| MICROSTRUCTURE AND MECHANICAL PROPERTY OF STEEL/Al ALLOY LASER WELDING WITH Sn POWDER ADDITION |
| ZHOU Dianwu, PENG Yan, XU Shaohua, LIU Jinshui |
| State Key Laboratory of Advanced Design and Manufacturing for Vehicle Body,Hunan University, Changsha 410082 |
|
Cite this article:
ZHOU Dianwu, PENG Yan, XU Shaohua, LIU Jinshui. MICROSTRUCTURE AND MECHANICAL PROPERTY OF STEEL/Al ALLOY LASER WELDING WITH Sn POWDER ADDITION. Acta Metall Sin, 2013, 49(8): 959-968.
|
|
|
Abstract The laser welding test with Sn powder addition was carried out on DC56D+ZF galvanized steel with thickness 1.4 mm and 6016 aluminum alloy with thickness 1.2 mm. By using optical microscopy, scanning electron microscopy, X-ray diffraction and tensile test, the microstructure, fracture morphology, interface element distribution, main phase and mechanical properties of joints were studied. Elastic moduli and thermodynamic properties were calculated by using first-principles method based on density functional theory for FeAl and FeSn compounds. The results indicate that the morphology of welding surface can be improved and grain size is fine when the welding power is 2000 W, welding speed is 45 mm/s, the defocus distance is +2.0 mm, and Ar gas acts as the protection gas with flow rate 15 L/min. The average shear strength of the welding sample with Sn powder reaches 62.17 MPa. Compared to that without Sn powder addition, the average shear strength of weld joint increases by 1.46 times. Because of fine-grain strengthening and the improvement of the fluidity of the molten pool metal with Sn addition, it promotes the combination of the steel and aluminum interface and decreases the thickness of the intermetallic layer. FeSn intermetallic compounds has better ductility and is more stable than that of FeAl at high temperature that retard and reduce the generation of Fe-Al intermetallic compound, which can improve the mechanical properties of weld joint with Sn addition.
|
|
Received: 31 December 2012
|
| [1] Lei Z, Wang X Y, Wang W B, Lin S Y. Trans China Weld Inst, 2007; 28(11): 65
(雷振, 王旭友, 王伟波, 林尚杨. 焊接学报, 2007; 28(11): 65)
[2] Torkamany M J, Tahamtan S, Sabbaghzadeh J. Mater Des, 2010; 31: 458
[3] Zhang Q Y, Liu S Q. Acta Metall Sin, 1981; 17: 300
(张启运, 刘淑淇. 金属学报, 1981; 17: 300)
[4] Guo J T, Sun C, Tan M H, Li H, Lai W H. Acta Metall Sin, 1990; 26: 20
(郭建亭, 孙超, 谭明晖, 李辉, 赖万慧. 金属学报, 1990; 26: 20)
[5] Zhang Q X. Rare Met Mater Eng, 1990; 20: 27
(章桥新. 稀有金属材料与工程, 1990; 20: 27)
[6] Wang L G, Zhang B F, Guan S K, Qi X H, Geng J Y. Rare Met Mater Eng, 2007; 36: 59
(王利国, 张保丰, 关绍康, 齐新华, 耿家源. 稀有金属材料与工程, 2007; 36: 59)
[7] Boag A, Hughes A E, Wilson N C, Torpy A, Macrae M C, Glenn A M, Muster T H. Corros Sci, 2009; 51: 1565
[8] Akdeniz M V, Mekhrabov A O. Acta Mater, 1998; 46: 1185
[9] Mathieu A, Pontevicci S, Viala J C, Cicala E, Matte\"{\i S, Grevey D.Mater Sci Eng, 2006; A435-436: 19
[10] Lin S B, Song J L, Yang C L, Fan C L, Zhang D W. Mater Des, 2010; 31: 2637
[11] Braun R. Mater Sci Eng, 2006; A426: 250
[12] Sierra G, Peyre P, Deschaux B F. Mater Charact, 2008; 59: 1705
[13] Segall M D, Lindan P L D, Probert M J, Pickard C J, Hasnip P J, Clark S J,Payne M C. J Phys: Condens Matter, 2002; 14: 2717
[14] Marlo M, Milman V. Phys Rev, 2000; 62B: 2899
[15] White J A, Bird D M. Phys Rev, 1994; 50B: 4954
[16] Lei Z, Yu N, You A Q, Lin S Y. Trans China Weld Inst, 2008; 29(6): 21
(雷振, 于宁, 游爱清, 林尚扬. 焊接学报, 2008; 29(6): 21)
[17] Song J L, Lin S B, Yang C L, Ma G C. Aeronaut Manuf Technol, 2008; 12: 26
(宋建岭, 林三宝, 杨春利, 马广超. 航空制造技术, 2008; 12: 26)
[18] Hao Y L, Xu D S, Cui Y Y, Yang R, Li D. Acta Mater, 1999; 47: 1129
[19] Kobayashi S, Yakou T. Mater Sci Eng, 2002; A338: 44
[20] Simmons G, Wang H. Single Crystal Elastic Constants and Calculated Aggregate Properties. Cambridge: MIT Press, 1971: 80
[21] Fu C L, Yoo M H. Acta Mater, 1992, 40: 703
[22] Kong Y, Hu W Y, Huang Y C, Shu X L. Rare Met Mater Eng, 2003; 32: 87
(孔毅, 胡望宇, 黄杨程, 舒小林. 稀有金属材料与工程, 2003; 32: 87)
[23] Mehl M J, Osburn J E, Papaconstantopoulos D A, Klein B M. Phys Rev,1990; 41B: 10311
[24] Pugh S F. Philos Mag, 1954; 45: 823
[25] Yu W Y, Wang N, Xiao X B, Tang B Y, Peng L M, Ding W J. Solid State Sci,2009; 11: 1400
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|