| Research Progress on Laser Cladding of Refractory High-Entropy Alloy Coatings |
XIA Xingchuan1( ), ZHANG Enkuan1, DING Jian1, WANG Yujiang2, LIU Yongchang3 |
1 School of Material Science and Engineering, Hebei University of Technology, Tianjin 300401, China 2 National Key Laboratory for Remanufacturing, Army Academy of Armored Forces, Beijing 100072, China 3 School of Material Science and Engineering, Tianjin University, Tianjin 300072, China |
|
Cite this article:
XIA Xingchuan, ZHANG Enkuan, DING Jian, WANG Yujiang, LIU Yongchang. Research Progress on Laser Cladding of Refractory High-Entropy Alloy Coatings. Acta Metall Sin, 2025, 61(1): 59-76.
|
|
|
Abstract Refractory high-entropy alloys (RHEAs) have emerged as an innovative and promising class of high-entropy alloys that are primarily composed of multiple refractory elements, such as Ta, Nb, Mo, W, and Hf. These elements confer to the RHEAs with exceptional mechanical properties at high temperature, including excellent strength and stability. In addition to their desirable high-temperature performance, RHEAs also exhibit remarkable resistance to oxidation, wear, corrosion, and radiation. These resistance characteristics grant them potential as application materials in extreme environments, such as aerospace, nuclear reactors, and high-performance industrial machinery. As application materials, RHEAs have attracted evergrowing attention as the candidate materials to replace the traditional nickel-based superalloys due to their single solid solution phases and excellent stability in terms of structure and performance. Although they are promising, RHEAs fabricated using traditional methods, such as casting and powder metallurgy, present several shortcomings that limit their widespread application. It is often difficult to achieve a uniform composition in RHEAs that are prepared by conventional arc melting, which results in significant elemental segregation. Additionally, the size of the ingots prepared by this way is restricted to a small, button-like scale due to the limitations of the casting molds. These drawbacks significantly restrict the development, customization, and application of RHEAs in various industries, underscoring the need for advanced manufacturing techniques that can overcome these restrictions. Laser additive manufacturing (LAM) has emerged as a transformative approach to addressing the abovementioned challenges. By utilizing a high-energy density laser beam as a heat source, LAM enables a “discrete-stacking” or layer-by-layer forming process that can be precisely controlled through computer-aided design. This process offers exceptional flexibility in the manufacture of complex shapes, the fine-tuning of alloy composition, and the achievement of a uniform microstructure, thereby minimizing problems such as elemental segregation. Additionally, laser cladding (LC), which is a subset of LAM, provides the ability to deposit coatings that demonstrate superior mechanical and chemical properties to the surface of substrates, which further expands the application potential of RHEAs. This study presents a comprehensive review of current research on the LC of RHEAs while focusing on the unique microstructures and properties of RHEA coatings (RHEACs). It delves into the influences of alloy composition and processing parameters on the phase composition, microstructure, microhardness, as well as abrasion, oxidation, and corrosion resistances of RHEACs. Furthermore, this review discusses the evolution of RHEAC microstructure during the LC process and how it affects the performance of the coatings. Lastly, this review summarizes the current state of research on LC-RHEAs and outlines future development trends. It also highlights key challenges such as optimizing processing parameters, improving coating-substrate bonding, and tailoring microstructures for enhanced performance to guide future research studies and industrial applications.
