Please wait a minute...
Acta Metall Sin  2026, Vol. 62 Issue (7): 1297-1309    DOI: 10.11900/0412.1961.2024.00322
Research paper Current Issue | Archive | Adv Search |
Molecular Dynamics Simulations of Tensile Deformation of Cu/Ta Nano-Bilayer Films and the Effect of Al and W Atoms Doping on the Deformation
SHI Tenglong1,2, CHEN Juan2, ZHAO Bin3, SHI Junqin1()
1 Center of Advanced Lubrication and Seal Materials, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi'an 710072, China
2 School of Materials Science and Engineering, Taiyuan University of Science and Technology, Taiyuan 030024, China
3 Xi'an Surface Material Protection Co. Ltd., Xi'an 710200, China
Cite this article: 

SHI Tenglong, CHEN Juan, ZHAO Bin, SHI Junqin. Molecular Dynamics Simulations of Tensile Deformation of Cu/Ta Nano-Bilayer Films and the Effect of Al and W Atoms Doping on the Deformation. Acta Metall Sin, 2026, 62(7): 1297-1309.

Download:  HTML  PDF(5703KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Nano-multilayers composed of immiscible metals have been widely investigated over the past decades due to their exceptional microstructural stability. The Cu/Ta system, which is also immiscible, is particularly notable because Ta offers higher melting point, strength, and superior wear and corrosion resistance compared to metals like Nb. Cu/Ta nano-bilayer films are extensively used in the electronics industry for semiconductors, microelectronic devices, optical systems, and magnetic applications. However, the presence of interfaces and the distinct deformation responses of the Cu and Ta layers during processing, fabrication, and service conditions make mechanical deformation and subsequent failure inevitable, potentially compromising the performance of microscale devices. Therefore, understanding the deformation mechanisms and enhancing the mechanical strength of Cu/Ta nano-bilayer films at the microscopic scale is essential. In this study, molecular dynamics simulations were employed to investigate the tensile behavior and deformation mechanisms of Cu/Ta nano-bilayer films. In addition, the effects of Al and W doping in the Cu layer on the deformation behavior were analyzed. The results indicate that tensile loading direction significantly influences the plastic deformation mode. When the bilayer films were stretched parallel to the interface, both Cu and Ta layers exhibited sequential plastic deformation. In contrast, when the loading was applied perpendicular to the interface, only the Cu layer deformed plastically, while the Ta layer remained elastically constrained throughout. Doping with Al or W atoms enhanced the overall hardness and yield strength of the nano-bilayer films. Furthermore, W doping induced stacking faults in both loading directions when stretched parallel to the interface, and a martensitic transformation from fcc to bcc structure occurred in the Cu layer under perpendicular tension.

Key words:  Cu/Ta interface      stretching deformation      alloying strengthening      molecular dynamics     
Received:  11 September 2024     
ZTFLH:  TG146.1  
Fund: National Science and Technology Major Project(2025ZD0618600);Science and Technology Plan Project of Xi'an(24ZDCYJSGG0050)
Corresponding Authors:  SHI Junqin, associate professor, Tel: (029)88460311, E-mail: junqin.shi@nwpu.edu.cn

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2024.00322     OR     https://www.ams.org.cn/EN/Y2026/V62/I7/1297

Fig.1  Molecular dynamics models of Cu/Ta (a), Cu95Al5/Ta (b), and Cu95W5/Ta (c) nano-bilayer films, and interfacial mismatch network structure (d)
