheng,XIAO Kui,LI Xiaogang. Effect of Alloying Elements on Initial Corrosion Behavior of Aluminum Alloy in Bangkok, Thailand[J]. 金属学报, 2020, 56(1): 119-128.
[13] Kaiqiang LI, Lujia YANG, Yunze XU, Xiaona WANG, Yi HUANG. Influence of SO42- on the Corrosion Behavior of Q235B Steel Bar in Simulated Pore Solution[J]. 金属学报, 2019, 55(4): 457-468.
[14] FENG Hao,LI Huabing,LU Pengchong,YANG Chuntian,JIANG Zhouhua,WU Xiaolei. Investigation on Microbiologically Influenced Corrosion Behavior of CrCoNi Medium-Entropy Alloy byPseudomonas Aeruginosa[J]. 金属学报, 2019, 55(11): 1457-1468.
[15] Xiangru GUO, Chaoyang SUN, Chunhui WANG, Lingyun QIAN, Fengxian LIU. Investigation of Strain Rate Effect by Three-Dimensional Discrete Dislocation Dynamics for fcc Single Crystal During Compression Process[J]. 金属学报, 2018, 54(9): 1322-1332.
No Suggested Reading articles found!