|
|
Received: 08 May 2024
|
|
|
| Fund: Special Project of Local Science and Technology Development Guided by the Central Government of China(236Z1007G);National Natural Science Foundation of China(52175312) |
Corresponding Authors:
XIA Xingchuan, professor, Tel: (022)60202011, E-mail: xc_xia@hebut.edu.cn
|
| 1 |
Senkov O N, Gorsse S, Miracle D B. High temperature strength of refractory complex concentrated alloys[J]. Acta Mater., 2019, 175: 394
doi: 10.1016/j.actamat.2019.06.032
|
| 2 |
Wang F L, Balbus G H, Xu S Z, et al. Multiplicity of dislocation pathways in a refractory multiprincipal element alloy[J]. Science, 2020, 370: 95
doi: 10.1126/science.aba3722
pmid: 33004516
|
| 3 |
Yeh J W, Chen S K, Lin S J, et al. Nanostructured high-entropy alloys with multiple principal elements: Novel alloy design concepts and outcomes[J]. Adv. Eng. Mater., 2004, 6: 299
|
| 4 |
Senkov O N, Wilks G B, Miracle D B, et al. Refractory high-entropy alloys[J]. Intermetallics, 2010, 18: 1758
|
| 5 |
Senkov O N, Wilks G B, Scott J M, et al. Mechanical properties of Nb25Mo25Ta25W25 and V20Nb20Mo20Ta20W20 refractory high entropy alloys[J]. Intermetallics, 2011, 19: 698
|
| 6 |
Nutor R K, Cao Q P, Wang X D, et al. Phase selection, lattice distortions, and mechanical properties in high-entropy alloys[J]. Adv. Eng. Mater., 2020, 22: 2000466
|
| 7 |
Mills L H, Emigh M G, Frey C H, et al. Temperature-dependent tensile behavior of the HfNbTaTiZr multi-principal element alloy[J]. Acta Mater., 2023, 245: 118618
|
| 8 |
Tseng K K, Juan C C, Tso S, et al. Effects of Mo, Nb, Ta, Ti, and Zr on mechanical properties of equiatomic Hf-Mo-Nb-Ta-Ti-Zr alloys[J]. Entropy, 2018, 21: 15
|
| 9 |
Xu L J, Zong L, Luo C Y, et al. Toughening pathways and regulatory mechanisms of refractory high-entropy alloys[J]. Acta Metall. Sin., 2022, 58: 257
doi: 10.11900/0412.1961.2021.00286
|
|
徐流杰, 宗 乐, 罗春阳 等. 难熔高熵合金的强韧化途径与调控机理[J]. 金属学报, 2022, 58: 257
doi: 10.11900/0412.1961.2021.00286
|
| 10 |
Li T X, Wang S D, Fan W X, et al. CALPHAD-aided design for superior thermal stability and mechanical behavior in a TiZrHfNb refractory high-entropy alloy[J]. Acta Mater., 2023, 246: 118728
|
| 11 |
Zhang E K, Tang Y, Wen M W, et al. On phase stability of Mo-Nb-Ta-W refractory high entropy alloys[J]. Int. J. Refract. Met. Hard Meter., 2022, 103: 105780
|
| 12 |
El Atwani O, Vo H T, Tunes M A, et al. A quinary WTaCrVHf nanocrystalline refractory high-entropy alloy withholding extreme irradiation environments[J]. Nat. Commun., 2023, 14: 2516
doi: 10.1038/s41467-023-38000-y
pmid: 37130885
|
| 13 |
Cheng T, Wei G, Jiang S M, et al. Enhanced resistance to helium irradiations through unusual interaction between high-entropy-alloy and helium[J]. Acta Mater., 2023, 248: 118765
|
| 14 |
Ouyang D, Chen Z J, Yu H B, et al. Oxidation behavior of the Ti38V15Nb23Hf24 refractory high-entropy alloy at elevated temperatures[J]. Corros. Sci., 2022, 198: 110153
|
| 15 |
Wei S L, Kim S J, Kang J Y, et al. Natural-mixing guided design of refractory high-entropy alloys with as-cast tensile ductility[J]. Nat. Mater., 2020, 19: 1175
|
| 16 |
Gou S Y, Gao M Y, Shi Y Z, et al. Additive manufacturing of ductile refractory high-entropy alloys via phase engineering[J]. Acta Mater., 2023, 248: 118781