Fig.2  Stress-strain curves for stretching for each model
(a) parallel to the interface direction (X direction)
(b) perpendicular to the interface direction (Z direction)
Fig.3  Crystal structures of Cu/Ta bilayer films at different strains during stretching along X direction (ε—strain. Dashed lines indicate the interfaces between different structures, the same below)
(a) ε = 0.063 (b) ε = 0.066 (c) ε = 0.085 (d) ε = 0.163 (e) ε = 0.169 (f) ε = 0.260
Fig.4  Crystal structures of Cu95Al5/Ta bilayer films at different strains during stretching along X direction
(a) ε = 0.060 (b) ε = 0.070 (c) ε = 0.100 (d) ε = 0.155 (e) ε = 0.175 (f) ε = 0.260
Fig.5  Crystal structures of Cu95W5/Ta bilayer films at different strains during stretching along X direction
(a) ε = 0.050 (b) ε = 0.075 (c) ε = 0.090 (d) ε = 0.140 (e) ε = 0.170 (f) ε = 0.260
Fig.6  Variation curves of the number of atoms of Cu (a1-c1) and Ta (a2-c2) layers with different crystal structures for models Cu/Ta (a1, a2), Cu95Al5/Ta (b1, b2), and Cu95W5/Ta (c1, c2) bilayer films during the stretching process along X direction
Fig.7  Dislocation structures of Cu/Ta (a-c), Cu95Al5/Ta (d-f), and Cu95W5/Ta (g-i) bilayer films at different strains during stretching process along X direction
(a) ε = 0.063 (b) ε = 0.169 (c) ε = 0.260
(d) ε = 0.060 (e) ε = 0.175 (f) ε = 0.260
(g) ε = 0.050 (h) ε = 0.170 (i) ε = 0.260
Fig.8  Variation curves of the dislocation line lengths in Cu (a1-c1) and Ta (a2-c2) layers for Cu/Ta (a1, a2), Cu95Al5/Ta (b1, b2), and Cu95W5/Ta (c1, c2) bilayer film models during the stretching process along X direction
Fig.9  Crystal structures of Cu/Ta bilayer films at different strains during stretching along Z direction
(a) ε = 0.042 (b) ε = 0.060 (c) ε = 0.150 (d) ε = 0.190
Fig.10  Crystal structures of Cu95Al5/Ta bilayer films at different strains during stretching along Z direction
(a) ε = 0.030 (b) ε = 0.042 (c) ε = 0.150 (d) ε = 0.200
Fig.11  Crystal structures of Cu95W5/Ta bilayer films at different strains during stretching along Z direction
(a) ε = 0.014 (b) ε = 0.030 (c) ε = 0.150 (d) ε = 0.210
Fig.12  Schematics of internal defects at the initial strain (ε = 0) (a1-c1) and dislocation structure generation during stretching along the Z direction (a2-c2) for Cu/Ta (a1, a2), Cu95Al5/Ta (b1, b2), and Cu95W5/Ta (c1, c2) bilayer film models
(a2) ε = 0.042 (b2) ε = 0.030 (c2) ε = 0.014
Fig.13  Variation curves of the number of different types of atoms (a1-c1) and the length of dislocation lines (a2-c2) during stretching along Z direction for models Cu/Ta (a1, a2), Cu95Al5/Ta (b1, b2), and Cu95W5/Ta (c1, c2)
[1] Chen H B. Fabrication and property of Ta-based diffusion barrier for Cu interconnection in new generation IC [D]. Changsha: Central South University, 2007
陈海波. 新一代集成电路Cu互连用Ta基扩散阻挡层的制备及特性研究 [D]. 长沙: 中南大学, 2007
[2] Holloway K, Fryer P M, Cabral Jr C, et al. Tantalum as a diffusion barrier between copper and silicon: Failure mechanism and effect of nitrogen additions [J]. J. Appl. Phys., 1992, 71: 5433
doi: 10.1063/1.350566
[3] Fullwood D T, Niezgoda S R, Adams B L, et al. Microstructure sensitive design for performance optimization [J]. Prog. Mater. Sci., 2010, 55: 477
doi: 10.1016/j.pmatsci.2009.08.002
[4] Mondal S, Polley D, Pattabi A, et al. Single-shot switching in Tb/Co-multilayer based nanoscale magnetic tunnel junctions [J]. J. Magn. Magn. Mater., 2023, 581: 170960
doi: 10.1016/j.jmmm.2023.170960
[5] Sakhonenkov S S, Filatova E O. Nanoscale W/Be multilayers: Intermixing during magnetron sputtering deposition and effect of heat treatment [J]. Appl. Surf. Sci., 2022, 571: 151265
