| Positron Annihilation Investigation of Embrittlement Behavior in Chinese RPV Steels after Fe-Ion Irradiation |
Tianci ZHANG1,2, Haitao WANG1, Zhengcao LI2( ), Henk SCHUT3, Zhengming ZHANG1, Ming HE4, Yuliang SUN1 |
1 Collaborative Innovation Center of Advanced Nuclear Energy Technology, Key Laboratory of Advanced Reactor Engineering and Safety of Ministry of Education, Institute of Nuclear and New Energy Technology, Tsinghua University, Beijing 100084, China 2 Key Laboratory of Advanced Materials (MOE), School of Materials Science and Engineering, Tsinghua University, Beijing 100084, China 3 Department of Radiation Science and Technology, Delft University of Technology, Mekelweg 15, 2629 JB Delft, Netherlands 4 Shanghai Electric Nuclear Power Equipment Co., Ltd., Shanghai 201306, China |
|
Cite this article:
Tianci ZHANG, Haitao WANG, Zhengcao LI, Henk SCHUT, Zhengming ZHANG, Ming HE, Yuliang SUN. Positron Annihilation Investigation of Embrittlement Behavior in Chinese RPV Steels after Fe-Ion Irradiation. Acta Metall Sin, 2018, 54(4): 512-518.
|
|
|
Abstract The reactor pressure vessel (RPV) is the key component in the nuclear power plant, which is considered irreplaceable and can be the life-limiting feature of the operation of nuclear power plant if its mechanical properties degrade sufficiently. High temperature gas-cooled reactor (HTGR) has perfect inherent safety, which is intended to be one of the fourth generation advanced nuclear reactors. However, HTGR has different service temperature with pressurized water reactor (PWR), that the service temperature of HTGR is 250 ℃ and that of PWR is 290 ℃. So the irradiation behaviour of RPV in HTGR is expected to be investigated. In this wok, 3 MeV Fe-ion irradiation was performed on Chinese A508-3 reactor pressure vessel steel which is employed by high-temperature gas-cooled reactors and pure Fe under room temperature (about 25 ℃) and high temperature (250 ℃). The ion doses were 0.1, 0.5 and 1.0 dpa for both room temperature irradiation and high temperature irradiation. SRIM modeling was performed before irradiation experiments to guide the experimental details. Positron annihilation Doppler broadening (PADB) spectroscopy experiments and nano-indentation tests (to study embrittlement behavior) were conducted for characterization. It is found that after both room temperature irradiation and high temperature irradiation, the densities of defects in the reactor pressure vessel steel and pure Fe increase, and the type of defects could be vacancy-type and solute cluster type from PADB results. The vacancy-type defect density under high temperature irradiation is lower than that under room temperature irradiation. That is because high temperature can recover the defects formed during irradiation. The hardness test results show that for both the reactor pressure vessel steel and pure Fe, the irradiation hardening increases with increasing dose. Compared to room temperature irradiation, high temperature irradiation can produce more solute clusters and fewer vacancy-type defects in the reactor pressure vessel steel. So the irradiation hardening of the reactor pressure vessel steel might be caused mainly by the formation of solute clusters.
|
|
Received: 10 November 2017
|
|
|
| Fund: Supported by National Key Research and Development Program of China (No.2017YFB0702200) |
| [1] | Zhang Z Y, Dong Y J, Li F, et al.The Shandong Shidao Bay 200 MWe high-temperature gas-cooled reactor pebble-bed module (HTR-PM) demonstration power plant: An engineering and technological innovation[J]. Engineering, 2016, 2: 112 | | [2] | Lee B S, Hong J H, Yang W J, et al.Master curve characterization of the fracture toughness in unirradiated and irradiated RPV steels using full-and 1/3-size pre-cracked Charpy specimens[J]. Int. J. Pressure Vessels Piping, 2000, 77: 599 | | [3] | Gurovich B, Kuleshova E, Shtrombakh Y, et al.Evolution of microstructure and mechanical properties of VVER-1000 RPV steels under re-irradiation[J]. J. Nucl. Mater., 2015, 456: 373 | | [4] | Xu G, Cai L L, Feng L, et al.Effect of the precipitation of Cu-rich clusters on the DBTT of RPV simulated steel[J]. Acta Metall. Sin., 2012, 48: 753(徐刚, 蔡琳玲, 冯柳 等. 富Cu团簇的析出对RPV模拟钢韧-脆转变温度的影响 [J]. 金属学报, 2012, 48: 753) | | [5] | Li Z C, Chen L.Irradiation embrittlement mechanisms and relevant influence factors of nuclear reactor pressure vessel steels[J]. Acta Metall. Sin., 2014, 50: 1285(李正操, 陈良. 核能系统压力容器辐照脆化机制及其影响因素 [J]. 