|
| 17 |
Liu Y N, Ding Y, Yang L J, et al. Research and progress of laser cladding on engineering alloys: A review[J]. J. Manuf. Process., 2021, 66: 341
|
| 18 |
Zhang J C, Shi S H, Gong Y Q, et al. Research progress of laser cladding technology[J]. Surf. Technol., 2020, 49(10): 1
|
|
张津超, 石世宏, 龚燕琪 等. 激光熔覆技术研究进展[J]. 表面技术, 2020, 49(10): 1
|
| 19 |
Zhu L D, Xue P S, Lan Q, et al. Recent research and development status of laser cladding: A review[J]. Opt. Laser Technol., 2021, 138: 106915
|
| 20 |
Kumar D. Recent advances in tribology of high entropy alloys: A critical review[J]. Prog. Mater. Sci., 2023, 136: 101106
|
| 21 |
Zhang Y, Zhou Y J, Lin J P, et al. Solid-solution phase formation rules for multi-component alloys[J]. Adv. Eng. Mater., 2008, 10: 534
|
| 22 |
Yang X, Zhang Y. Prediction of high-entropy stabilized solid-solution in multi-component alloys[J]. Mater. Chem. Phys., 2012, 132: 233
|
| 23 |
Snyder J C, Rupp M, Hansen K, et al. Finding density functionals with machine learning[J]. Phys. Rev. Lett., 2012, 108: 253002
|
| 24 |
Mu Y K. Design and fabrication of refractory multicomponent high entropy alloys coating with laser cladding[D]. Kunming: Kunming University of Science and Technology, 2017
|
|
穆永坤. 激光熔覆难熔多组元高熵合金涂层设计与制备[D]. 昆明: 昆明理工大学, 2017
|
| 25 |
Wen C. Composition design and property optimization of high entropy alloys based on machine learning[D]. Beijing: University of Science and Technology Beijing, 2021
|
|
文 成. 基于机器学习的高熵合金成分设计与性能优化[D]. 北京: 北京科技大学, 2021
|
| 26 |
Senkov O N, Miller J D, Miracle D B, et al. Accelerated exploration of multi-principal element alloys with solid solution phases[J]. Nat. Commun., 2015, 6: 6529
doi: 10.1038/ncomms7529
pmid: 25739749
|
| 27 |
Wei M W, Chen S Y, Sun M, et al. Atomization simulation and preparation of 24CrNiMoY alloy steel powder using VIGA technology at high gas pressure[J]. Powder Technol., 2020, 367: 724
|
| 28 |
Xia M, Chen Y X, Wang R, et al. Fabrication of spherical MoNbTaWZr refractory high-entropy powders by spray granulation combined with plasma spheroidization[J]. J. Alloys Compd., 2023, 931: 167542
|
| 29 |
Zhang H, Cai J L, Geng J L, et al. Development of high strength high plasticity refractory high entropy alloy based on Mo element optimization and advanced forming process[J]. Int. J. Refract. Met. Hard Mater., 2023, 112: 106163
|
| 30 |
Shen Z L, Su H J, Liu Y, et al. Laser additive manufacturing of melt-grown Al2O3/GdAlO3 eutectic ceramic composite: Powder designs and crack analysis with thermo-mechanical simulation[J]. J. Eur. Ceram. Soc., 2022, 42: 6583
|
| 31 |
Sun B, Wang Q Q, Chen Y X, et al. Design of heterogeneous structure for enhancing formation quality of laser-manufactured WTaMoNb refractory high-entropy alloy[J]. J. Alloys Compd., 2023, 953: 170066
|
| 32 |
Arrizubieta J I, Martínez S, Lamikiz A, et al. Instantaneous powder flux regulation system for laser metal deposition[J]. J. Manuf. Process., 2017, 29: 242
|
| 33 |
Dobbelstein H, Gurevich E L, George E P, et al. Laser metal deposition of compositionally graded TiZrNbTa refractory high-entropy alloys using elemental powder blends[J]. Addit. Manuf., 2019, 25: 252
doi: 10.1016/j.addma.2018.10.042
|
| 34 |