doi: 10.1016/j.apsusc.2021.151265
[6] Tran A S, Fang T H. Dislocation interaction and fracture of Cu/Ta bilayer interfaces [J]. Phys. Scr., 2019, 94: 095402
[7] Feng X T, Lin Z J, Xin K, et al. The deformation mechanisms and mechanical properties of Cu/Fe multilayer during compression process [J]. J. Mater. Res., 2021, 36: 3203
doi: 10.1557/s43578-021-00333-z
[8] Zhang R F, Wang J, Beyerlein I J, et al. Dislocation nucleation mechanisms from fcc/bcc incoherent interfaces [J]. Scr. Mater., 2011, 65: 1022
doi: 10.1016/j.scriptamat.2011.09.008
[9] Chen Y, Li N, Hoagland R G, et al. Effects of three-dimensional Cu/Nb interfaces on strengthening and shear banding in nanoscale metallic multilayers [J]. Acta Mater., 2020, 199: 593
doi: 10.1016/j.actamat.2020.08.019
[10] Wang Y, Zhu X Y, Liu G M, et al. Strain rate sensitivity of Cu/Ni and Cu/Nb nanoscale multilayers [J]. Acta Metall. Sin., 2017, 53: 183
王 尧, 朱晓莹, 刘贵民 等. Cu/Ni和Cu/Nb纳米多层膜的应变率敏感性 [J]. 金属学报, 2017, 53: 183
[11] Zhang R F, Wang J, Beyerlein I J, et al. Atomic-scale study of nucleation of dislocations from fcc-bcc interfaces [J]. Acta Mater., 2012, 60: 2855
doi: 10.1016/j.actamat.2012.01.050
[12] Lu L, Huang C, Pi W L, et al. Molecular dynamics simulation of effects of interface imperfections and modulation periods on Cu/Ta multilayers [J]. Comp. Mater. Sci., 2018, 143: 63
doi: 10.1016/j.commatsci.2017.10.034
[13] Shi T L, Xu L L, Chen J, et al. Influence of grain boundary and twin boundary on the stretching deformation behaviors of Cu/Ta interface material [J]. Mater. Today Commun., 2024, 39: 108633
[14] Tu A D, Teng C Y, Wang H, et al. Molecular dynamics simulation of the structure and deformation behavior of γ/α2 interface in TiAl alloys [J]. Acta Metall. Sin., 2019, 55: 291
涂爱东, 滕春禹, 王 皞 等. Ti-Al合金γ/α2界面结构及拉伸变形行为的分子动力学模拟 [J]. 金属学报, 2019, 55: 291
doi: 10.11900/0412.1961.2018.00182
[15] Karimzadeh A, Rouhaghdam A S, Aliofkhazraei M, et al. Sliding wear behavior of Ni-Co-P multilayer coatings electrodeposited by pulse reverse method [J]. Tribol. Int., 2020, 141: 105914
doi: 10.1016/j.triboint.2019.105914
[16] Major L, Lackner J M, Kot M, et al. Nanostructural aspects of the wear process of multilayer tribological coatings [J]. Tribol. Int., 2020, 151: 106411
doi: 10.1016/j.triboint.2020.106411
[17] Shi J Q, Li L L, Wang J Y, et al. Alloy strengthening toward improving mechanical and tribological performances of Cu x Ni100 - x /Ta nano multilayer materials [J]. Tribol. Int., 2023, 190: 109039
doi: 10.1016/j.triboint.2023.109039
[18] Bai Z W, Ding Z G, Zhou A L, et al. Molecular dynamics simulation of thermo-kinetics of tensile deformation of α-Fe single crystal [J]. Acta Metall. Sin., 2024, 60: 848
柏智文, 丁志刚, 周爱龙 等. α-Fe单晶拉伸变形热-动力学的分子动力学模拟 [J]. 金属学报, 2024, 60: 848
doi: 10.11900/0412.1961.2022.00606
[19] Zhang J Y, Qu Q M, Wang Y Q, et al. Research progress on irradiation effects and mechanical properties of metal/high-entropy alloy nanostructured multilayers [J]. Acta Metall. Sin., 2022, 58: 1371
doi: 10.11900/0412.1961.2022.00113
张金钰, 屈启蒙, 王亚强 等. 金属/高熵合金纳米多层膜的力学性能及其辐照效应研究进展 [J]. 金属学报, 2022, 58: 1371
doi: 10.11900/0412.1961.2022.00113
[20] Abraham F F. Computational statistical mechanics methodology, applications and supercomputing [J]. Adv. Phys., 1986, 35: 1
doi: 10.1080/00018738600101851
[21] Stukowski A. Structure identification methods for atomistic simulations of crystalline materials [J]. Modell. Simul. Mater. Sci. Eng., 2012, 20: 045021
[22] Choudhuri D, Srinivasan S G, Mishra R S. Deformation of lamellar FCC-B2 nanostructures containing Kurdjumov-Sachs interfaces: Relation between interfacial structure and plasticity [J]. Int. J. Plast., 2020, 125: 191