金属学报, 2014, 50: 1285) | | [6] | Odette G R, Lucas G E.Recent progress in understanding reactor pressure vessel steel embrittlement[J]. Radiat. Eff. Defects Solids, 1998, 144: 189 | | [7] | Chaouadi R, Gérard R.Copper precipitate hardening of irradiated RPV materials and implications on the superposition law and re-irradiation kinetics[J]. J. Nucl. Mater., 2005, 345: 65 | | [8] | Yeli G, Li Z C, Yu X Y, et al.Mechanical and magnetic properties of copper dispersed ferrum films under heat treatment[J]. Rare Met., 2014, 33: 641 | | [9] | Styman P D, Hyde J M, Wilford K, et al.Characterisation of interfacial segregation to Cu-enriched precipitates in two thermally aged reactor pressure vessel steel welds[J]. Ultramicroscopy, 2015, 159: 292 | | [10] | Carter R G, Soneda N, Dohi K, et al.Microstructural characterization of irradiation-induced Cu-enriched clusters in reactor pressure vessel steels[J]. J. Nucl. Mater., 2001, 298: 211 | | [11] | Zelenty J E.Understanding thermally induced embrittlement in low copper RPV steels utilising atom probe tomography[J]. Mater. Sci. Technol., 2015, 31: 981 | | [12] | Odette G R, Nanstad R K.Predictive reactor pressure vessel steel irradiation embrittlement models: Issues and opportunities[J]. JOM, 2009, 61(7): 17 | | [13] | Ortner S.Anomalous hardening in RPV surveillance and MTR data [R]. London, UK: NNL, 2010 | | [14] | Xu G, Chu D F, Cai L L, et al.Investigation on the precipitation and structural evolution of Cu-rich nanophase in RPV model steel[J]. Acta Metall. Sin., 2011, 47: 905(徐刚, 楚大锋, 蔡琳玲 等. RPV模拟钢中纳米富Cu相的析出和结构演化研究 [J]. 金属学报, 2011, 47: 905 | | [15] | Watanabe H, Arase S, Yamamoto T, et al.Hardening and microstructural evolution of A533b steels irradiated with Fe ions and electrons[J]. J. Nucl. Mater., 2016, 471: 243 | | [16] | Bergner F, Gillemot F, Hernández-Mayoral M, et al.Contributions of Cu-rich clusters, dislocation loops and nanovoids to the irradiation-induced hardening of Cu-bearing low-Ni reactor pressure vessel steels[J]. J. Nucl. Mater., 2015, 461: 37 | | [17] | Slugeň V, Kryukov A.Microstructural study of WWER reactor pressure vessel steels[J]. Nucl. Eng. Des., 2013, 263: 308 | | [18] | Ko???k J, Keilova E, ????ek J, et al. TEM and PAS study of neutron irradiated VVER-type RPV steels[J]. J. Nucl. Mater., 2002, 303: 52 | | [19] | Nagai Y, Takadate K, Tang Z, et al.Positron annihilation study of vacancy-solute complex evolution in Fe-based alloys[J]. Phys. Rev., 2003, 67B: 224202 | | [20] | Meslin E, Lambrecht M, Hernández-Mayoral M, et al.Characterization of neutron-irradiated ferritic model alloys and a RPV steel from combined APT, SANS, TEM and PAS analyses[J]. J. Nucl. Mater., 2010, 406: 73 | | [21] | Toyama T, Nagai Y, Tang Z, et al.Nanostructural evolution in surveillance test specimens of a commercial nuclear reactor pressure vessel studied by three-dimensional atom probe and positron annihilation[J]. Acta Mater., 2007, 55: 6852 | | [22] | Nikolaeva A V, Nikolaev Y A, Kryukov A M.The contribution of grain boundary effects to low-alloy steel irradiation embrittlement[J]. J. Nucl. Mater., 1995, 218: 85 | | [23] | Lü Z, Faulkner R G, Flewitt P E J. Neutron irradiation-induced phosphorus segregation in reactor pressure vessel steels[J]. Acta Metall. Sin., 2005, 41: 79(吕铮, Faulkner R G, Flewitt P E J. 中子辐照诱导压力容器钢中磷的偏析 [J]. 金属学报, 2005, 41: 79) | | [24] | Chen L, Li Z C, Schut H, et al.Positron annihilation study of Fe-ion irradiated reactor pressure vessel model alloys[J]. J. Phys. Conf. Ser., 2016, 674: 012012 | | [25] | Jiang J, Wu Y C, Liu X B, et al.Microstructural evolution of RPV steels under proton and ion irradiation studied by positron annihilation spectroscopy[J]. J. Nucl. Mater., 2015, 458: 326 | | [26] | Chen D Y, Murakami K, Dohi K, et al.Depth distribution of Frank loop defects formed in ion-irradiated stainless steel and its dependence on Si addition[J]. Nucl. Instrum. Methods Phys. Res., 2015, 365B: 503 | | [27] | Schut H, van Gog H, van Veen A, et al. A positron beam study of hydrogen confined in nano-cavities in crystalline silicon[J]. Nucl. Instrum. Methods Phys. Res., 2004, 216B: 251 | | [28] | Eleveld H, van Veen A. Void growth and thermal desorption of deuterium from voids in tungsten [J]. J. Nucl. Mater., 1994, 212-215: 1421 | | [29] | Vehanen A, Saarinen K, Hautoj?rvi P, et al.Profiling multilayer structures with monoenergetic positrons[J]. Phys. Rev, 1987, 35B: 4606 | | [30] | Slugeň V.Defects investigation in neutron irradiated reactor steels by positron annihilation[J]. Nucl. Eng. Des., 2005, 235: 1961 | | [31] | Liu X B, Wang R S, Jiang J, et al.Slow positron beam and nanoindentation study of irradiation-related defects in reactor vessel steels[J]. J. Nucl. Mater., 2014, 451: 249 | | [32] | Jin S X, Zhang P, Lu E Y, et al.Correlation between Cu precipitates and irradiation defects in Fe-Cu model alloys investigated by positron annihilation spectroscopy[J]. Acta Mater., 2016, 103: 658 |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|