Melia M A, Whetten S R, Puckett R, et al. High-throughput additive manufacturing and characterization of refractory high entropy alloys[J]. Appl. Mater. Today, 2020, 19: 100560
|
| 35 |
Zhao Y, Wu M F, Jiang P C, et al. Microstructure of WTaNbMo refractory high entropy alloy coating fabricated by dynamic magnetic field assisted laser cladding process[J]. J. Mater. Res. Technol., 2022, 20: 1908
|
| 36 |
Zhao Y, Wu M F, Hou J, et al. Microstructure and high temperature properties of laser cladded WTaNbMo refractory high entropy alloy coating assisted with ultrasound vibration[J]. J. Alloys Compd., 2022, 920: 165888
|
| 37 |
Zhao S, Taheri M, Shirvani K, et al. Microstructure of NbMoTaTiNi refractory high-entropy alloy coating fabricated by ultrasonic field-assisted laser cladding process[J]. Coatings, 2023, 13: 995
|
| 38 |
Gao Q, Liu H, Chen P J, et al. Multi-objective optimization for laser cladding refractory MoNbTiZr high-entropy alloy coating on Ti6Al4V[J]. Opt. Laser Technol., 2023, 161: 109220
|
| 39 |
Goel S, Neikter M, Capek J, et al. Residual stress determination by neutron diffraction in powder bed fusion-built Alloy 718: Influence of process parameters and post-treatment[J]. Mater. Des., 2020, 195: 109045
|
| 40 |
Marola S, Bosia S, Veltro A, et al. Residual stresses in additively manufactured AlSi10Mg: Raman spectroscopy and X-ray diffraction analysis[J]. Mater. Des., 2021, 202: 109550
|
| 41 |
Guo Y X, Wang H L, Liu Q B. Microstructure evolution and strengthening mechanism of laser-cladding MoFe x CrTiWAlNb y refractory high-entropy alloy coatings[J]. J. Alloys Compd., 2020, 834: 155147
|
| 42 |
Liu S S, Zhao G L, Wang X H, et al. Design and characterization of AlNbMoTaCu x high entropy alloys laser cladding coatings[J]. Surf. Coat. Technol., 2022, 447: 128832
|
| 43 |
Miracle D B, Senkov O N. A critical review of high entropy alloys and related concepts[J]. Acta Mater., 2017, 122: 448
|
| 44 |
Wu J X, Li P Y, Dong H F, et al. Research progress in composition design, microstructure and properties of refractory high entropy alloys[J]. J. Aeronaut. Mater., 2022, 42(6): 33
|
|
武俊霞, 李培友, 董洪峰 等. 难熔高熵合金成分设计微观组织及性能研究进展[J]. 航空材料学报, 2022, 42(6): 33
doi: 10.11868/j.issn.1005-5053.2021.000205
|
| 45 |
Chen G, Luo T, Shen S C, et al. Research progress in refractory high-entropy alloys[J]. Mater. Rep., 2021, 35: 17064
|
|
陈 刚, 罗 涛, 沈书成 等. 难熔高熵合金的研究进展[J]. 材料导报, 2021, 35: 17064
|
| 46 |
Zhang M N, Zhou X L, Yu X N, et al. Synthesis and characterization of refractory TiZrNbWMo high-entropy alloy coating by laser cladding[J]. Surf. Coat. Technol., 2017, 311: 321
|
| 47 |
Guo Y X, Liu Q B. MoFeCrTiWAlNb refractory high-entropy alloy coating fabricated by rectangular-spot laser cladding[J]. Intermetallics, 2018, 102: 78
|
| 48 |
Wang H L, Liu Q B, Guo Y X, et al. MoFe1.5CrTiWAlNb x refractory high-entropy alloy coating fabricated by laser cladding[J]. Intermetallics, 2019, 115: 106613
|
| 49 |
Guo Y X, Li X M, Liu Q B. A novel biomedical high-entropy alloy and its laser-clad coating designed by a cluster-plus-glue-atom model[J]. Mater. Des., 2020, 196: 109085
|
| 50 |
Guan H T, Chai L J, Wang Y Y, et al. Microstructure and hardness of NbTiZr and NbTaTiZr refractory medium-entropy alloy coatings on Zr alloy by laser cladding[J]. Appl. Surf. Sci., 2021, 549: 149338