doi: 10.1016/j.ijplas.2019.09.014
[23] Zhou Q, Ren Y, Du Y, et al. Cracking and toughening mechanisms in nanoscale metallic multilayer films: A brief review [J]. Appl. Sci., 2018, 8: 1821
doi: 10.3390/app8101821
[24] Mendelev M I, Han S, Srolovitz D J, et al. Development of new interatomic potentials appropriate for crystalline and liquid iron [J]. Philos. Mag., 2003, 83: 3977
doi: 10.1080/14786430310001613264
[25] Wei M Z, Cao Z H, Shi J, et al. Anomalous plastic deformation in nanoscale Cu/Ta multilayers [J]. Mater. Sci. Eng., 2014, A598: 355
[26] Zhao X, Lu C, Tieu A K, et al. Deformation mechanisms and slip-twin interactions in nanotwinned body-centered cubic iron by molecular dynamics simulations [J]. Comput. Mater. Sci., 2018, 147: 34
[27] An M R, Song H Y, Deng Q, et al. Influence of interface with mismatch dislocations on mechanical properties of Ti/Al nanolaminate [J]. J. Appl. Phys., 2019, 125: 165307
doi: 10.1063/1.5085455
[28] Liu Y, Yang K M, Hay J, et al. The effect of coherent interface on strain-rate sensitivity of highly textured Cu/Ni and Cu/V multilayers [J]. Scr. Mater., 2019, 162: 33
doi: 10.1016/j.scriptamat.2018.10.021
[29] Yin F X, Zhao Y Z, Yu S Y, et al. Molecular dynamics studies on the interface evolution characteristics and deformation mechanisms of Cu/Al multilayers during compression process [J]. J. Appl. Phys., 2019, 125: 025112
[30] Eder S J, Rodríguez Ripoll M, Cihak-Bayr U, et al. Unraveling and mapping the mechanisms for near-surface microstructure evolution in CuNi alloys under sliding [J]. ACS Appl. Mater. Interfaces, 2020, 12: 32197
doi: 10.1021/acsami.0c09302
[31] Wang J Y, Shi J Q, Lu Y, et al. Deformation evolution of Cu/Ta nanoscale multilayer during nanoindentation by a molecular dynamics study [J]. Surf. Coat. Technol., 2022, 441: 128562
doi: 10.1016/j.surfcoat.2022.128562
[32] Shi J Q, Wang J Y, Yi X B, et al. Nanoscratching-induced plastic deformation mechanism and tribology behavior of Cu/Ta bilayer and multilayer by a molecular dynamics study [J]. Appl. Surf. Sci., 2022, 586: 152775
doi: 10.1016/j.apsusc.2022.152775
[33] Wang T, Jin L, Shi T L, et al. Effect of Al and W atom doping on the deformation mechanism and tribological properties of Cu95 X5/Ta nanobilayer by molecular dynamics simulation [J]. Tribol. Int., 2025, 210: 110818
doi: 10.1016/j.triboint.2025.110818
[34] Faken D, Jónsson H. Systematic analysis of local atomic structure combined with 3D computer graphics [J]. Comput. Mater. Sci., 1994, 2: 279
doi: 10.1016/0927-0256(94)90109-0
[35] Stukowski A, Bulatov V V, Arsenlis A. Automated identification and indexing of dislocations in crystal interfaces [J]. Modell. Simul. Mater. Sci. Eng., 2012, 20: 085007
[36] Fu E G, Li N, Misra A, et al. Mechanical properties of sputtered Cu/V and Al/Nb multilayer films [J]. Mater. Sci. Eng., 2008, A493: 283
[37] Bain E C. Factors affecting the inherent hardenability of steel [J]. J. Heat Treat., 1979, 1: 57
[38] Burgers W G. On the process of transition of the cubic-body-centered modification into the hexagonal-close-packed modification of zirconium [J]. Physica, 1934, 1: 561
doi: 10.1016/S0031-8914(34)80244-3
[39] Bertin N, Carson R, Bulatov V V, et al. Crystal plasticity model of BCC metals from large-scale MD simulations [J]. Acta Mater., 2023, 260: 119336
doi: 10.1016/j.actamat.2023.119336
[1] JIANG Guolong, ZHOU Xia. Molecular Dynamics Simulation on the Interfacial Behavior of Mg/Mg-Zn-Al Brazing with Ultrasonic Assistance[J]. 金属学报, 2026, 62(2): 372-382.
