| INFLUENCE OF ELECTRIC FIELD TREATMENT ON PRECIPITATION BEHAVIOR OF d PHASE IN GH4169 SUPERALLOY |
Lei WANG1( ),Jinlan AN1,Yang LIU1,Xiu SONG1,Guohua XU2,Guangpu ZHAO2 |
1 Key Lab for Anisotropy and Texture of Materials, Ministry of Education, Northeastern University, Shenyang 110819 2 High Temperature Material Research Institute, Central Iron and Steel Research Institute, Beijing 100081 |
|
Cite this article:
Lei WANG,Jinlan AN,Yang LIU,Xiu SONG,Guohua XU,Guangpu ZHAO. INFLUENCE OF ELECTRIC FIELD TREATMENT ON PRECIPITATION BEHAVIOR OF d PHASE IN GH4169 SUPERALLOY. Acta Metall Sin, 2015, 51(10): 1235-1241.
|
|
|
Abstract GH4169 alloy is widely used to make aero engine, gas turbine as it is one of the most important superalloy. γ’' phase is the main strengthen phase, however, the metastable γ’' phase will transform to stable d phase during aging or servicing for certain time. d phase is significance in the alloy, its precipitating and distributing behavior have an effect on the properties of the alloy. In recent year, researchers pay more attention on electric field treatment (EFT), this is because of high energy density, accurate controlling, clean and safety. EFT is one of the most important energy field except temperature field and stress field. In this work, EFT was performed on GH4169 superalloy to investigate the influence of EFT on precipitation behavior of d phase in the alloy, and the mechanism of the effect of EFT on the phase transformation was also discussed. The results show that d phases precipitate on the grain boundaries after EFT with 8 kV/cm at 850 ℃ for 15 min, and large amounts of γ’' phases precipitate inside the grains. With the increasing of EFT time, both the volume fraction and the size of d phase increase, at the same time the size of γ’' phase increases. The volume fraction of d phase is less and the size of d phase is smaller, and the volume fraction of γ’' phase is higher by EFT, compared with that by aging treatment (AT) for the same time. In addition, the Nb content on the grain boundary decreases and both Fe and Cr content increase, meanwhile the lattice parameters of c decreases and a, b increase. The vacancy concentrations can be accelerated by EFT, so that the diffusion of Fe and Cr atoms can be promoted. Meanwhile, the Nb atoms in d phases on the grain boundaries can be displaced by Fe atoms and Cr atoms, therefore the Nb atoms are dissolved into the grain. The nucleation rate of γ’' phases increases with the increasing of vacancy concentrations. The vacancies relax coherent distortion between γ phases and γ’' phases, and suppress γ’' phases to transform to d phases. Thus the stabilization of γ’' phases is enhanced.
|
|
|
| Fund: Supported by High Technology Research and Development Program of China (No.2012AA03A513) and National Natural Science Foundation of China (Nos.51171039 and 51371044) |
| [1] | Guo J T. Materials Science and Engineering for Superalloys. Vol.3, Beijing: Science Press, 2010: IX (郭建亭. 高温合金材料学(下册). 北京: 科学出版社, 2010: IX) | | [2] | Deng G J, Tu S T, Zhang X C, Wang Q Q, Qin C H. Eng Fract Mech, 2015; 134: 433 | | [3] | Wang Y, Lin L, Shao W Z. Trans Mater Heat Treatment, 2007; 28(suppl): 176 | | [4] | Medeiros S C, Prasad Y V R K, Frazier W G, Srinivasan R. Mater Sci Eng, 2000; A293: 198 | | [5] | Tian S G, Wang X, Xie J, Liu C, Guo Z G, Liu J, Sun W R. Acta Metall Sin, 2013; 49: 845 (田素贵, 王 欣, 谢 君, 刘 臣, 郭忠革, 刘 姣, 孙文儒. 金属学报, 2013; 49: 845) | | [6] | Cai D Y, Zhang W H, Liu W C, Xiao F R, Yao M, Sun G D, Chen Z L, Wang S G. Nonferrous Met, 2003; 55(1): 4 (蔡大勇, 张伟红, 刘文昌, 肖福仁, 姚 枚, 孙贵东, 陈宗霖, 王少刚. 有色金属, 2003; 55(1): 4) | | [7] | Srinivasan D. Mater Sci Eng, 2004; A364: 27 | | [8] | Azadian S, Wei L Y, Warren R. Mater Charact, 2004; 53(1): 7 | | [9] | Yuan H, Liu W C. Mater Sci Eng, 2005; A408: 281 | | [10] | Wang Y, Zhen L, Shao W Z, Yang L, Zhang M. J Alloys Compd, 2009; 44: 341 | | [11] | Wang Y, Shao W Z, Zhen L, Zhang B Y. Mater Sci Eng, 2011; A528: 3218 | | [12] | Zhang H, Ying Z Y, Chang X Z. J Mater Eng, 1992; (S1): 131 (张 华, 应志毅, 常雪智. 材料工程, 1992; (S1): 131) | | [13] | Tang C, Du J H, Liu J H, Deng Q. J Iron Steel Res, 2013; 25(9): 38 (唐 程, 杜金辉, 刘军和, 邓 群. 钢铁研究学报, 2013; 25(9): 38) | | [14] | An J L, Wang L, Liu Y, Xu G H, Zhao G P. Acta Metall Sin, 2015; 51: 835 (安金岚, 王 磊, 刘 杨, 胥国华, 赵光普. 金属学报, 2015; 51: 835) | | [15] | Pouranvari M, Ekrami A, Kokabi A H. Mater Des, 2013; 50: 694 | | [16] | Conrad H, Yang D. Acta Mater, 2002; 50: 2851 | | [17] | Yang D, Conrad H. Intermetallics, 2001; 9: 943 | | [18] | Liu Y, Wang L, Qiao X Y, Wang Y Q. Rare Met Mater Eng, 2008; 37(1): 66 (刘 杨, 王 磊, 乔雪璎, 王延庆. 稀有金属材料与工程, 2008; 37(1): 66) | | [19] | Liu Y, Wang L, Ding Y, Cui T, Wang Y Q. China J Nonferrous Met, 2006; 16: 1749 (刘 杨, 王 磊, 丁 扬, 崔 彤, 王延庆. 中国有色金属学报, 2006; 16: 1749) | | [20] | Zhang X Y, Wang L, Wang Y, Liu Y, Lv X D, Chao Y S. J Iron Steel Res, 2011; 23(Suppl 2): 146 (张新宇, 王 磊, 王 尧, 刘 杨, 吕旭东, 晁月盛. 钢铁研究学报, 2011; 23(增刊2): 146) | | [21] | Wang Y. PhD Dissertation, Northeastern University, Shenyang, 2013 (王 尧. 东北大学博士学位论文, 沈阳, 2013) | | [22] | Liu W, Liang K M, Zheng Y K. J Mater Sci, 1998; 33: 1043 | | [23] | Li S Q, Zhuang J Y, Yang J Y, Deng Q, Du J H, Xie X S, Li B, Xu Z C, Cao Z, Su Z Q, Jiang C Z. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Pittsburgh, PA: TMS, 1994: 545 | | [24] | Dong J X, Xie X S, Xu Z C, Zhang S H, Chen M Z, Radavich J F. In: Loria E A ed., Superalloys 718, 625, 706 and Various Derivatives, Pittsburgh, PA: TMS, 1994: 649 | | [25] | Dean J A. Lange's Chemistry Handbook Version 15th. New York: McGraw-Hill Professional, 1998: 430 |
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|