|
| 51 |
Kuang S H, Zhou F, Zheng S S, et al. Annealing-induced microstructure and properties evolution of refractory MoFeCrTiWAlNb3 eutectic high-entropy alloy coating by laser cladding[J]. Intermetallics, 2021, 129: 107039
|
| 52 |
Zhang X R, Cui X F, Jin G, et al. Microstructure evolution and properties of NiTiCrNbTa x refractory high-entropy alloy coatings with variable Ta content[J]. J. Alloys Compd., 2022, 891: 161756
|
| 53 |
Zhao P, Li J, Zhang Y, et al. Wear and high-temperature oxidation resistances of AlNbTaZr x high-entropy alloys coatings fabricated on Ti6Al4V by laser cladding[J]. J. Alloys Compd., 2021, 862: 158405
|
| 54 |
Chen L, Wang Y Y, Hao X H, et al. Lightweight refractory high entropy alloy coating by laser cladding on Ti-6Al-4V surface[J]. Vacuum, 2021, 183: 109823
|
| 55 |
Lou L Y, Liu K C, Jia Y J, et al. Microstructure and properties of lightweight Al0.2CrNbTiV refractory high entropy alloy coating with different dilutions deposited by high speed laser cladding[J]. Surf. Coat. Technol., 2022, 447: 128873
|
| 56 |
Liao T H, Wang Z L, Wu X H, et al. Effect of V on microstructure, wear and corrosion properties in AlCoCrMoV x high entropy alloy coatings by laser cladding[J]. J. Mater. Res. Technol., 2023, 23: 4420
|
| 57 |
Huang Y M, Wang Z Y, Xu Z Z, et al. Microstructure and properties of TiNbZrMo high entropy alloy coating[J]. Mater. Lett., 2021, 285: 129004
|
| 58 |
Ren Z Y, Hu Y L, Tong Y G, et al. Wear-resistant NbMoTaWTi high entropy alloy coating prepared by laser cladding on TC4 titanium alloy[J]. Tribol. Int., 2023, 182: 108366
|
| 59 |
Hao X H, Liu H X, Zhang X W, et al. Microstructure and wear resistance of in-situ TiN/(Nb, Ti)5Si3 reinforced MoNbTaWTi-based refractory high entropy alloy composite coatings by laser cladding[J]. Appl. Surf. Sci., 2023, 626: 157240
|
| 60 |
Zhou J L, Cheng Y H, Wan Y X, et al. Solidification characteristics and microstructure of TaNbZrTi refractory high entropy coating by extreme high-speed laser cladding[J]. Int. J. Refract. Met. Hard Mater., 2023, 115: 106257
|
| 61 |
Wang Y, Li P J, Ma N, et al. Effect of Y2O3 on the microstructure and tribology property of WMoTaNb refractory high entropy alloy coating prepared by laser cladding[J]. Int. J. Refract. Met. Hard Mater., 2023, 115: 106273
|
| 62 |
Jiang X J, Wang S Z, Fu H, et al. A novel high-entropy alloy coating on Ti-6Al-4V substrate by laser cladding[J]. Mater. Lett., 2022, 308: 131131
|
| 63 |
Zhang X R, Cui X F, Jin G, et al. Microstructure evolution and performance enhancement of NbTaTiV-(Cr, Zr, W) single-phase refractory high-entropy alloy coatings: Role of additional elements[J]. J. Alloys Compd., 2023, 951: 169918
|
| 64 |
Li Q T, Lei Y P, Fu H G, et al. Microstructure and mechanical properties of in situ (Ti, Nb)Cp/Fe-based laser composite coating prepared with different heat inputs[J]. Rare Met., 2018, 37: 852
|
| 65 |
Cheng W, Ji L F, Zhang L T, et al. Refractory high-entropy alloys fabricated using laser technologies: A concrete review[J]. J. Mater. Res. Technol., 2023, 24: 7497
|
| 66 |
Ren J, Zhang Y, Zhao D X, et al. Strong yet ductile nanolamellar high-entropy alloys by additive manufacturing[J]. Nature, 2022, 608: 62
|
| 67 |