[2] YUAN Hang, ZHANG Yanyun, WANG Cong. Influence of MnO upon Electrical Conductive Mechanisms of Submerged Arc Welding Fluxes: Insights from Ab Initio Molecular Dynamics Simulations[J]. 金属学报, 2026, 62(1): 191-202.
[3] ZHOU Tingting, ZHAO Fuqi, ZHOU Hongqiang, ZHANG Fengguo, YIN Jianwei. Mechanism and Damage Model for the Dynamic Tensile Fracture of Liquid Aluminum Containing He Bubbles[J]. 金属学报, 2025, 61(4): 643-652.
[4] WANG Shucheng, PENG Ping. On the Homogeneous Nucleation Characteristics of Al Droplets During Isothermal Crystallization[J]. 金属学报, 2025, 61(12): 1925-1932.
[5] BAI Zhiwen, DING Zhigang, ZHOU Ailong, HOU Huaiyu, LIU Wei, LIU Feng. Molecular Dynamics Simulation of Thermo-Kinetics of Tensile Deformation of α-Fe Single Crystal[J]. 金属学报, 2024, 60(6): 848-856.
[6] MENG Zikai, MENG Zhichao, GAO Changyuan, GUO Hui, CHEN Hansen, CHEN Liutao, XU Dongsheng, YANG Rui. Molecular Dynamics Simulation of Creep Mechanism in Nanocrystalline α-Zirconium Under Various Conditions[J]. 金属学报, 2024, 60(5): 699-712.
[7] REN Junqiang, SHAO Shan, WANG Qi, LU Xuefeng, XUE Hongtao, TANG Fuling. Molecular Dynamics Simulation of Tensile Mechanical Properties and Deformation Mechanism of Oxygen-Containing Nano-Polycrystalline α-Ti[J]. 金属学报, 2024, 60(2): 220-230.
[8] LIU Shi, HUANG Jiawei, WU Jing. Application of Machine Learning Force Fields for Modeling Ferroelectric Materials[J]. 金属学报, 2024, 60(10): 1312-1328.
[9] CHEN Mingyi, HU Junwei, YU Yaochen, NIU Haiyang. Advances in Machine Learning Molecular Dynamics to Assist Materials Nucleation and Solidification Research[J]. 金属学报, 2024, 60(10): 1329-1344.
[10] LI Zhishang, ZHAO Long, ZONG Hongxiang, DING Xiangdong. Machine-Learning Force Fields for Metallic Materials: Phase Transformations and Deformations[J]. 金属学报, 2024, 60(10): 1388-1404.
[11] LI Haiyong, LI Saiyi. Effect of Temperature on Migration Behavior of <111> Symmetric Tilt Grain Boundaries in Pure Aluminum Based on Molecular Dynamics Simulations[J]. 金属学报, 2022, 58(2): 250-256.
[12] LIANG Jinjie, GAO Ning, LI Yuhong. Interaction Between Interstitial Dislocation Loop and Micro-Crack in bcc Iron Investigated by Molecular Dynamics Method[J]. 金属学报, 2020, 56(9): 1286-1294.
[13] LI Yuancai, JIANG Wugui, ZHOU Yu. Effect of Nanopores on Tensile Properties of Single Crystal/Polycrystalline Nickel Composites[J]. 金属学报, 2020, 56(5): 776-784.
[14] LI Yuancai, JIANG Wugui, ZHOU Yu. Effect of Temperature on Mechanical Propertiesof Carbon Nanotubes-Reinforced Nickel Nano-Honeycombs[J]. 金属学报, 2020, 56(5): 785-794.
[15] LI Meilin, LI Saiyi. Motion Characteristics of <c+a> Edge Dislocation on the Second-Order Pyramidal Plane in Magnesium Simulated by Molecular Dynamics[J]. 金属学报, 2020, 56(5): 795-800.
No Suggested Reading articles found!