Abstract With the development of hydrogen economy, the demand of structural materials with high strength suitable for service in hydrogen or hydrogen-bearing environments such as storage of hydrogen gas was incremental. An optional structural materials is J75 alloy, which is mainly strengthened by an ordered fcc γ' phase, Ni3(Al, Ti), coherent with the austenite matrix. Investigation on J75 alloy indicated that the commercial alloy free of B would lose about half its ductility when charged with hydrogen, accompanied by a change of fracture mode from ductile rupture to brittle-appearing intergranular fracture. Otherwise, an improvement in ductility and hydrogen resistant performance was observed in the J75 alloy with trace B, however, its role in the alloy is unclear. So, in present work, mechanism of B in the J75 hydrogen-resistant alloy was investigated by means of OM, SEM, TEM, EPMA, 3DAP, SIMS, hydrogen penetration, thermal hydrogen charging experiments and tensile tests. It was found that a lot of Ti segregated at grain boundaries (GBs) in the alloy free of B, resulted in abundant precipitation of cellular η phases. However, the cellular η phase was not observed in the alloy with B, and it could be attributed to the segregation of B atoms at GBs and inhibited the segregation of Ti. A lower hydrogen diffusion coefficient was observed in the alloy with B than that in the alloy free of B by hydrogen permeation, indicating that diffusion velocity of H atoms in the alloy had been decreased by the addition of B. Moreover, segregation of B at GBs could not only inhibit the precipitation of η phases but also decrease the number of H atoms there, which would improve the hydrogen-resistant performance of the alloy.
|
|
|
| Fund: Supported by National Natural Science Foundation of China and China Academy of Engineering Physics (No.U1230118) and National Natural Science Foundation of China (No.51171178) |
| [1] | Li X Y,Li Y Y. Hydrogen Damage of Austenitic Alloy. Beijing: Science Press, 2003: 1 | | [1] | (李秀艳,李依依. 奥氏体合金的氢损伤. 北京: 科学出版社, 2003: 1) | | [2] | Zhang J, Li X Y, Zhao M J, Rong L J. Acta Metall Sin, 2008; 44: 1095 | | [2] | (张 建, 李秀艳, 赵明久, 戎利建. 金属学报, 2008; 44: 1095) | | [3] | Li X Y, Rong L J, Li Y Y. Acta Metall Sin, 2005; 41: 1155 | | [3] | (李秀艳, 戎利建, 李依依. 金属学报, 2005; 41: 1155) | | [4] | Li X Y, Zhang J, Rong L J, Li Y Y. Mater Sci Eng, 2008; A488: 547 | | [5] | Zhang J, Li X Y, Rong L J, Zheng Y N, Zhu S Y. Acta Metall Sin, 2006; 42: 469 | | [5] | (张 建, 李秀艳, 戎利建, 郑永男, 朱升云. 金属学报, 2006; 42: 469) | | [6] | Chen S H, Zhao M J, Rong L J. Acta Metall Sin, 2012; 48: 1335 | | [6] | (陈胜虎, 赵明久, 戎利建. 金属学报, 2012; 48: 1335) | | [7] | Brooks J A, Thompson A W. Metall Trans, 1993; 24A: 1983 | | [8] | Zhao M J, Rong L J. Acta Metall Sin, 2009; 45: 119 | | [8] | (赵明久, 戎利建. 金属学报, 2009; 45: 119) | | [9] | Zhao M J, Guo Z F, Liang H, Rong L J. Mater Sci Eng, 2010; A527: 5844 | | [10] | Yao X X. Mater Sci Eng, 1999; A271: 353 | | [11] | Sourmail T, Okuda T, Taylor J E. Scr Mater, 2004; 50: 1271 | | [12] | Fujwara M, Uchida H, Ohta S. J Mater Sci Lett, 1994; 13: 557 | | [13] | Kennedy R L, Cao W D, Thomas W M. Adv Mater Process, 1996; 149: 33 | | [14] | Sellamuthu R, Giamei A F. Metall Trans, 1986; 17A: 419 | | [15] | Wills V A, Mccartney D G. Mater Sci Eng, 1991; A145: 223 | | [16] | Franzoni U, Marchetti F, Sturless S. Scr Metall, 1985; 19: 511 | | [17] | Shulga A V. J Alloys Compd, 2007; 486: 155 | | [18] | Liu W Q, Liu Q D, Li C, Fang S F, Zhou B X. J Jiangsu Univ (Nat Sci Ed), 2008; 29: 131 | | [18] | (刘文庆, 刘庆冬, 李 聪, 方淑芳, 周邦新. 江苏大学学报(自然科学版), 2008; 29: 131) | | [19] | Guo J T. Material Science and Engineering for Superalloys. Beijing: Science Press, 2008: 123 | | [19] | (郭建亭. 高温合金材料学. 北京: 科学出版社, 2008: 123) | | [20] | Ducki K J, Hetmanczyk M, Kuc D. Mater Chem Phys, 2003; 81: 490 | | [21] | Cicco H D, Luppo M I, Gribaudo L M, Garcia J O. Mater Charact, 2004; 52: 85 | | [22] | Zhao J C, Ravikumar V. Metall Mater Trans, 2001; 32A: 1271 | | [23] | Zhao S Q, Xie X S, Smith G D, Patel S J. Mater Sci Eng, 2003; A355: 96 | | [24] | Wu P, He X L. Acta Metall Sin, 1999; 35: 1009 | | [24] | (吴 平, 贺信莱. 金属学报, 1999; 35: 1009) | | [25] | Aust K, Hanneman R, Niessen P, Westbrook J. Acta Metall, 1968; 16: 291 | | [26] | Li X Y, Zhang J, Rong L J, Li Y Y. J Mater Sci Eng, 2005; 23: 483 | | [26] | (李秀艳, 张 建, 戎利建, 李依依. 材料科学与工程学报, 2005; 23: 483) | | [27] | Wu Y X, Li X Y, Wang Y M. Acta Mater, 2007; 55: 4845 | | [28] | Wan X J, Chen Y X, Cheng X Y. Prog Nat Sci, 2001; 11: 458 | | [28] | (万晓景, 陈业新, 程晓英. 自然科学进展, 2001; 11: 458) |
|