Leijon F, Wachter S, Fu Z W, et al. A novel rapid alloy development method towards powder bed additive manufacturing, demonstrated for binary Al-Ti, -Zr and -Nb alloys[J]. Mater. Des., 2021, 211: 110129
|
| 68 |
Li Q Y, Zhang H, Li D C, et al. Comparative study of the microstructures and mechanical properties of laser metal deposited and vacuum arc melted refractory NbMoTa medium-entropy alloy[J]. Int. J. Refract. Met. Hard Mater., 2020, 88: 105195
|
| 69 |
Yan X H, Zhang Y. A body-centered cubic Zr50Ti35Nb15 medium-entropy alloy with unique properties[J]. Scr. Mater., 2020, 178: 329
|
| 70 |
Liu L, Liu H X, Zhang X W, et al. Corrosion behavior of TiMoNbX (X = Ta, Cr, Zr) refractory high entropy alloy coating prepared by laser cladding based on TC4 titanium alloy[J]. Materials, 2023, 16: 3860
|
| 71 |
Huang H L, Wu Y, He J Y, et al. Phase-transformation ductilization of brittle high-entropy alloys via metastability engineering[J]. Adv. Mater., 2017, 29: 1701678
|
| 72 |
Wang R X, Tang Y, Li S, et al. Novel metastable engineering in single-phase high-entropy alloy[J]. Mater. Des., 2019, 162: 256
|
| 73 |
Massalski T B, Okamoto H. Binary Alloy Phase Diagrams[M]. 2nd Ed., Materials Park: ASM International, 1990: 2249
|
| 74 |
Stein F, Palm M, Sauthoff G. Structure and stability of Laves phases. Part I. Critical assessment of factors controlling Laves phase stability[J]. Intermetallics, 2004, 12: 713
|
| 75 |
Kawamoto M, Okabayashi K. Study of dry sliding wear of cast iron as a function of surface temperature[J]. Wear, 1980, 58: 59
|
| 76 |
Alvi S, Jarzabek D M, Kohan M G, et al. Synthesis and mechanical characterization of a CuMoTaWV high-entropy film by magnetron sputtering[J]. ACS Appl. Mater. Interfaces, 2020, 12: 21070
|
| 77 |
Rahimi H, Mozaffarinia R, Hojjati Najafabadi A. Corrosion and wear resistance characterization of environmentally friendly sol-gel hybrid nanocomposite coating on AA5083[J]. J. Mater. Sci. Technol., 2013, 29: 603
doi: 10.1016/j.jmst.2013.03.013
|
| 78 |
Xu Z M, Sun Z P, Li C, et al. Effect of Cr on microstructure and properties of WVTaTiCr x refractory high-entropy alloy laser cladding[J]. Materials, 2023, 16: 3060
|
| 79 |
Wu H, Zhang S, Wang Z Y, et al. New studies on wear and corrosion behavior of laser cladding FeNiCoCrMo x high entropy alloy coating: The role of Mo[J]. Int. J. Refract. Met. Hard Mater., 2022, 102: 105721
|
| 80 |
Müller F, Gorr B, Christ H J, et al. On the oxidation mechanism of refractory high entropy alloys[J]. Corros. Sci., 2019, 159: 108161
|
| 81 |
Liu C Y, Ma Z L, Li H Y, et al. Designing NbTiTa-Cr/Al refractory complex concentrated alloys with balanced strength-ductility-oxidation resistance properties: Insights into oxidation mechanisms[J]. Int. J. Refract. Met. Hard Mater., 2023, 115: 106308
|
| 82 |
Li T X, Lu Y P, Cao Z Q, et al. Opportunity and challenge of refractory high-entropy alloys in the field of reactor structural materials[J]. Acta Metall. Sin., 2021, 57: 42
doi: 10.11900/0412.1961.2020.00293
|
|
李天昕, 卢一平, 曹志强 等. 难熔高熵合金在反应堆结构材料领域的机遇与挑战[J]. 金属学报, 2021, 57: 42
doi: 10.11900/0412.1961.2020.00293
|
| 83 |
Xu C H, Gao W. Pilling-Bedworth ratio for oxidation of alloys[J]. Mater. Res. Innov., 2000, 3: 231
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|