| EFFECT OF DEFORMATION AND THERMOMECHA- NICAL PROCESSING ON GRAIN BOUNDARY CHARACTER DISTRIBUTION OF ALLOY 825 TUBES |
Qing ZHAO1,Shuang XIA1( ),Bangxin ZHOU1,Qin BAI1,Cheng SU2,Baoshun WANG2,Zhigang CAI2 |
1 School of Materials Science and Engineering, Shanghai University, Shanghai 200072 2 Zhejiang Jiuli Hi-Tech Metals Co. Ltd., Huzhou 313008 |
|
Cite this article:
Qing ZHAO,Shuang XIA,Bangxin ZHOU,Qin BAI,Cheng SU,Baoshun WANG,Zhigang CAI. EFFECT OF DEFORMATION AND THERMOMECHA- NICAL PROCESSING ON GRAIN BOUNDARY CHARACTER DISTRIBUTION OF ALLOY 825 TUBES. Acta Metall Sin, 2015, 51(12): 1465-1471.
|
|
|
Abstract Alloy 825 is widely used for chemical and petrochemical applications due to its good combination of mechanical properties and corrosion resistance. However, intergranular corrosion (IGC) is one of the serious problems for alloy 825 exposed to aggressive environments, which could result in unexpected failures and lead to huge losses. The grain boundary structure, which can partly be described by coincidence site lattice (CSL) model, can influence the grain boundary chemistry and the susceptibility to intergranular corrosion. The field of grain boundary engineering (GBE) has developed a lot over the last two decades since the concept of grain boundary design was proposed. The aim of GBE is to enhance the grain-boundary-related properties of materials by increasing the frequency of low ΣCSL (Σ≤29) grain boundaries (GBs) and tailoring the grain boundary network. It was reported that in some fcc materials with low stacking fault energy, such as Ni-based alloys, lead alloys, austenitic stainless steels and copper alloys, the frequency of low ΣCSL GBs can be greatly increased by using proper thermomechanical processing (TMP), and as a result the grain boundary related properties were greatly enhanced. In this work, GBE is applied to the manufacture of Ni-based alloy 825 tubes by cold drawing using a draw-bench on a factory production line and the subsequent annealing. The effect of thermomechanical processing on the grain boundary character distribution (GBCD) of alloy 825 was studied by means of the EBSD technique and orientation image microcopy (OIM). The results show that the proportion of low ΣCSL grain boundaries increase to more than 75% by the TMP after 5% cold drawing and subsequent annealing at 1050 ℃ for 10 min, and simultaneously the large-size highly-twinned grain-cluster microstructure is formed. The size of the grain-cluster and proportion of low ΣCSL grain boundaries decrease with the increase of pre-strain. The proportion of low ΣCSL grain boundaries decreases with the increase of the mean grain size. The annealing temperatures in the range of 1050~1125 ℃ have no obvious effect on the GBCD of the specimen with 5% cold drawing deformation; while the proportions of low ΣCSL GBs of the sample with 3%, 7% and 10% cold drawing deformation decrease with the increase of annealing temperature.
|
|
|
| Fund: Supported by National Basic Research Program of China (No.2011CB610502) and Shanghai Science and Technology Commission Key Support Project (No.13520500500) |
| [1] | Yang J F, Fan F X, Li M, Bai Y. Develop Appl Mater, 2009; 24(4): 26 | | [1] | (杨俊峰, 范芳雄, 李 墨, 白 杨. 材料开发与应用, 2009; 24(4): 26) | | [2] | Feng Y, He D L, Gong D S, Li F, Wu J X. J Chin Soc Corros Prot, 2013; 33 :164 | | [2] | (冯 勇, 何德良, 龚德胜, 李 菲, 吴建新. 中国腐蚀与防护学报, 2013; 33: 164) | | [3] | Shimada M, Kokawa H, Wang Z J, Sato Y S, Karibe I. Acta Mater, 2002; 50: 2331 | | [4] | Palumbo G, Erb U. MRS Bull, 1999; 24: 27 | | [5] | Watanabe T, Tsurekawa S. Acta Mater, 1999; 47: 4171 | | [6] | Kokawa H, Watanabe T, Karashima S. Philos Mag, 1981; 44A: 1239 | | [7] | Hong Y B, Kokawa H, Zhan J W. Scr Mater, 2003; 49: 219 | | [8] | Watanabe T. Res Mech, 1984; 11(1): 47 | | [9] | Palumbo G, Lehockey E M, Lin P. JOM, 1998; 50(2): 40 | | [10] | Cheung C, Erb U, Palumbo G. Mater Sci Eng, 1994; A185: 39 | | [11] | Lehockey E M, Palumbo G, Lin P. Metall Mater Trans, 1998; 29A: 3069 | | [12] | Palumbo G. US Pat, 5702543, 1997 | | [13] | Thomson C B, Randle V. J Mater Sci, 1997; 32: 1909 | | [14] | Fang X Y, Wang W G, Cai Z X, Qin C X, Zhou B X. Mater Sci Eng, 2010; A527: 1571 | | [15] | Xia S, Li H, Liu T G, Zhou B X. J Nucl Mater, 2011; 416: 303 | | [16] | Kumar M, King W E, Schwartz A J. Acta Mater, 2000; 48: 2081 | | [17] | Ding X, Chen W J. Shanghai Metall, 2006; 28(4): 14 | | [17] | (丁 霞, 陈文觉. 上海金属, 2006; 28(4): 14) | | [18] | Palumbo G, Aust K T. Acta Metall, 1990; 38: 2343 | | [19] | Liu T G, Xia S, Li H, Zhou B X, Bai Q, Su C, Cai Z G. J Mater Res, 2013; 28: 1165 | | [20] | Liu T G, Xia S, Li H, Zhou B X, Bai Q. Mater Charact, 2014; 91: 89 | | [21] | Kopezky C V, Andreeva A V, Sukhomlin G D. Acta Metall Mater, 1991; 39: 1603 | | [22] | Gottstein G. Acta Met, 1984; 32: 1117 | | [23] | Chen X P, Li L F, Sun H F, Wang L X, Liu Q. Mater Sci Eng, 2015; A622: 108 | | [24] | Xia S, Zhou B X, Chen W J. J Mater Sci, 2008; 43: 2990 | | [25] | Xia S, Zhou B X, Chen W J. Metall Mater Trans, 2009; 40A: 3016 | | [26] | Berger A, Wilbrandt P J, Ernst F. Prog Mater Sci, 1988; 32: 1 | | [27] | Liu T G, Xia S, Li H, Zhou B X, Bai Q. Mater Lett, 2014; 133: 97 |
|